A plasma arc welding (PAW)-tungsten inert gas (TIG) hybrid welding process is proposed to weld pure nickel. In PAW-TIG welding, the arc of the PAW was first to be ignited, then TIG was ignited, while in PAW welding, only the PAW arc was launched. This paper investigated the effect of different welding processes on electrochemical and corrosion performance of between a pure nickel joint and a base metal in an aerated 1 M NaCl solution, respectively. The average grain size of the joint fabricated by PAW welding (denoted as JP joint) is 463.57 μm, the joint fabricated by PAW-TIG welding(denoted as JP-T joint) is 547.32 μm, and the base metal (BM) is 47.32 μm. In this work, the passivity behaviors of samples were characterized for two welding processes by electrochemical impedance spectroscopy (EIS), open circuit potential versus immersion time (OCP-t), and the potentiodynamic polarization plots. EIS spectra, attained with different immersion times, were analyzed and fitted by an equivalent electrical circuit. Photomicrographs of BM, JP, and JP-T were also taken with a scanning electron microscope (SEM) to reveal the morphological structure of the pit surfaces. Electrochemical tests show that the sequence of the corrosion resistance is BM > JP > JP-T. The size and quantity of the hemispherical corrosion pits of all samples are different. The corrosion morphology observations found a consistency with the consequence of the electrochemical measurements. The results show that an increase of the grain dimensions due to different heat treatments decreased the pure nickel stability to pitting corrosion.
Contrast experiments of lap joints among dissimilar AZ31B Mg alloy, Mg99.50, zinc-coated DP600 sheet, and non-zinc-coated DP600 sheet were made by friction stir keyholeless spot welding (FSKSW) and vacuum diffusion welding (VDW), respectively. Scanning electron microscopy (SEM) and energy disperse spectroscopy (EDS) were used to investigate the microstructures and components of the joints welded. The experimental results show that the FSKSW bonding method is a kind of compound mode that contains a mechanical connection and element diffusion fusion connection, in which mechanical connection has the main decisive function on joints of Mg/steel. Elements diffusion exists in the interfacial region of the joints and the elements diffusion extent is basically the same to that of VDW. The elements’ diffusion in Mg/steel using FSKSW is defined in the reaction between small amounts elements of the base metal and zinc-coated metals. The intermetallic compounds and composite oxide perform some reinforcement on the mechanical connection strength.
1 April 2019 in Journal of Wuhan University of Technology-Mater. Sci. Ed.
To investigate the evolution of grain morphologies, grain boundary features, and dislocation structure in upper part of nugget zone during friction stir welding of 6082-T6 aluminum alloys, electron backscattered diffraction and transmission electron microscope techniques were employed. The results showed that the metal on retreating side of the weld zone produced thermoplastic deformation during the welding process. The substructure of the lamellar dislocation wall formed at retreating side. Motivated by the welding thermal cycle, geometric dynamic recrystallization occurred in the substructure of the lamellar grains, leading to the lamellar array of grains. Discontinuous dynamic recrystallization occurred in the lamellar grain, leading the grain to be arranged in a "necklace" form. Simultaneously, the coarse grain of base material was refined. Due to the inhomogenous distribution of stress during the welding process, the alternating presence of large grain and small grain regions on advancing side took place. During the process of welding joint tensile, the fracture results from dislocation piling-up at the Mg2Si interface in large grains with a (111)[110] orientation. Thus, the advancing side becomes the weakest part of the mechanical properties in the welding joint,the tensile strength of the joint was 275MPa with a break elongation of 6%.
Water extracts of leaves from fourteen (14) mulberry varieties growing in China were investigated for their antioxidant activity by the 2,2-diphenyl-1-picrylhydrazyl (DPPH) method. DPPH scavenging activities ranged from 34.60% to 61.70%. Total phenolic content of mulberry leaf (based on the Folin-Ciocalteu method) varied from 14.00 to 43.67 mg gallic acid equivalent/g leaf, and flavonoid content (based on the colorimetric aluminum nitrate method) varied from 4.02 to 28.32 mg rutin equivalent/g leaf. There was a significant linear relationship between the total phenolic and/or flavonoid content and the antioxidant activity in mulberry leaf extracts.