Forming co-alloying solid solutions has long been considered as an effective strategy for improving thermoelectric performance. Herein, the dense Cu2−x(MnFeNi)xSe (x = 0–0.09) with intrinsically low thermal conductivity was prepared by a melting-ball milling-hot pressing process. The influences of nanostructure and compositional gradient on the microstructure and thermoelectric properties of Cu2Se were evaluated. It was found that the thermal conductivity decreased from 1.54 Wm−1K−1 to 0.64 Wm−1K−1 at 300 K via the phonon scattering mechanisms caused by atomic disorder and nano defects. The maximum zT value for the Cu1.91(MnFeNi)0.09Se sample was 1.08 at 750 K, which was about 27% higher than that of a pristine sample.
Thermoelectric materials can directly convert heat and electricity, which is a kind of promising energy material. In view of cost and mechanical properties, polycrystalline SnSe material with high zT value is greatly desired. In this study, polycrystalline Sn0.94Pb0.01Se1-xTex samples were prepared by the vacuum melting–hot pressing sintering method. Sn vacancies, Pb and Te atoms were simultaneously introduced into the polycrystalline SnSe. The power factor of Sn0.94Pb0.01Se1-xTex samples was decreased, which could be attributed to the generation of n-type semiconductor SnSe2. In addition, the phonons were strongly scattered by point defects and dislocations, which led to the decrease of thermal conductivity—from 0.43 Wm−1K−1 to 0.29 Wm−1K−1 at 750 K. Finally, the polycrystalline Sn0.94Pb0.01Se0.96Te0.04 sample achieved the maximum zT value of 0.60 at 750 K.