In this work, a coating method was used to prepare a liquid crystal physical gel with a high orientation of liquid crystal molecules, excellent electrical conductivity, and mechanical stability. The liquid crystal matrix used was nematic phase liquid crystal (5CB), the gel factor was polyvinyl alcohol (PVA), and the conductive filler was carbon nanotubes/polyaniline (CNT/PANI). Chemical in situ polymerization was used to create CNT/PANI composites, wherein polyaniline encapsulates the carbon nanotubes to enhance their dispersion. At 4 mm/s, 7.2 N of coating pressure, and 72 s of interval duration, the shear flow-induced orientation was achieved. The consistent and large-area orientation of the liquid crystal molecules was realized and the orientation direction of the liquid crystal molecules was parallel to the coating direction. Additionally, a type of stress sensor assembly based on multiple coating demonstrated a good sensor performance in the 90° bending test and high sensitivity in the 20% tensile test, with a sensor sensitivity of 23.25. Regarding the use of liquid crystal materials in flexible electronic devices, it is quite important.
Flexible gel sensors can lose mechanical compliance and electrical stability at low temperature or during solvent loss. A poly(vinyl alcohol) (PVA)/sodium alginate (SA)/graphene oxide (GO) composite gel was prepared by freeze–thaw cycling and post-treated in either aqueous NaCl or a NaCl-containing water/glycerol mixture (1:2, v/v). The water/glycerol–NaCl-treated gel (F-G/S/P/G) exhibited a maximum tensile stress of 428 ± 27 kPa and an elongation at break of 432 ± 27% at room temperature (n = 3), and remained visibly deformable after 24 h at −20 °C. During ambient storage, it retained approximately 89% of its initial mass after 35 days. The cycle-averaged peak ΔR/R0 increased from 0.135 at 20% strain to 1.142 at 250% strain, and the 20–60% linear region gave a gauge factor of 1.01 (R2 = 0.9988). Three independently prepared sensing elements gave a peak ΔR/R0 of 0.710 ± 0.019 at 100% strain, with response and recovery times of 1.22 ± 0.07 and 1.04 ± 0.06 s, respectively. After 500 cycles at 100% strain, the normalized peak response retained 95.1% of its initial value. Overall, F-G/S/P/G combined low-temperature deformability, ambient-storage mass retention, and repeatable resistance sensing.