The paper focuses on the issue of using reclaimed asphalt (RA) in asphalt mixtures used for highly traffic-loaded asphalt pavements—in asphalt mixtures of the stone mastic asphalt (SMA) type. It is a skeleton-type mixture, where the traffic load is bore by a skeleton of coarse aggregates bonded with mastic (i.e., bitumen and fine aggregates). It is therefore essential to pay close attention to the properties of this coarse aggregate. Higher demands on properties of the aggregate are probably due to the fact that RA is not currently being used in SMA-type mixtures. Most standards do not allow usage of RA in this type of mixtures. Given that traffic load of road networks is constantly increasing, the ratio of SMA-type asphalt mixtures also increases in the road network. This paper presents results of 5-year research focused on the possibility of using RA in SMA-type asphalt mixtures. This included laboratory design of these mixtures with various dosages and types of RA. Their empirical and functional properties were verified. Based on the positive results of the laboratory testing, a test section was subsequently constructed using several variants of the mixtures containing up to 50% of RA. This test section is regularly being monitored, and despite very intense traffic load, there are no failures apparent after 2 and half years of operation. Based on the laboratory research and subsequent construction and monitoring of a test section, it can be said that RA can be used in SMA-type mixtures without any negative impacts on functional properties or mixture lifetime.
24 March 2017 in Road Materials and Pavement Design
Some bituminous binders currently available on the Central European market contain a certain ratio of visbreaking residues, obtained during non-catalytic thermal cracking of atmospheric or vacuum crude oil residues. This paper deals with a potential presence of visbreaking residues in commercially available paving grade bitumens, and their impact on the thermooxidative properties of the bitumen. The presence of visbreaking residues can be possibly indicated by the compromised chemical compatibility of the bituminous binder that can be determined by Heithaus titration. However, Heithaus titration is a relatively complicated process. It is therefore sufficient to use a simplified alternative in practice – single-point precipitation titration using isooctane. All of the tested bitumens were submitted to the accelerated ageing procedure. The changes in parameters caused by the ageing process were determined by means of a dynamic shear rheometer and bending beam rheometer. The obtained data were subsequently compared with the results from laboratory prepared binders, which contained a known portion of visbreaking residues. The content of visbreaking residues in these binders ranged from 0% to 40%. The results showed that the presence of visbreaking residues has a negative impact on the properties of paving bitumens, especially with respect to their thermooxidative ageing. Particularly, the modified method of accelerated ageing RTFOT with an extended exposition time can differentiate between the individual binders very well, and is able to correlate their properties to the content of visbreaking residues. As the content of these residues increases, the extent of change increases proportionally for the analysed parameters describing the properties of the binders in middle and elevated service temperatures. The results of the analysis suggest that the disrupted chemical compatibility proved by single-point precipitation titration using isooctane may indicate a thermooxidatively unstable bitumen, and that this fact might be related to a higher content of visbreaking residues.
In addition to the conventional laboratory tests of input materials and construction mixtures, the technically correct design of pavement structure involves more frequent functional tests of the input materials and mixtures. Our study summarizes findings from a long-term monitoring of pavement on selected road sections with lower traffic intensity. The research involved the comparison of resilient moduli as a design parameter of unbound pavement base layers’ unbound granular materials (UGMs), determined in a laboratory by a test device for a cyclical triaxial test and in situ by impact load test using a falling weight deflectometer (FWD). In particular, the resilient moduli determined in the laboratory by a cyclic triaxial test (Mr,CTT) were compared with the real values of resilient moduli measured by FWD (Mr,FWD). A new, unique, and innovative FWD device was used to determine the Mr,FWD of the UGMs. The innovation lay in the dual-axis deflection measurement—measurement performed not just in the axis parallel to the road, but also in the axis in the transversal direction. It was found that, especially on roads with lower traffic load, such dual-axis (spatial) determination of Mr,FWD moduli was of great importance because it often allowed the identification of local pavement sections with low bearing capacities, especially at the edges, which have a significantly lower value of Mr,FWD.
28 February 2020 in Road Materials and Pavement Design
The amount of produced asphalt mixtures incorporating reclaimed asphalt has been steadily increasing in the past years and so has the use of recycling agents. Some countries in Europe and elsewhere have already come into contact with repeatedly recycled materials. This study, therefore, investigated the influence of long-term ageing on multiple recycled binder blends and thereby simulated a repeated recycling process. In order to be able to understand the behaviour and well describe the characteristics of recycled binder blends, the obtained results were compared to the behaviour (results) of paving bitumens and reclaimed binders (binders extracted from Reclaimed Asphalt). Each binder group was then described by empirical tests as specified in the harmonised standard for paving bitumens (EN 12591) as well as by performance parameters for assessing long–term embrittlement such as viscoelastic temperature (VET) and the Glover–Rowe (G–R) parameter. It was found that recycled binder blends exhibited similar or higher penetration compared to paving bitumens upon recycling as well as after ageing, but the softening point shifted to a higher temperature domain. Likewise, reclaimed binders’ properties were rather similar to long-term aged paving bitumens than to recycled binder blends. Furthermore, it was confirmed that a strong correlation between VET and G–R exists although different binder groups manifested different durability thresholds. Additionally, a relationship was found between VET, G–R and softening point. It was proved that usage of empirical tests can in some cases provide asphalt engineers with equivalent information about binder rheology as modern functional parameters in case of non-modified binders.
This study investigates the synergistic effects of combining polyphosphoric acid (PPA) and styrene–butadiene–styrene (SBS) as modifiers in asphalt binders to enhance their performance. The research focuses on optimizing the concentrations of PPA and SBS to improve the resistance to permanent deformation, cracking at intermediate and low temperatures, and resistance to aging. A series of empirical and rheological tests, including penetration, softening point, elastic recovery, dynamic shear rheometer (DSR), multiple stress creep recovery (MSCR), and bending beam rheometer (BBR), were conducted to evaluate the rheological and engineering properties of the modified binders. The results indicate that PPA can partially replace SBS, offering comparable improvements in high-temperature performance and creep resistance. The MSCR test revealed a statistically significant synergistic effect between PPA and SBS, resulting in improved recovery and reduced non-recoverable compliance. However, PPA alone shows limited effectiveness at low temperatures and in properties that are governed by elastic response. This study highlights the potential for optimizing asphalt modifiers by leveraging the complementary properties of PPA and SBS in hybrid systems, particularly regarding high-temperature properties and dynamic loading.