Functionality of mortar and concrete mixes is regulated by surfactants, which act as plasticizers. The molecular structure of these admixtures can be changed during hydration of alkali-activated cements (AAC). The objective was to determine the chemical nature of plasticizers effective for property modification of mortars and concretes based on AACs with changing content of granulated blast furnace slag from 0 to 100 %. The admixtures without ester links become more effective than polyesters when content of alkaline component increase. The admixtures effective in high alkaline medium were used in dry mixes for anchoring (consistency of mortar 150 mm by Vicat cone; 1 d tensile strength in bending / compressive strength of mortar 6.6 /30.6 MPa) and in ready-mixed concretes (consistency class changed from S1 to S3, S4 with consistency safety during 60 min; 3 d compressive strength of modified concrete was not less than the reference one without admixtures).
The use of blast furnace cement is an effective way to meet the requirements of sustainable development. However, CEM III/C is characterized by slow strength gain. The problem can be worse for plasticized reinforced blast furnace cement concretes mixed with sea water in view of shorter durability. The mitigation of corrosion in plasticized blast furnace cement concretes mixed with sea water can be provided through a composition of minor additional constituents, with percentage by mass of the main constituents: alkali metal compounds, 2…3; calcium aluminate cement, 1; clinoptilolite, 1. The alkali metal compounds are known to activate hydraulic properties of ground granulated blast furnace slag. A calcium aluminate cement promotes the accelerated chemical binding of Cl− and SO42−-ions with the formation of Kuzel’s salt. A clinoptilolite occludes these aggressive ions. The positive effects of the mentioned minor additional constituents in the blast furnace cement were supported by the increased early strength gain and the higher structural density, as well as by a good state of steel reinforcement, in the plasticized concretes mixed with sea water.
The paper is devoted to mitigation of steel reinforcement corrosion in alkali-activated slag cement (further, AASC) concretes, based on soluble sodium silicates (further, SSS’s), obtained from high consistensy concrete mixes. Enhancement of AASC fine concretes crack resistance due to modification by complex shrinkage-reducing additives (further, SRA’s) based on surfactants and trisodium phosphate Na3PO .12H2O (further, TSP) was proposed for mitigation of steel reinforcement corrosion. SSS’s were presented by sodium metasilicate (silica modulus 1.0, dry state) and water glass (silica modulus 2.9, density 1400 kg/m3). In case of sodium metasilicate the application of SRA composition “ordinary portland cement clinker – TSP – sodium lignosulphonate – sodium gluconate” provides enhancement of crack resistance starting from early age structure formation with restriction of drying shrinkage from 0,984 to 0,713 mm/m after 80 d. The effect is caused by reduction of water and by higher volume of crystalline hydrates. In turn, SRA presented by compositions “TSP – glycerol” and “TSP – glycerol – polyacrylamide” provide enhancement of AASC fine concretes fracture toughness during late structure formation with increasing ratio of tensile strength in bending to compressive strength up to 37 – 49 % if compare with the reference AASC when water glass is used.
Properties of dry mixes for anchoring application (increasing of mortars strength, adhesion, volume stability etc.) based on alkali activated Portland cement (AAPC) are influenced by different factors. One of them is application of chemical admixtures with different functionality. Adhesive properties are mainly achieved by redispersible polymer powders (RPP). The main problem in choice of RPP’s type is destruction of their molecules with ester links due to alkaline hydrolysis.The purpose of work was investigation of RPP’s molecular structure influence on properties of mortar for anchoring application based on AAPC and determination of the most effective.Efficiency of RPP based on copolymer of versatile acid ester was shown. The application of this RPP provides adhesion of 1.1 MPa and consistency of 190 mm. Positive effect of copolymer of ethylene and vinyl acetate was shown despite of partial destruction of RPP’s molecule as a result of alkaline hydrolysis of vinyl acetate at early terms of hardening. Negative effect of RPP is in decreasing of mortar strength. Thus this problem solving is decreasing of powder content to values which provide necessary physical-mechanical properties (strength, adhesion).
The peculiarity of alkali-activated slag cements (further, AASC’s) is increased proper deformations, which can cause increased cracking and reduced durability of structure. The paper is devoted to manage AASC’s proper deformations. The main task was to determine the composition of complex additives (further, CA’s) in system «ordinary portland cement (further, OPC) clinker - mineral compound of different anionic type - surfactant» in presence of sodium metasilicate (further, MS) to affect on hydrated AASC performance while ensuring effective structure of artificial stone by criterion of shrinkage deformations. Comparative analysis of hydrated cement systems "OPC clinker - MS", "OPC clinker - mineral compound - MS" and "OPC clinker - mineral compound - MS - surfactant" showed that the greatest effect on reduction of proper deformations occurs when the mineral compounds relate to electrolytes, i.e. Na2SO4 and NaNO3. Hydrated system is characterized by expansion (+0,062 mm/m) in presence of Na2SO4. Almost no shrinkage is supplied by application of NaNO3 (-0,062 mm/m). The obtained CA’s were tested in AASC. CA in the system “OPC clinker - NaNO3 - surfactant” provides the initial setting 43 min, the end - 65 min with accelerated strength. Investigated AASC can be classified as non-shrinking cement. This phenomena is ensured by increasing density, homogeneity and monolithicity of hydrosilicate formations, as well as due to formation of hydroaluminosilicate structures with different morphology by inclusion of nitrate anions.