This work investigates the behavior of porous alumina (with the porosity ranging from 18% to 70%) and zirconia (with the porosity ranging from 10% to 60%) ceramics when subjected to deformation by compression and shearing. The analysis of stress-strain curves showed that there is a transition from a typical brittle state for relatively dense ceramics, to a pseudo-plastic one for ceramics with high porosity. The values of the effective Young’s modulus, effective shear modulus and Poisson’s ratio decrease with the increase of the pore space volume of ceramics, which correlates with the appearance of multiple cracking during the deformation of the high porosity ceramics.
WC-(Fe-Mn-C) composites with γ-iron and γ + α’ matrices were sintered and then tested at sliding speeds in the range 7–37 m/s. The coefficient of friction was exponentially reduced as a function of sliding speed reaching its minimum at 37 m/s. This behavior was provided by the mechanochemical formation of iron tungstate FeWO4 on the worn surfaces of composite samples. The lubricating effect of iron tungstate did not, however, allow for a reduction in wear. The worn surface was represented by a 3–10 μm-thickness tribological layer composed of fine WC and iron particles cemented by FeWO4. This layer provided the self-lubricating effect in high-speed (high-temperature) sliding because of its easy shear and quasi-viscous behavior. The underlying 25–65 μm of thickness layer was composed of only heat-affected WC and recrystallized iron grains.
1 January 2018 in Epitoanyag - Journal of Silicate Based and Composite Materials