Basalt rockwool wastes with large output, which are toxic and require expensive environmental treatment, are produced during the production of rock wool. Hence, it is urgent to find an effective method to reuse these materials. In this study, polyaniline (PANI)-coated basalt rockwool wastes (BRWs) were prepared as fillers to serve in coatings for the anticorrosion study. Results show that the PANI-coated BRW (PANI@BRW) had enhanced dispersion stability in several conventional solvents and improved the anticorrosion performance of the epoxy resin coating. A high protection efficiency of 97.7% could be obtained from the coating with 5% fillers after immersion for 30 days. This study not only provides a promising method of solving the issues caused by BRW, but also turns these wastes into valuable substances.
The accumulation of marine biological growth has irreversible negative effects on shipping and coastal fisheries. In this paper, a new antibacterial nanofiller—triazole fluoroaromatic hydrocarbon−modified nano−zinc oxide (ZnO−APTES−TRF)—was prepared by a Cu(I)−catalyzed azide–alkyne click chemical reaction. The modification of nano−ZnO with triazole ring fluoroaromatic hydrocarbons were testified by FT−IR, XPS, and EDS. The grafting rate of ZnO−APTES−TRF can reach 32.38%, which was verified by the TGA test. The ZnO−APTES−TRF was mixed with zinc acrylate resin to produce a low surface energy antifouling coating with a surface water contact angle of 106°. The bactericidal rate of ZnO−APTES−TRF against Escherichia coli, Staphylococcus aureus, and Pseudoalteromonas sp. can reach more than 98% due to the synergistic effect of triazole and fluorine. The 120−day marine experiment shows that the low surface energy antifouling coating of ZnO−APTES−TRF/ZA is expected to be widely used in the field of marine antifouling.