Tiangang Zhang

Tiangang Zhang


Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
27 June 2022 in Coatings
Verified
Journal Article
Open access
PDF file
ZZZhiqiang Zhang
Zhiqiang Zhang
QYQIan Yang
QIan Yang
FYFan Yang
Fan Yang
HZHongwei Zhang
Hongwei Zhang
TZTiangang Zhang
Tiangang Zhang
QMQiang Ma
Qiang Ma
Several innovative mixed powders of Ti6Al4V and NiCr-Cr3C2 with different CeO2 contents (0, 1, 2, 3, and 4 wt.%) were designed, and Ti2C-reinforced CrTi4-based composite coatings were prepared on the Ti6Al4V surface via laser cladding technology. The effects of CeO2 amount on the forming quality, microstructure, hardness, and wear resistance of the composite coatings were studied. The results showed that the CeO2 amount had a significant influence on the forming quality of the composite coatings. The cracks were eliminated completely when the CeO2 content was 2 wt.%; furthermore, the lowest porosity was obtained with the addition of 3 wt.% CeO2. The primary phase constituents of the coatings were non-stoichiometric Ti2C and a β-type solid solution (CrTi4) as the reinforcement and matrix, respectively. CeO2 and a low quantity of Ce2O3 were re-precipitated at the Ti2C/CrTi4 interface and CrTi4 grain boundary in the coatings with CeO2 addition. In addition, the average hardness of the composite coatings was 1.28–1.34 times higher than that of the Ti6Al4V substrate. The wear resistance of the composite coatings was significantly higher than that of the substrate. However, both the composite coatings and the Ti6Al4V substrate exhibited a mixed-wear mode, i.e., abrasive and adhesive wear.

8 January 2024 in Actuators
Verified
Journal Article
Open access
PDF file
SHShiwei He
Shiwei He
ZZZhiqiang Zhang
Zhiqiang Zhang
HLHanxi Li
Hanxi Li
TZTiangang Zhang
Tiangang Zhang
XLXuecheng Lu
Xuecheng Lu
JKJiajie Kang
Jiajie Kang
A thin-walled structure of high-strength aluminum alloy 2024 (AA2024) was fabricated using novel laser and cold metal transfer and pulse (CMT-P) arc hybrid additive manufacturing (LCAHAM) technology. The influence of the wire feeding speed, scanning speed, and laser power on the forming quality was systematically studied by the response surface methodology, probability statistical theory, and multi-objective optimization algorithm. The result showed that the forming accuracy was significantly more affected by the laser power than by the wire feeding speed and scanning speed. Specifically, there was an obvious correlation between the interaction of the laser power and wire feeding speed and the resulting formation accuracy of LCAHAM AA2024. Moreover, the laser power, wire feeding speed, and scanning speed all had noticeable effects on the spattering degree during the LCAHAM AA2024 process, with the influence of the laser power surpassing that of the other two factors. Importantly, these three factors demonstrated minimal mutual interaction on spattering. Furthermore, the scanning speed emerged as the most significant factor influencing porosity compared to the wire feeding speed and laser power. It was crucial to highlight that the combined effects of the wire feed speed and laser power played an obvious role in reducing porosity. Considering the forming accuracy, spattering degree, and porosity collectively, the recommended process parameters were as follows: a wire feeding speed ranging from 4.2 to 4.3 m/min, a scanning speed between 15 and 17 mm/s, and a laser power set at approximately 2000 W, where the forming accuracy was 84–85%, the spattering degree fell within 1.0–1.2%, and the porosity was 0.7–0.9%.

21 June 2022 in Coatings
Verified
Journal Article
Open access
PDF file
TZTiangang Zhang
Tiangang Zhang
HZHao Zhen
Hao Zhen
TLTianxiang Liu
Tianxiang Liu
XHXiaoyun Hou
Xiaoyun Hou
ZZZhiqiang Zhang
Zhiqiang Zhang
Lubricating-reinforcing composite coatings were successfully prepared on Ti6Al4V using laser-clad Ti6Al4V/Ni60/Ni-MoS2 mixed powders with different Ni-MoS2 contents (25, 35, and 45 wt.%), and their microstructure and tribological properties were studied. The reinforcing phase TiC, Ti2Ni, and the lubricating phase Ti2SC were in situ precipitated while Ti2SC and Ti2Ni formed a mosaic coherent structure within the above three coatings. In the 25 and 45 wt.% Ni-MoS2 coatings, the microstructure distribution uniformity of the coatings was not effectively improved by the Ti2SC-Ti2Ni mosaic structure phase due to the lower or higher content of Ti2SC. In the 35 wt.% Ni-MoS2 coating, the forming quality of the coating was the best due to an appropriate amount of the uniformly distributed Ti2SC-Ti2Ni mosaic structure phase. Furthermore, the microhardness of the coatings gradually decreased as the amount of Ni-MoS2 increased. In the 35 wt.% Ni-MoS2 coating, due to the uniformly and diffusely distributed Ti2SC-Ti2Ni mosaic structure phase, the stable lubricating-reinforcing mosaic structure transfer composite films were formed during the progress of the friction and wear tests, which led to the optimal worn surface evenness and quality, the anti-friction and the wear resistance properties compared with the Ti6Al4V, 25 and 45 wt.% Ni-MoS2 coating.

2 September 2024 in Coatings
Verified
Journal Article
Open access
PDF file
CWChanghao Wang
Changhao Wang
QZQiyu Zhang
Qiyu Zhang
TZTiangang Zhang
Tiangang Zhang
HZHao Zhen
Hao Zhen
ZZZhiqiang Zhang
Zhiqiang Zhang
HCHuijun Cao
Huijun Cao
To extend the safety service life of aviation TC4 alloy, the composite coatings of TC4 + Ni-MoS2 + WC + xY2O3 (x = 0, 1, 2, 3, 4 wt.%) were prepared on TC4 by coaxial powder feeding laser cladding technology. The results showed that all the coatings had the same generated phases which mainly consisted of TiC, Ti2Ni, Ti2S, matrix β-Ti, and unfused residual WC. Y2O3 formed co-dependent growth relationships with TiC, Ti2S, and Ti2Ni. Meanwhile, TiC-Ti2S, TiC-Ti2Ni, and Ti2S-Ti2Ni coherent composite structure phases were effectively synthesized in all the coatings. With the increase in the Y2O3 content, the exposed area of the matrix increased and other phases refined progressively. When the Y2O3 content in the coatings were 3 and 4 wt.%, the degree of phase refinement in the coatings was consistent and the phases grew along grain boundaries, but microstructure segregated in the 4 wt.% Y2O3 coating. The microhardness of all the coatings was higher than that of TC4 and decreased with the increase in the Y2O3 content. Higher friction coefficients and lower wear rates both appeared in all the coatings than in the substrate, and they presented a trend of decreased first and then increased with the addition of Y2O3, in which the 3 wt.% Y2O3 coating had the lowest friction coefficient and optimal wear resistance. The research found that the Y2O3 could not change the types of phases in the coatings and could serve as a heterogeneous nucleation center for the refinement of the TiC-Ti2S-Ti2Ni coherent structure phase. Meanwhile, except for the matrix phase, Y2O3 could attract other phases to pinning on the grain boundaries of the coatings. The content of Y2O3 was negatively correlated with the hardness and wear resistance of the coating and it had the optimal tribological properties with the moderate amount of Y2O3. The wear mechanism of all coatings was abrasive wear.