28 May 2019 in Applied Sciences
Verified
Journal Article
Open access
PDF file
JFJie Fan
Jie Fan
GLGengying Li
Gengying Li
SDSijie Deng
Sijie Deng
ZWZhongkun Wang
Zhongkun Wang
The mechanical properties of cement mortars with 0~2.0% (by mass) polyvinyl alcohol (PVA) were experimentally studied, and the effects of PVA incorporation on the hydration products and microstructure of the cement mortar were determined with differential scanning calorimetry (DSC), Fourier transform infrared spectroscopy (FTIR) and scanning electron microscopy (SEM). The results show that the rational content of PVA formed evenly dispersed network-like thin films within the cement matrix, and these network-like films can bridge cracks in the cement matrix and improve the mechanical properties of the cement mortar. Over- incorporation of PVA may result in the formation of large piece polymer films that coat the cement particles, delay the hydration of the cement mortar and adversely affect its performance. The mechanical properties of the cement mortar show a significant increase and then decrease with a change in the PVA incorporation. When the PVA content was 0.6% and 1.0%, the mortar had the best compressive and flexural strengths, respectively. The compressive strength of the cement mortar increased by 12.15% for a PVA content of 0.6%, and the flexural strength of the cement mortar increased by 24.83% for a PVA content of 1.0%.

22 June 2020 in Materials
Verified
Journal Article
Open access
PDF file
JFJie Fan
Jie Fan
GLGengying Li
Gengying Li
SDSijie Deng
Sijie Deng
CDChengwei Deng
Chengwei Deng
ZWZhongkun Wang
Zhongkun Wang
Zhijun ZhangZhijun Zhang
Zhijun Zhang
Carbon nanotubes (CNTs) are considered as one of the ideal modifiers of cement materials, since CNTs can improve the mechanical properties of cement paste effectively. However, the interfacial interaction between CNTs and the cement matrix is weak. Moreover, it is difficult to disperse CNTs within cement paste. To overcome these shortages, in this study, CNTs were firstly dispersed into a styrene-acrylic emulsion (SAE). Then the homo-dispersion CNT/SAE emulsion was incorporated into cement paste. The effect of the CNT/SAE hybrid-system on the mechanical properties and microstructure of cement paste was studied. For purposes of comparison, the properties of cement paste mono incorporating CNTs or SAE are also investigated. The results show that CNT/SAE network films could be observed in cement paste by using a field emission scanning electron microscope (FESEM). These network films could bridge the cracks and refine the pores of a cement matrix. Infrared analysis and Raman spectroscopy show that the CNT/SAE hybrid modifier has stronger interfacial adhesion and better load transfer ability over the mono adding of CNTs and SAE emulsion. As a result, the hybrid addition of CNT/SAE significantly improved the flexural strength of cement paste. Especially, the addition of 0.1% CNTs and 15% SAE by mass of cement improved the 28-day flexural strength of cement paste by 21% and 25% as compared to the mono addition of CNTs or SAE, respectively.

19 January 2022 in Nanomaterials
Verified
Journal Article
Open access
PDF file
JHJingjing Huang
Jingjing Huang
ZWZhongkun Wang
Zhongkun Wang
DLDongsheng Li
Dongsheng Li
GLGengying Li
Gengying Li
Sulfate resistance of high-volume fly ash/cement mortars hybrid containing 0~1.5 wt.% of nano-silica (Nano-SiO2, NS) and 0~1.0 vol.% of polyvinyl alcohol (PVA) fibers was investigated in this study. Fly ash was replaced with Portland cement at levels of 60% by weight. The resistance to sulfate attack was investigated by exposing the mortars to 10 wt.% sodium sulfate (Na2SO4) solutions for 72 days, after which change in mass, compressive, and flexural strengths were determined. For comparison, the compressive and flexural strengths of cement mortar after 100 days of curing in water were also investigated. Microstructural deteriorations caused by sulfate attack were analyzed by using scanning electron microscope (SEM). The test results showed that the combination of NS and PVA fibers was effective in enhancing the mechanical properties and the resistance to sulfate attack. After 28 days curing, the hybrid addition of 1.5 wt.% NS and 1.0 vol.% PVA fibers increased the flexural strength by 90% over the control one without NS and PVA fiber. Moreover, regardless of PVA fibers content, due to the crystal nucleus and pore-filling effects, the adding of 0.5 wt.% NS increased the compressive strength by 67.1~118.2%. Chemical reaction took place between fly ash and Na2SO4 as no un-hydration particles could be observed in the samples immersed in Na2SO4 solutions for 72 days, while a lot of un-hydration fly ash particles could be found in the SEM image of mortar after 100 days curing in water. The chemical reaction production could increase the adhesive property and fill the pores of cement mortar. As a result, the compressive and flexural strengths of cement mortars after immersed in Na2SO4 solution for 72 days, were much higher than that after 28 days curing. Moreover, the compressive strength of mortars incorporating 1.0~1.5 wt.% NS was even higher than that after 100 days curing in water, indicating the combination of Nano-SiO2/PVA fiber is effective in enhancing the resistance to sulfate attack.

30 May 2022 in Materials
Verified
Journal Article
Open access
PDF file
JHJingjing Huang
Jingjing Huang
ZWZhongkun Wang
Zhongkun Wang
DLDongsheng Li
Dongsheng Li
GLGengying Li
Gengying Li
In this paper, the influence of Nano-silica (NS) and Polyvinyl alcohol (PVA) fibers on the corrosion behavior of steel rebar embedded in high-volume fly ash cement mortars under accelerated chloride attack was studied by using an impressed voltage technique. The PVA fibers used were 1.0 vol.%, and two mass fractions of cement (50 and 60 wt.%) were replaced by fly ash. Four NS mass fractions (0, 0.5, 1.0, and 1.5 wt.%) were utilized in this paper. In addition, the mono and hybrid effects of NS and PVA on the mechanical properties and water absorption of mortar were also studied. The results showed that the incorporation of PVA and nano-SiO2 can improve the flexural and compressive strengths of high-volume fly ash mortar. Generally, the flexural and compressive strengths increased with the increase of nano-SiO2 content. Moreover, the incorporation NS can also reduce the capillary water–absorption rate of cement mortar. The impressed voltage corrosion test indicated that the composite incorporation of nano-SiO2 and PVA can significantly delay the deterioration process of steel bars in mortar, effectively reducing the steel rebar’s corrosion level and increasing the exposure time of the surface crack. With hybrid-incorporation 1.0 vol.% PVA and 1.0 wt.% nano-SiO2, the steel rebar had the lowest corrosion degree, which exhibited a mass loss of 49% and increased the broken time by 71% as compared to the control mortar.

8 November 2023 in Materials
Verified
Journal Article
Open access
PDF file
CCChao Chai
Chao Chai
DZDa Zhang
Da Zhang
ZWZhongkun Wang
Zhongkun Wang
GDGuangya Ding
Guangya Ding
This paper studies the decay law of low-temperature crack resistance performance of rubber powder basalt fiber composite-modified porous asphalt concrete (CM-PAC) under medium- and high-temperature water erosion. Firstly, the prepared Marshall specimens were subjected to water erosion treatment at different temperatures of 20 °C, 40 °C, and 60 °C for 0–15 days. Then, the processed specimens were subjected to low-temperature splitting tests, and acoustic emission data during the splitting test process were collected using an acoustic emission device. It can be seen that the low-temperature splitting strength and low-temperature splitting stiffness modulus of CM-PAC gradually decrease with the increase in water erosion time. The maximum reduction rates of the two compared to the control group reached 72.63% and 91.60%, respectively. The low-temperature splitting failure strain gradually increases. Under the same erosion time, the higher the temperature of water, the more significant the amplitude of changes in the above parameters. In addition, it is shown that as the water erosion time increases, the first stage of loading on the specimen gradually shortens, and the second and third stages gradually advance. As the water temperature increases and the water erosion time prolongs, the acoustic emission energy released by the CM-PAC specimen during the splitting process slightly decreases. The application of acoustic emission technology in the splitting process can clarify the changes in the failure pattern of CM-PAC specimens during the entire loading stage, which can better reveal the impact of medium- to high-temperature water on the performance degradation of CM-PAC.

2 November 2021 in Applied Sciences
Verified
Journal Article
Open access
PDF file
JFJie Fan
Jie Fan
ZWZhongkun Wang
Zhongkun Wang
GLGengying Li
Gengying Li
In this paper, the preparation method and reasonable mix ratio of non-calcination brick with rock powder, cement, lime and fly ash ceramsite (FAC) as the raw materials were experimentally evaluated. To better understand the effects of each component on the performance of non-calcination rock powder brick (NCRPB), an orthogonal experimental design was conducted with the water–cement ratio (W/C), rock powder–cement ratio (R/C), lime content (wl) and FAC content (wf) as the main factors, which involved four factors and three factor levels. According to the orthogonal experimental design, the compressive strength, water resistance and bulk density of nine groups of NCRPB specimens were tested. The results show that R/C was the most important factor affecting the compressive strength and water resistance, while the FAC content influenced the bulk density of NCRPB greatly. In this study, the reasonable mix of W/C, R/C, wl, and wf in weight was 0.6, 3.0, 30% and 21%, respectively. In addition, the microstructure and strength formation mechanism of NCRPB were analyzed by using SEM and XRD. The test results show that the rock powder having pozzolanic activity could react with the additional Ca(OH)2 to produce hydration products, leading to the improvement of the performance of NCRPB.