Well-dispersed Ni and Sm 2 O 3 nanoparticles embedded in an ordered mesoporous Al 2 O 3 material simultaneously exhibit high catalytic activity and stability for the CO methanation reaction.
ZrO2 is an excellent ceramic preparation material that can maintain chemical stability in medium–strong acid and alkali environments. The sintering impregnation method was used to prepare the ZrO2/TiO2/Al2O3 composite nanofiltration membrane (ZTA membrane). Nano-ZrO2, submicron TiO2, and microporous Al2O3 were used as the surface layer, the transition layer, and the support layer, respectively. The structure and phase of the membrane were measured by scanning electron microscopy (SEM) and X-ray diffractometer (XRD). The composite membrane’s retention, hydrophilic and hydrophobic properties were characterized and evaluated using a UV–Vis spectrophotometer, a water contact angle tester (WCA), and a dead-end filtration device. With the increase in separation layer deposition time, the retention rate of methyl blue increased, and the water flux decreased. At a deposition time of 75 min, the retention rate of methyl blue was more than 80%, and the water flux reached 337.5 L·m−2 h−1 bar−1 at −1 bar transmembrane pressure. The membranes are hydrophilic and have different interception abilities for metal ions, and the order of retention effect is Ag+ > Cu2+ > Mg2+ > Na+, and Ag+ and Cu2+ reached 65.3% and 50.5%, respectively. The prepared ZTA composite nanofiltration membrane has potential application value in heavy metal ion filtration.
In this paper, the roles of the welding process on the heterogeneous microstructure and mechanical properties of Q345R welded joints were analyzed by a series of tests, including the preparation of welded joints with different welding processes, optical microscope observation, uniaxial tensile tests, and hardness and impact measurements. The experimental results show that with the increase in welding heat input, the content of pre-eutectoid ferrite and the size of the Weidner structure increased, while the hardness and the impact absorption energy of the weld zone decreased gradually. With the increase in heat input, the volume proportion of eutectoid ferrite in the weld increased from 9.90% to 18.78%; the volume proportion of acicular ferrite decreased from 85.10% to 76.21%. With the decrease in heat input, the volume proportion of eutectoid ferrite decreased from 10.58% to 1.45%, and the volume proportion of acicular ferrite increased from 84.21% to 92.74%. Under the influence of the second welding heat, the first weld zone, the fusion zone and part of the heat-affected zone were re-austenitizing, and the distribution of ferrite and pearlite was more uniform. The hardness value of the former weld was lower than that of the second weld, and the distribution was more uniform. The maximum hardness value of the second weld zone and its corresponding heat-affected zone increased with the increase in depth. The distribution of the yield strength and the tensile strength of welded joints was similar to that of hardness.
The corrosion behavior of N80 steel in Multiple thermal fluid environment containing O2 and CO2 was analyzed by Scanning Electron Microscopy (SEM), Energy-dispersive Spectrometry (EDS) and X-ray Diffraction (XRD) techniques. The results showed that, the corrosion products formed on N80 steel showed double layer structure. The outer layer are loose and porous, providing little protection. The inner layer are mainly FeCO3 crystals, and a small amount of Fe2O3 and FeOOH composition. The formation of Fe oxide on the inner layer of the film destroyed the integrity of the inner layer, resulting in localized corrosion. During the development of pitting, Cl− is enriched only at the tip of the pitting hole, which is the main cause of pitting corrosion and eventually leads to the formation of dendritic localized corrosion. The difference between internal and external potentials, the O2 concentration and the decrease of pH in the pitting holes combined to increase the corrosion process.
CoSb3-based skutterudites, as a medium-temperature thermoelectric material, show excellent thermoelectric performance, but high thermal conductivity suppresses the high ZT value. Here, x% SnTe/Yb0.2(CoSb2.875Te0.125)4 samples were synthesized through vacuum melting reaction and spark plasma sintering (SPS). With increasing of SnTe content, the dispersed phase CoSb2, SnTe and CoTe2 appear successively via a selection of nucleation kinetics for 1%, 3% and 5% SnTe composited sample. Due to scattering of the dispersed phase and the solid solution distortion, lattice conductivity (κlat) of the 3% SnTe/Yb0.2(CoSb2.875Te0.125)4 sample decreases from 1.55 W m−1 K−1 to 1.19 W m−1 K−1 compared with the Yb0.2(CoSb2.875Te0.125)4 sample, which reduces by ∼22.8% at 773 K. The maximum thermoelectric merit ZT of the 3% SnTe/Yb0.2(CoSb2.875Te0.125)4 sample achieves 1.18 at 773 K.
About Me
Teacher from Shandong University of Science and Technology
Teacher from Shandong University of Science and Technology