Xiaodong Hu

Prof. Xiaodong Hu


Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
15 April 2020 in International Journal of Steel Structures
Verified
Journal Article
Closed access
PDF file
XHXiaodong Hu
Xiaodong Hu
CMChongbin Ma
Chongbin Ma
YYYicheng Yang
Yicheng Yang
QZQingliang Zeng
Qingliang Zeng

26 May 2020 in Materials
Verified
Journal Article
Open access
PDF file
XHXiaodong Hu
Xiaodong Hu
HJHao-Yong Jiang
Hao-Yong Jiang
YLYun Luo
Yun Luo
QJQiang Jin
Qiang Jin
WPWei Peng
Wei Peng
CYChun-Mei Yi
Chun-Mei Yi
The repair reinforcement height is an important parameter of repair welding, which may have a great influence on structural integrity. In this paper, the effects of repair welding reinforcement height on the microstructure, microhardness, residual stresses and stress corrosion cracking (SCC) behavior of a 304 stainless steel-repaired joint were investigated by experimentation and simulation. With an increase of the repair weld reinforcement height, the δ ferrite content in weld and fusion zone is obviously reduced, and the ferrite shape is gradually changed from the skeleton to the worm shape. With the increase of repair welding reinforcement height, the microhardness and residual stresses decrease gradually. The tensile strength and elongation for higher repair weld reinforcement height are larger than those with lower repair weld reinforcement height. The higher the repair weld reinforcement height, the harder it is for SCC to occur. The repair welding in 304 stainless steel is recommended to be repaired no more than two times.

28 September 2020 in Materials
Verified
Journal Article
Open access
PDF file
ZCZhaoxing Cui
Zhaoxing Cui
XHXiaodong Hu
Xiaodong Hu
SDShiyun Dong
Shiyun Dong
SYShixing Yan
Shixing Yan
XZXuan Zhao
Xuan Zhao
The performance and service life of the nuclear emergency diesel engine shaft made of 12CrNi2 alloy steel is very important for the safety of nuclear power. Laser melting deposition (LMD) is a challenging camshaft-forming technology due to its high precision, rapid prototyping, and excellent parts performance. However, LMD is an unsteady process under the local action of laser, especially for curved surface forming, which is more likely to generate large residual stress on components, resulting in cracks and other defects. At present, the stress research on LMD curved surface forming is relatively insufficient. In the present paper, material parameter testing, high-temperature mechanical properties analysis, single-track sample preparation, and heat source checks are conducted. At the same time, the ABAQUS software and the DFLUX heat source subroutine are used to compile the curved double-ellipsoidal moving heat source, and the effects of the temperature-dependent thermophysical parameters and phase change latent heat on the temperature field are considered. A three-dimensional finite element model is established to analyze the thermal stress evolution and residual stress distribution of multi-track multi-layer on a curved surface by LMD, and the effect of the scanning method and interlayer cooling time on the residual stress of the formed components is studied. The results show that with the increase in temperature, the strength of the material reduces, and the fracture morphology of the material gradually transitions from ductile fracture to creep fracture. The material parameters provide a guarantee for the simulation, and the errors of the width and depth of the melt pool are 4% and 9.6%, respectively. The simulation and experiment fit well. After cooling, the maximum equivalent stress is 686 MPa, which appears at the junction of the substrate and the deposited layer. The larger residual stress is mainly concentrated in the lower part of the deposited layer, where the maximum circumferential stress and axial stress are the tensile stress. Compared with the axial parallel lap scanning method, the arc copying lap scanning method has a relatively smaller maximum thermal stress and residual stress after cooling. The residual stress in the deposited layer is increased to some extent with the increase in the interlayer cooling time.

1 June 2020 in Metals
Verified
Journal Article
Open access
PDF file
XHXiaodong Hu
Xiaodong Hu
JXJie Xu
Jie Xu
XDXiangmei Du
Xiangmei Du
YZYong Zhang
Yong Zhang
FZFan Zhou
Fan Zhou
The fatigue crack propagation of 304 austenitic stainless steel was studied both by experiments and numerical simulations. Two methods were applied to simulate the crack propagation: the extended finite element method (XFEM) and the cohesive zone model (CZM). Based on the XFEM, the direct cyclic solver was used to simulate the fatigue crack propagation. Based on the CZM, the VUMAT subroutine was used to describe the crack tip constitutive equation during fatigue crack propagation, and the mechanical properties of the crack tip were simulated. The effects of different frequency, f, and stress ratio, R, on the fatigue crack growth life were studied by XFEM and CZM separately and compared with the experimental results. Results show that the crack propagation path simulated by the XFEM agrees well with the experimental result, but the deviation of the fatigue life between the simulated results and the experimental results is large. The CZM model can predict the crack propagation life very well in comparison with the experimental data, but it has certain limitations because the crack propagation path is preset.

24 October 2019 in Materials
Verified
Journal Article
Open access
PDF file
XHXiaodong Hu
Xiaodong Hu
YYYicheng Yang
Yicheng Yang
MSMing Song
Ming Song
In this study, the welding process of 304 stainless steel/Q345R low alloy steel composite plate is modeled by experimental and finite element methods to study the complex thermomechanical behavior. The residual stress and microstructure evolution of composite plate in the welding process are also investigated. The welding thermal cycle curve and residual stress distribution at the joint are obtained by using thermocouple and blind-hole methods. Optical microscopy, scanning electron microscopy, and energy-dispersive X-ray spectroscopy were used to investigate the evolution of microstructure, morphology, and element diffusion of the joint. The results show that the maximum von Mises welding residual stress is 312 MPa, which is located in the bottom of the start point of the weld zone. The residual stress gradually decreases and tends to be stable along the direction from the weld to the base metal. In addition, a residual stress discontinuity is found at the interface between the bimetal. It is also found that the closer it is to the weld joint, the more uniform is the austenite distribution and the smaller are the grain sizes.

12 October 2022 in Metals
Verified
Journal Article
Open access
PDF file
QHQingkun He
Qingkun He
XHXiaodong Hu
Xiaodong Hu
QSQitong Sun
Qitong Sun
ZDZhilong Dong
Zhilong Dong
XXXuefang Xie
Xuefang Xie
HWHan Wang
Han Wang
In this paper, the roles of the welding process on the heterogeneous microstructure and mechanical properties of Q345R welded joints were analyzed by a series of tests, including the preparation of welded joints with different welding processes, optical microscope observation, uniaxial tensile tests, and hardness and impact measurements. The experimental results show that with the increase in welding heat input, the content of pre-eutectoid ferrite and the size of the Weidner structure increased, while the hardness and the impact absorption energy of the weld zone decreased gradually. With the increase in heat input, the volume proportion of eutectoid ferrite in the weld increased from 9.90% to 18.78%; the volume proportion of acicular ferrite decreased from 85.10% to 76.21%. With the decrease in heat input, the volume proportion of eutectoid ferrite decreased from 10.58% to 1.45%, and the volume proportion of acicular ferrite increased from 84.21% to 92.74%. Under the influence of the second welding heat, the first weld zone, the fusion zone and part of the heat-affected zone were re-austenitizing, and the distribution of ferrite and pearlite was more uniform. The hardness value of the former weld was lower than that of the second weld, and the distribution was more uniform. The maximum hardness value of the second weld zone and its corresponding heat-affected zone increased with the increase in depth. The distribution of the yield strength and the tensile strength of welded joints was similar to that of hardness.