Masahisa Fujino

Mr. Masahisa Fujino


Research Focus & Metrics

Academic Career Length

23Years (2004-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
10 May 2016 in ECS Journal of Solid State Science and Technology
Verified
Journal Article
Closed access
PDF file
RHRan He
Ran He
MFMasahisa Fujino
Masahisa Fujino
AYAkira Yamauchi
Akira Yamauchi
YWYinghui Wang
Yinghui Wang
Tadatoma SugaTadatoma Suga
Tadatoma Suga
Cu/dielectric hybrid bonding at low temperatures of no more than 200°C remains challenging because of the different features of Cu-Cu and dielectric-dielectric (such as SiO2-SiO2) bonding. This paper reports a combined surface activated bonding (SAB) technique for low-temperature Cu-Cu, SiO2-SiO2, and SiO2-SiNx bonding. This technique involves a combination of surface irradiation using a Si-containing Ar beam and prebonding attach-detach process prior to bonding in vacuum. Wafer bonding experiments were conducted at either room temperature or 200°C. Results of bonding strength measurements, transmission electron microscopy (TEM) and energy-dispersive X-ray spectroscopy (EDS) observations, and X-ray photoelectron spectroscopy (XPS) analysis were reported and discussed to understand the present combined SAB technique.

15 January 2015 in Japanese Journal of Applied Physics
Verified
Journal Article
Closed access
PDF file
Tadatoma SugaTadatoma Suga
Tadatoma Suga
FMFengwen Mu
Fengwen Mu
MFMasahisa Fujino
Masahisa Fujino
YTYoshikazu Takahashi
Yoshikazu Takahashi
HNHaruo Nakazawa
Haruo Nakazawa
KIKenichi Iguchi
Kenichi Iguchi
4H-SiC wafer bonding has been achieved by the modified surface activated bonding (SAB) method without any chemical-clean treatment and high temperature annealing. Strong bonding between the SiC wafers with tensile strength greater than 32 MPa was demonstrated at room temperature under 5 kN force for 300 s. Almost the entire wafer has been bonded very well except a small peripheral region and few voids. The interface structure was analyzed to verify the bonding mechanism. It was found an amorphous layer existed as an intermediate layer at the interface. After annealing at 1273 K in vacuum for 1 h, the bonding tensile strength was still higher than 32 MPa. The interface changes after annealing were also studied. The results show that the thickness of the amorphous layer was reduced to half after annealing.

26 November 2019 in Japanese Journal of Applied Physics
Verified
Journal Article
Closed access
PDF file
MFMasahisa Fujino
Masahisa Fujino
KTKenji Takahashi
Kenji Takahashi
YAYuuki Araga
Yuuki Araga
KKKatsuya Kikuchi
Katsuya Kikuchi
Wafer bonding technology is one of the key technologies for high-density three-dimensional integration. We demonstrated 300 mm wafer-level hybrid bonding with Cu and an interlayer dielectric (ILD) layer with the design of 1 × 1 μ m 2 pads with 2 μ m pitch. In this sequence of the bonding process, the structure of Cu bonding pads was controlled to be precisely convex to the ILD layer by chemical-mechanical polishing. Then the bonding process was performed in vacuum. Lastly, the bonded wafers were annealed at 200 °C for the postannealing process. As a result, hybrid wafer bonding with few voids was successfully accomplished.

24 March 2016 in Japanese Journal of Applied Physics
Verified
Journal Article
Closed access
PDF file
MFMasahisa Fujino
Masahisa Fujino
HNHirozumi Narusawa
Hirozumi Narusawa
YKYuzuru Kuramochi
Yuzuru Kuramochi
EHEiji Higurashi
Eiji Higurashi
Tadatoma SugaTadatoma Suga
Tadatoma Suga
MMMasataka Mizukoshi
Masataka Mizukoshi
In this research, we develop transient liquid-phase bonding by uniaxial pressing using a Ag–Sn system. The Ag–Sn system was fabricated using Ag and Sn fine powder paste at optimized the proportions. The die bonding was performed for Cu substrates and metalized Si chips, and the sintering process was analyzed by cross-sectional observation. Die shear strength of bonded specimens was also measured. As a result, Ag–Sn completely formed a solid solution, also, Sn and Cu from substrates formed an intermetallic compound. The die shear strength was approximately 40 MPa obtained at 50 wt % Ag proportion of paste at 260, 280, and 300 °C sintering.

18 March 2016 in Japanese Journal of Applied Physics
Verified
Journal Article
Closed access
PDF file
FMFengwen Mu
Fengwen Mu
KIKenichi Iguchi
Kenichi Iguchi
HNHaruo Nakazawa
Haruo Nakazawa
YTYoshikazu Takahashi
Yoshikazu Takahashi
MFMasahisa Fujino
Masahisa Fujino
Tadatoma SugaTadatoma Suga
Tadatoma Suga
A modified surface activated bonding (SAB) with Fe–Si multi-nanolayers is expected to achieve the wafer bonding of SiC to various materials. However, Fe diffusion, which affects device performance, cannot be avoided during some annealing processes. In this work, the room-temperature wafer bonding of SiC–Si by only one sputtered Si nanolayer was successfully achieved. The bonding interface was investigated. A uniform intermediate layer with a thickness of ∼15 nm just containing Si, C, and Ar was found at the interface. The bonding strength between the SiC surface and the sputtered Si nanolayer could reach the bulk Si strength in accordance with the results of the strength test. This indicates that the wafer bonding of SiC to any other materials can be achieved easily if the material could be also strongly bonded to the sputtered Si nanolayer. In addition, the thermal and chemical reliabilities of the SiC–Si bonding interface were investigated by rapid thermal annealing and KOH etching, respectively.

9 March 2016 in Japanese Journal of Applied Physics
Verified
Journal Article
Closed access
PDF file
RHRan He
Ran He
MFMasahisa Fujino
Masahisa Fujino
AYAkira Yamauchi
Akira Yamauchi
Tadatoma SugaTadatoma Suga
Tadatoma Suga
A combined surface-activated bonding technique is studied for surface activation and water management to improve the hydrophilic SiO2–SiO2 bonding quality. Prebonding treatment involving a Si-containing Ar beam bombardment and prebonding attach-detach is employed prior to wafer bonding in vacuum. The results of bonding strength measurement, Monte Carlo simulation, and surface analysis by Fourier transform infrared spectroscopy are reported. A mechanism is proposed to better understand the nature of the hydrophilic bonding at low temperatures of no more than 200 °C. We suggest that the Si-containing Ar beam modifies the SiO2 surfaces by Si enrichment to make them more reactive for OH adsorption, while the prebonding attach and detach facilitate a further increase in the number of OH and the removal of excess trapped H2O prior to bonding, respectively. As a consequence, SiO2–SiO2 bonding strength close to the Si bulk fracture energy can be achieved after low-temperature annealing.