Tungsten trioxide (WO3) is a wide band gap semiconductor material that is used as an important electrochromic layer in electrochromic devices. In this work, the effects of the annealing temperature on the optical band gap of sol-gel WO3 films were investigated. X-ray Diffraction (XRD) showed that WO3 films were amorphous after being annealed at 100 °C, 200 °C and 300 °C, respectively, but became crystallized at 400 °C and 500 °C. An atomic force microscope (AFM) showed that the crystalline WO3 films were rougher than the amorphous WO3 films (annealed at 200 °C and 300 °C). An ultraviolet spectrophotometer showed that the optical band gap of the WO3 films decreased from 3.62 eV to 3.30 eV with the increase in the annealing temperature. When the Li+ was injected into WO3 film in the electrochromic reaction, the optical band gap of the WO3 films decreased. The correlation between the optical band gap and the electrical properties of the WO3 films was found in the electrochromic test by analyzing the change in the response time and the current density. The decrease in the optical band gap demonstrates that the conductivity increases with the corresponding increase in the annealing temperature.
Printing technologies for thin-film transistors (TFTs) have recently attracted much interest owing to their eco-friendliness, direct patterning, low cost, and roll-to-roll manufacturing processes. Lower production costs could result if electrodes fabricated by vacuum processes could be replaced by inkjet printing. However, poor interfacial contacts and/or serious diffusion between the active layer and the silver electrodes are still problematic for achieving amorphous indium–gallium–zinc–oxide (a-IGZO) TFTs with good electrical performance. In this paper, silver (Ag) source/drain electrodes were directly inkjet-printed on an amorphous a-IGZO layer to fabricate TFTs that exhibited a mobility of 0.29 cm2·V−1·s−1 and an on/off current ratio of over 105. To the best of our knowledge, this is a major improvement for bottom-gate top-contact a-IGZO TFTs with directly printed silver electrodes on a substrate with no pretreatment. This study presents a promising alternative method of fabricating electrodes of a-IGZO TFTs with desirable device performance.
Polyethylene oxide (PEO)-modified silicon dioxide (SiO2)-doped crystalline tungsten trioxide (WO3) films for use as electrochromic layers were prepared on indium tin oxide (ITO) glass by the sol–gel spin coating technique. The effects of the PEO template and SiO2 on the electrochromic transmittance modulation ability of crystalline WO3 films were investigated. Fourier transform infrared spectroscopy (FT-IR) spectra analysis indicated that PEO was decomposed after annealing at 500 °C for 3 h. X-ray diffraction (XRD) pattern analysis showed that both SiO2 and PEO helped reduce the crystalline grain size of the WO3 films. Atomic force microscope (AFM) images showed that the combined action of SiO2 and PEO was helpful for achieving high surface roughness and a macroporous structure. An electrochromic test indicated that PEO-modified SiO2-doped crystalline WO3 films intercalated more charges (0.0165 C/cm2) than pure WO3 crystalline films (0.0095 C/cm2). The above effects resulted in a good transmittance modulation ability (63.2% at 628 nm) of PEO-modified SiO2-doped crystalline WO3 films, which was higher than that of pure WO3 crystalline films (9.4% at 628 nm).
Recently, amorphous indium-gallium-zinc-oxide thin film transistors (a-IGZO TFTs) with inkjet printing silver source/drain electrodes have attracted great attention, especially for large area and flexible electronics applications. The silver ink could be divided into two types: one is based on silver nanoparticles, and the other is silver salt ink. Organic materials are essential in the formulation of nanoparticle ink as a strong disperse stabilizer to prevent agglomeration of silver particles, but will introduce contact problems between the silver electrodes and the a-IGZO active layer after annealing, which is difficult to eliminate and leads to poor device properties. Our experiment is aimed to reduce this effect by using a silver salt ink without stabilizer component. With optimized inkjet printing conditions, the high performance of a-IGZO TFT was obtained with a mobility of 4.28 cm2/V·s and an on/off current ratio over 106. The results have demonstrated a significant improvement for a-IGZO TFTs with directly printed silver electrodes. This work presents a promising platform for future printed electronic applications.
Bottom-gate all-aluminum thin film transistors with multi conductor/insulator nanometer heterojunction were investigated in this article. Alumina (Al2O3) insulating layer was deposited on the surface of aluminum doping zinc oxide (AZO) conductive layer, as one AZO/Al2O3 heterojunction unit. The measurements of transmittance electronic microscopy (TEM) and X-ray reflectivity (XRR) revealed the smooth interfaces between ~2.2-nm-thick Al2O3 layers and ~2.7-nm-thick AZO layers. The devices were entirely composited by aluminiferous materials, that is, their gate and source/drain electrodes were respectively fabricated by aluminum neodymium alloy (Al:Nd) and pure Al, with Al2O3/AZO multilayered channel and AlOx:Nd gate dielectric layer. As a result, the all-aluminum TFT with two Al2O3/AZO heterojunction units exhibited a mobility of 2.47 cm2/V·s and an Ion/Ioff ratio of 106. All processes were carried out at room temperature, which created new possibilities for green displays industry by allowing for the devices fabricated on plastic-like substrates or papers, mainly using no toxic/rare materials.
In this work, transparent, stable coplanar top-gate thin film transistors (TFTs) with an active layer of neodymium-doped indium oxide and zinc oxide (Nd-IZO) were successfully fabricated on a glass substrate by all sputtering processes. The devices with a post-annealing temperature of 400 °C exhibited good electrical performances with a saturation mobility (μsat) of 4.25 cm2·V−1·S−1, Ion/Ioff ratio about 106, Vth of −0.97 V and SS about 0.34 V/decade. Furthermore, the devices exhibited excellent negative and positive bias stability (NBS, PBS) of only a ΔVth shift of about −0.04 V and 0.05 V after 1 h, respectively. In addition, the devices showed high transparency about 96% over the visible-light region of 400–700 nm, which indicates a great potential in transparent displays.