Muyang Shi

Mr. Muyang Shi


Research Focus & Metrics

Academic Career Length

9Years (2018-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
14 January 2021 in Micromachines
Verified
Journal Article
Open access
PDF file
MSMuyang Shi
Muyang Shi
TQTian Qiu
Tian Qiu
BTBiao Tang
Biao Tang
GZGuanguang Zhang
Guanguang Zhang
RYRihui Yao
Rihui Yao
Junbiao PengJunbiao Peng
Junbiao Peng
Nickel oxide (NiO) is a wide band gap semiconductor material that is used as an electrochromic layer or an ion storage layer in electrochromic devices. In this work, the effect of annealing temperature on sol-gel NiO films was investigated. Fourier transform infrared spectroscopy (FTIR) showed that the formation of NiO via decomposition of the precursor nickel acetate occurred at about 300 °C. Meanwhile, an increase in roughness was observed by Atomic force microscope (AFM), and precipitation of a large number of crystallites was observed at 500 °C. X-ray Diffraction (XRD) showed that the NiO film obtained at such a temperature showed a degree of crystallinity. The film crystallinity and crystallite size also increased with increasing annealing temperature. An ultraviolet spectrophotometer was used to investigate the optical band gap of the colored NiO films, and it was found that the band gap increased from 3.65 eV to 3.74 eV with the increase in annealing temperature. An electrochromic test further showed that optical modulation density and coloring efficiency decreased with the increase in crystallite size. The electrochromic reaction of the nickel oxide film is more likely to occur at the crystal interface and is closely related to the change of the optical band gap. An NiO film with smaller crystallite size is more conducive to ion implantation and the films treated at 300 °C exhibit optimum electrochromic behavior.

30 July 2018 in Micromachines
Verified
Journal Article
Open access
PDF file
GZGuanguang Zhang
Guanguang Zhang
KLKuankuan Lu
Kuankuan Lu
XZXiaochen Zhang
Xiaochen Zhang
YWYuan Weijian
Yuan Weijian
MSMuyang Shi
Muyang Shi
Junbiao PengJunbiao Peng
Junbiao Peng
Tungsten trioxide (WO3) is a wide band gap semiconductor material that is used as an important electrochromic layer in electrochromic devices. In this work, the effects of the annealing temperature on the optical band gap of sol-gel WO3 films were investigated. X-ray Diffraction (XRD) showed that WO3 films were amorphous after being annealed at 100 °C, 200 °C and 300 °C, respectively, but became crystallized at 400 °C and 500 °C. An atomic force microscope (AFM) showed that the crystalline WO3 films were rougher than the amorphous WO3 films (annealed at 200 °C and 300 °C). An ultraviolet spectrophotometer showed that the optical band gap of the WO3 films decreased from 3.62 eV to 3.30 eV with the increase in the annealing temperature. When the Li+ was injected into WO3 film in the electrochromic reaction, the optical band gap of the WO3 films decreased. The correlation between the optical band gap and the electrical properties of the WO3 films was found in the electrochromic test by analyzing the change in the response time and the current density. The decrease in the optical band gap demonstrates that the conductivity increases with the corresponding increase in the annealing temperature.

16 March 2020 in Micromachines
Verified
Journal Article
Open access
PDF file
JLJinxiang Liu
Jinxiang Liu
GZGuanguang Zhang
Guanguang Zhang
KGKaiyue Guo
Kaiyue Guo
DGDong Guo
Dong Guo
MSMuyang Shi
Muyang Shi
Junbiao PengJunbiao Peng
Junbiao Peng
Tungsten trioxide (WO3) is a wide band gap semiconductor material, which is commonly not only used, but also investigated as a significant electrochromic layer in electrochromic devices. WO3 films have been prepared by inorganic and sol-gel free ammonium tungstate ((NH4)2WO4), with the modification of glycerol using the spin coating technique. The surface tension, the contact angle and the dynamic viscosity of the precursor solutions demonstrated that the sample solution with a 25% volume fraction of glycerol was optimal, which was equipped to facilitate the growth of WO3 films. The thermal gravimetric and differential scanning calorimetry (TG-DSC) analysis represented that the optimal sample solution transformed into the WO3 range from 220 °C to 300 °C, and the transformation of the phase structure of WO3 was taken above 300 °C. Fourier transform infrared spectroscopy (FT-IR) spectra analysis indicated that the composition within the film was WO3 above the 300 °C annealing temperature, and the component content of WO3 was increased with the increase in the annealing temperature. The X-ray diffraction (XRD) pattern revealed that WO3 films were available for the formation of the cubic and monoclinic crystal structure at 400 °C, and were preferential for growing monoclinic WO3 when annealed at 500 °C. Atomic force microscope (AFM) images showed that WO3 films prepared using ammonium tungstate with modification of the glycerol possessed less rough surface roughness in comparison with the sol-gel-prepared films. An ultraviolet spectrophotometer (UV) demonstrated that the sample solution which had been annealed at 400 °C obtained a high electrochromic modulation ability roughly 40% at 700 nm wavelength, as well as the optical band gap (Eg) of the WO3 films ranged from 3.48 eV to 3.37 eV with the annealing temperature increasing.

28 November 2019 in Applied Sciences
Verified
Journal Article
Open access
PDF file
XZXiaochen Zhang
Xiaochen Zhang
XLXianzhe Liu
Xianzhe Liu
KLKuankuan Lu
Kuankuan Lu
Honglong NingHonglong Ning
Honglong Ning
DGDong Guo
Dong Guo
Junbiao PengJunbiao Peng
Junbiao Peng
In this work, a thin film transistor (TFT) with Zr-doped aluminum-zinc-tin oxide (Zr-AZTO) semiconductor as active layer was investigated. The Zr-AZTO thin films were co-sputtered by ZrO2 and AZTO targets (RF-Sputter) in Ar, and annealed at 350 °C in air atmosphere. With the discharge power of AZTO increasing from 100 W to 120 W, the content of Zr element decreases from 0.63 ± 0.01 at.% to 0.34 ± 0.01 at.%, and the oxygen vacancy decreases from (19.0 ± 0.1)% to (17.3 ± 0.8)%. The results of Zr-AZTO thin film show that the main factor is the co-sputter power of ZrO2 target. With the co-sputter power of ZrO2 increasing from 15 W to 45 W, the content of Zr element increases from 0.63 ± 0.01 at.% to 2.79 ± 0.01 at.%, the content of oxygen vacancy decreases from (19.0 ± 0.1)% to (14.1 ± 0.1)%, Eg increases from 2.76 eV to 2.86 eV, and the root mean square (RMS) roughness firstly decreases from 0.402 nm to 0.387 nm and then increases to 0.490 nm. The Micro Wave Photo Conductivity Decay (μ-PCD, LTA-1620SP) was used to measure the quality of Zr-AZTO thin film and the mean peak and D value decreases from 139.3 mV to 80.9 mV and from 1.54 to 0.77 as the co-sputter power of ZrO2 increases from 15 W to 45 W, which means it has highest localized states and defects in high ZrO2 co-sputter power. The devices prepared at 15 W (ZrO2)/100 W (AZTO) co-sputter show a best performance, with a μsat of 8.0 ± 0.6 cm2/(V∙S), an Ion/Ioff of (2.01 ± 0.34) × 106, and a SS of 0.18 ± 0.03 V/dec. The device of Sample B has a 0.5 V negative shift under −20 V NBS and 9.6 V positive shift under 20 V PBS.