Sandra Tarancón

Dr. Sandra Tarancón

Universidad Politécnica de Madrid, Madrid, Spain
orcid

Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
10 August 2022 in Polymers
Verified
Journal Article
Open access
PDF file
TPTeresa Palacios
Teresa Palacios
STSandra Tarancón
Sandra Tarancón
Jose Ygnacio PastorJose Ygnacio Pastor
Jose Ygnacio Pastor
Two hybrid dental materials available for computer-aided design and manufacturing (CAD/CAM) dental restorations have been selected to explore their potential. On the one hand, the scarcely investigated polymer-based material Vita Enamic® (VE) and, on the other hand, the leucite-based material IPS Empress® CAD (EC). Their micro-structure and mechanical performance were analyzed in two environments: directly as received by the manufacturer (AR), and after immersion and storage in artificial saliva (AS) for 30 days to determine the influence of the saliva effect. To avoid an inappropriate selection of materials for clinical use, a full understanding of their mechanical behavior is essential. Therefore, this investigation aims to determine the micro-structural and chemical composition by field emission scanning electron microscopy (FE-SEM) and X-ray fluorescence analysis, establishing the density, micro- and nano-hardness, the nano-elastic modulus, and the flexural strength and fracture toughness (by introducing a femto-laser notch to replicate a real crack). In addition, fracture surfaces of the broken samples were analyzed to correlate the failure micro-mechanisms with their mechanical properties. Results indicate that while the crystalline phase of the materials is very similar (composed of SiO2 and Al2O3), the micro-structure and mechanical behavior is not. The material EC, with finer micro-structure, exhibits a higher mechanical performance but with greater variability of results. Furthermore, the material VE, with a 25 vol.% polymer phase, shows a mechanical performance similar to enamel and dentin and therefore more similar to human behavior.

1 November 2019 in International Journal of Refractory Metals and Hard Materials
Verified
Journal Article
Closed access
EGE.M. Garcia-Ayala
E.M. Garcia-Ayala
STSandra Tarancón
Sandra Tarancón
ZGZoilo Gonzalez
Zoilo Gonzalez
BFBegona Ferrari
Begona Ferrari
Jose Ygnacio PastorJose Ygnacio Pastor
Jose Ygnacio Pastor
Antonio Javier Sanchez-HerenciaAntonio Javier Sanchez-Herencia
Antonio Javier Sanchez-Herencia

6 March 2021 in Polymers
Verified
Journal Article
Open access
PDF file
TPTeresa Palacios
Teresa Palacios
STSandra Tarancón
Sandra Tarancón
Cristian Abad-CoronelCristian Abad-Coronel
Cristian Abad-Coronel
Jose Ygnacio PastorJose Ygnacio Pastor
Jose Ygnacio Pastor
This study aims to evaluate the microstructural and mechanical properties of three commercial resin-based materials available for computer-aid design and manufacturing (CAD/CAM)-processed indirect dental restoration: LavaTM Ultimate Restorative (LU), 3M ESPE; Brilliant Crios (BC), COLTENE and CerasmartTM (CS), GC Dental Product. The three types of resin-based composite CAD/CAM materials were physically and mechanically tested under two conditions: directly as received by the manufacturer (AR) and after storage under immersion in artificial saliva (AS) for 30 days. A global approximation to microstructure and mechanical behaviour was evaluated: density, hardness and nanohardness, nanoelastic modulus, flexural strength, fracture toughness, fracture surfaces, and microstructures and fractography. Moreover, their structural and chemical composition using X-ray fluorescence analysis (XRF) and field emission scanning electron microscopy (FESEM) were investigated. As a result, LU exhibited slightly higher mechanical properties, while the decrease of its mechanical performance after immersion in AS was doubled compared to BC and CS. Tests of pristine material showed 13 GPa elastic modulus, 150 MPa flexural strength, 1.0 MPa·m1/2 fracture toughness, and 1.0 GPa hardness for LU, 11.4 GPa elastic modulus; 140 MPa flexural strength, 1.1 MPa·m1/2 fracture toughness, and 0.8 GPa hardness for BC; and 8.3 GPa elastic modulus, 140 MPa flexural strength, 0.9 MPa·m1/2 fracture toughness, and 0.7 GPa hardness for CS. These values were significantly reduced after one month of immersion in saliva. The interpretation of the mechanical results could suggest, in general, a better behaviour of LU compared with the other two despite it having the coarsest microstructure of the three studied materials. The saliva effect in the three materials was critically relevant for clinical use and must be considered when choosing the best solution for the restoration to be used.

1 October 2021 in Fusion Engineering and Design
Verified
Journal Article
Open access
STSandra Tarancón
Sandra Tarancón
ETElena Tejado
Elena Tejado
MRM. Richou
M. Richou
JPJ.Y. Pastor
J.Y. Pastor

24 December 2022 in Polymers
Verified
Journal Article
Open access
PDF file
JOJaime Orellana-Barrasa
Jaime Orellana-Barrasa
STSandra Tarancón
Sandra Tarancón
Jose Ygnacio PastorJose Ygnacio Pastor
Jose Ygnacio Pastor
The effects of post-treatment temperature-based methods for accelerating the ageing of PLA were studied on 1D single-PLA filaments after fused filament fabrication (FFF). The goal was to answer the questions whether the PLA can be safely aged—i.e., without degrading—at higher temperatures; at which temperatures, if any; how long it takes for the PLA to fully age at the chosen temperature; and which are the main differences between the material aged at room temperature and the material aged at higher temperatures. We also share other helpful information found. The use of 1D filaments allows for decoupling the variables related to the 3D structure (layer height, raster angle, infill density, and layers adhesion) from the variables solely related to the material (here, we analysed the molecular weight, the molecular orientation, and the crystallinity). 1D PLA filaments were aged at 20, 39, 42, 51, 65, 75, and 80 °C in a water-bath-inspired process in which the hydrolytic degradation of the PLA was minimised for the ageing temperatures of interest. Those temperatures were selected based on a differential scanning calorimetry (DSC) scan of the PLA right after it was printed in order to study the most effective ageing temperature, 39 °C, and highlight possible degradation mechanisms during ageing. The evolution of the thermal and mechanical properties of the PLA filaments at different temperatures was recorded and compared with those of the material aged at room temperature. A DSC scan was used to evaluate the thermal and physical properties, in which the glass transition, enthalpic relaxation, crystallisation, and melting reactions were analysed. A double glass transition was found, and its potential implications for the scientific community are discussed. Tensile tests were performed to evaluate the tensile strength and elastic modulus. The flow-induced molecular orientation, the degradation, the logistic fitting, and the so-called summer effect—the stabilisation of properties at higher values when aged at higher temperatures—are discussed to assess the safety of accelerating the ageing rate and the differences between the materials aged at different temperatures. It was found that the PLA aged at 39 °C (1) reached almost stable properties with just one day of ageing, i.e., the ageing rate accelerated by 875% for the elastic modulus and by 1635% for the yield strength; (2) the stable properties were higher than those from the PLA aged at room temperature; and (3) no signs of degradation were identified for the ageing temperature of interest.

1 January 2020 in Materials Science and Engineering: A
Verified
Journal Article
Closed access
SNSaša Novak
Saša Novak
MKMatej Kocen
Matej Kocen
AZAndreja Šestan Zavašnik
Andreja Šestan Zavašnik
AGAndrei Galatanu
Andrei Galatanu
MGMagdalena Galatanu
Magdalena Galatanu
PJPetra Jenuš
Petra Jenuš