The creep resistance of single-crystalline Ni-base superalloys at elevated temperatures depends among others on solid solution strengthening of theγ-matrix. To study the influence of various solid solution strengtheners on the mechanical properties, a series of Ni-base superalloys with the same content of different alloying elements (Ir, Mo, Re, Rh, Ru, W) or element combinations (MoW, ReMo, ReW) was investigated. Nanoindentation measurements were performed to correlate the partitioning behavior of the solid solution strengtheners with the hardness of the individual phases. The lowestγ′/γ-hardness ratio was observed for the Re-containing alloy with the strongest partitioning of Re to theγ-matrix. As a result of the creep experiments in the high-temperature/low-stress regime (1373 K (1100 °C)/140 MPa), it can be concluded that solid solution hardening in theγ-phase plays an essential role. The stronger the partitioning to theγ-phase and the lower the interdiffusion coefficient of the alloying element, the better the creep resistance. Therefore, the best creep behavior is found for alloys containing high contents of slow-diffusing elements that partition preferably to theγ-phase, particularly Re followed by W and Mo.
The creep strength of single-crystalline Co-based superalloys was found to be comparable to first-generation Ni-base superalloys. However, considerable shearing of the γ′ precipitates was observed in the early creep stages. To determine the strengthening contribution of the Ta-containing γ′-Co3(Al,W) precipitates, the creep strength of several single-crystalline Co-Al-W-Ta superalloys was determined as a function of the γ′ volume fraction at 1223 K (950 °C) and stress levels between 25 and 600 MPa. Employing a Lagneborg–Bergman–Reppich (LBR) approach, it is found that the strengthening contribution of the γ′ precipitates increases significantly with increasing γ′ volume fraction. In a Co-base superalloy that exhibits a precipitate volume fraction of about 70 pct, the γ′-strengthening contribution calculated with the LBR approach ranges between the ones observed in first-generation Ni-base superalloy CMSX-6 and second-generation Ni-base superalloy CMSX-4.
Pushing the maximum service temperature of aircraft engines and industrial gas turbines is the major pathway to improve their energy efficiency and reduce CO2 emissions. This maximum is mostly limited by the temperature capability of key-component materials, including superalloys. In this alloy class, segregation of elements facilitates plastic deformation and is generally considered to cause softening during high-temperature deformation. Here, we show that segregation-assisted processes can also lead to strengthening and induce an anomalous increase of the yield strength. Atomic-resolution transmission electron microscopy and density functional theory calculations reveal a segregation-assisted dissociation process of dislocations at precipitate-matrix interfaces in combination with atomic-scale reordering processes. These processes lead to an inhibition of athermal deformation mechanisms and a transition to stacking fault shearing, which causes the strengthening effect. Unraveling these elementary mechanisms might guide a mechanism-based alloy design of future superalloys with enhanced high-temperature capabilities.