Coarse primary and eutectic Mg2Si phases were generally precipitated in Mg-Al-Si alloys during solidification at a low cooling rate, which tends to deteriorate the strength and ductility of magnesium alloys due to stress concentration. Different volume fractions of TiB2 nanoparticles (1%, 3%, and 5%) were added to an Mg-4Al-1.5Si alloy to refine the coarse Mg2Si phases based on a heterogeneous nucleation mechanism. The nanoparticles were incorporated and dispersed in the molten Mg alloys and by using semi-solid stirring followed by ultrasonic treatment (SSUT), and TiB2/Mg-4Al-1.5Si composites were obtained. The effect of TiB2 content on the microstructure and mechanical properties of the composites was studied. The results showed that the average size of primary Mg2Si phases and α-Mg grains decreased as the TiB2 content raised, the dendritic primary Mg2Si phases were refined into polygonal shapes with smaller sizes, and the refined primary Mg2Si phases were uniformly distributed in the alloys after adding 1 vol.% or 3 vol.% TiB2 nanoparticles. As the TiB2 content increased, the morphology of the eutectic Mg2Si phases was modified from coarse Chinese characters to short rod or fine dot shapes. Vickers hardness and yield strength of the composites reached a maximum (153 HV and 90.9 MPa, respectively) when TiB2 content was 5 vol.%, while the most superior ultimate tensile strength (142.4 MPa) and elongation (9.2%) were obtained when TiB2 content was 3 vol.%, which were improved by 173.2%, 31.5%, 69.8%, and 187.5%, respectively compared with the Mg-4Al-1.5Si alloys.
1 May 2020 in IOP Conference Series: Materials Science and Engineering
In order to investigate the effect of distortion energy on the microstructure of magnesium alloys prepared by strain induced melt activation (SIMA) process and partial remelting, Mg-6Al-0.9Gd magnesium alloys were deformed at 200 °C with 0-20% compression ratios, and the relationship between deformation and eutectic melting activation energy was established based on differential scanning calorimetry (DSC) analysis, thereby determining the distortion energy at different compression ratios. The results showed that distortion energy increased with increasing compression ratio, which contributed to the morphological transition from dentrictic to equiaxed structure, and accelerated the formation of liquid phase during subsequent partial remelting. All things (grain size, liquid fraction and distribution in the semi-solid microstructure) considered, the optimal compression ratio for this paper was 20%.
The microstructure evolution and creep fracture mechanism of Al2O3f/Mg-6Al-0.5Nd-1Gd at different creep stages have been investigated by high temperature creep apparatus, X-ray diffraction analysis, and scanning electron microscopy. The results show that the composite is composed of α-Mg, β-Mg17Al12, Al2O3, Mg2Si, Al2Nd, and Al2Gd. MgO was generated on the fiber surface as a transition layer. According to the creep test results, the composites are suitable for working conditions below 110 MPa at 200 °C. The creep fracture mode of the composites depends on the interfacial bonding conditions between the matrix alloy and fiber, and the fracture mechanism is a combination of interfacial debonding and fiber fracture.