In this review, we present an extensive summary of research on superhydrophobic electrodeposits reported in the literature over the past decade. As a synthesis technique, electrodeposition is a simple and scalable process to produce non-wetting metal surfaces. There are three main categories of superhydrophobic surfaces made by electrodeposition: (i) electrodeposits that are inherently non-wetting due to hierarchical roughness generated from the process; (ii) electrodeposits with plated surface roughness that are further modified with low surface energy material; (iii) composite electrodeposits with co-deposited inert and hydrophobic particles. A recently developed strategy to improve the durability during the application of superhydrophobic electrodeposits by controlling the microstructure of the metal matrix and the co-deposition of hydrophobic ceramic particles will also be addressed.
Controlling the wetting property of ceramics, which is characterized by their water contact angles (WCAs), is of great interest because of their better thermal and chemical robustness compared with polymer materials. Among many ceramics, rare earth oxides (REOs) have attracted attention because of their high WCA (∼115°). Although several non-wetting mechanisms of REOs have been proposed thus far, the intrinsic mechanism has not been clarified yet due to the lack of information on crystallographic orientation–surface energy (SE)–WCA relationships. Here we report the WCA of (001), (110), and (111) oriented REO epitaxial films, which have different surface energies. We found that the WCA of fresh REO epitaxial film surfaces, which were prepared using a pulsed laser deposition technique, strongly depends on the crystallographic orientations, WCA(111) > WCA(110) > WCA(001), which reflects the differences in surface energy; SE(111) < SE(110) < SE(001). Moreover, we found that the WCA on REOs increases rapidly and converges to about 80° upon exposure to ambient air, regardless of the crystallographic orientation, likely due to surface adsorption of airborne carbon species. The present finding of ‘There is a strong correlation between the crystallographic orientation, wetting property and the surface energy’ is of great importance for the understanding of the wetting properties of ceramics.
1 December 2016 in Journal of Alloys and Compounds
Corneal nano-nipple structures consisting of hexagonally arranged protrusions with diameters around 200 nm have long been known for their antireflection capability and have served as biological blueprint for solar cell, optical lens and other surface designs. However, little is known about the global arrangement of these nipples on the ommatidial surface and their growth during the eye development. This study provides new insights based on the analysis of nano-nipple arrangements on the mesoscale across entire ommatidia, which has never been done before. The most important feature in the nipple structures are topological 5- and 7-fold coordination defects, which align to form dislocations and interconnected networks of grain boundaries that divide the ommatidia into crystalline domains in different orientations. Furthermore, the domain size distribution might be log-normal, and the domains demonstrate no preference in crystal orientation. Both observations suggest that the nipple growth process may be similar to the nucleation and growth mechanisms during the formation of other crystal structures. Our results are also consistent with the most recently proposed Turing-type reaction-diffusion process. In fact, we were able to produce the key structural characteristics of the nipple arrangements using Turing analysis from the nucleation to the final structure development.