Geopolymer refers to a large group of nanoporous, nanoparticulate materials that are synthesized by dissolution and polycondensation of aluminosilicates in basic solutions and can be made from a variety of starting materials, such as industrial waste ash, volcanic rock, or calcined clay. Geopolymers are X‐ray amorphous, corrosion resistant, refractory, and made at ambient temperature and pressure similar to cements. In this study, potassium metakaolin‐based geopolymer (KGP) composites containing alumina platelets and glass frit were fabricated, and the impact of heating temperature, dwell time, and heating/cooling rate on the microstructure was studied. The composites, heat treated up to 900°C for up to 20 h using heating/cooling rates of up to 1°C/min, showed that the addition of alumina platelets prevented major microcracking and was also able to reduce linear shrinkage. Glass frit has been shown to heal microcracks formed during KGP dehydration and crystallization. The resulting material had an open porosity of less than 1% and a uniform surface glaze of 250 μm thickness, while Oswald ripening of round closed pores occurred due to the migration of molten glass in the system.
Geopolymers (GP) are a class of X-ray amorphous, nanoporous, nanoparticulate materials that can be mixed, poured, and cured under ambient conditions. Typically, geopolymers are made using a Group 1 (G1) alkali activator such as sodium or potassium metasilicate and an aluminosilicate precursor. An analogous material to GPs is ordinary Portland cement because of the similarities in processing, however, the resulting microstructure is more similar to that of a glass. Geopolymers are more thermally stable than OPC and can therefore be used in a variety of thermal energy storage systems, as energy storage is an increasing global concern. In this study, potassium metakaolin-based geopolymer composites containing glass particles and alumina platelets were manufactured, heated in air, and exposed to molten sodium chloride or potassium chloride under an air atmosphere. Results showed the formation of an amorphous self-healing geopolymer composite (ASH-G) that could contain molten G1 chlorides for over 200 h without signs of macro or microscopic chemical degradation. The filling of cracks by glass particles in the composite after heating to 850 °C makes this material self-healing. It was found that the morphology of ASH-G composites was more affected by temperature and duration than contact with corrosive molten chlorides in air. Future works include investigating the effect of molten salt on mechanical properties during initial heating, after prolonged heating, and the material compatibility with other molten Group 1 chloride eutectics.
8 April 2024 in International Journal of Applied Ceramic Technology
The objective of this project was to further develop new composites and a testing program for the performance‐based specification for natural Amazonian geopolymer (GP) for use in ceramics and construction. While fly ash‐based alkali activated materials are now an established technology, metakaolin‐based GPs still need to be developed and optimized regarding the knowledge of the specific characteristics and properties of local resources. Amazonian kaolin was calcined into metakaolin (AMK). AMK particle size reduction for better reactive material was evaluated by means of dry and wet ball milling and sieving. Three types of metakaolin were analyzed for particle size distribution, and their size d50 ranged from 7.9 to 2.8 µm. Further GP characterization followed physical and mechanical properties in flexural strength tests. In addition, scanning electron microscopy and energy dispersive spectroscopy were used to investigate the microstructure of the materials. Energy dispersive X‐ray fluorescence was used to measure the GP material composition. Analysis of the results revealed that the strength and stiffness of sodium–metakaolin‐based GP were inversely proportional to particle size. All distinct particle size GPs showed, in general, some increase in strength and stiffness within curing times ranging from 3 to 28 days.
1 September 2021 in Chemical Thermodynamics and Thermal Analysis