3 May 2025 in Materials and Structures
The need for sustainable and high-performance construction materials has led to the development of novel geopolymer matrices. This project aims to create an optimized, highly reactive, metakaolin-based geopolymer matrix for sustainable construction materials. The study involved mixing and optimizing commercial alkali silicates and metakaolin to enhance strength, stability, and durability. The goal was to maximize the flexural strength of the geopolymer matrix using one type of commercial metakaolin (MK), seven commercial waterglass formulations with varying water content, and a single, low-energy geopolymer processing method. The findings show that geopolymer matrices with charge-balancing potassium ions and 11 mol of water, and two formulations with charge-balancing sodium ions and 13 mol of water, resulted in the highest strengths (5.9–7.7–8.1 MPa on average), lower porosity, and reduced thermal degradation. These findings have practical applications in reducing the environmental impact of traditional construction materials. By utilizing metakaolin and commercial alkali silicates, the research enhances the mechanical properties of the geopolymer and promotes the use of industrial by-products. The low-energy processing method aligns with sustainability principles by minimizing energy consumption. The resulting geopolymer composites exhibit superior strength, durability, and thermal resistance, making them suitable for sustainable ceramics and construction materials. This research contributes to the development of eco-friendly construction solutions, promoting a sustainable and resilient built environment. Its significance lies in its holistic approach to optimizing geopolymer matrices for enhanced performance and sustainability.
15 January 2019 in Advances in Materials Science and Engineering
To determine the viability of using a local resource for geopolymer synthesis, geopolymers were synthesized using metakaolin made from clay mined in the Amazonian region of Brazil. Samples were made with mixed potassium-sodium and pure sodium metakaolin-based geopolymer. Samples were also made using commercial metakaolin (CMK) from BASF, Inc. as a comparison to the Amazonian metakaolin (AMK). Scanning electron microscopy was used to investigate the microstructure of the materials. X-ray diffraction was able to confirm the formation of geopolymer. The mechanical properties of AMK material were nearly equivalent to those based on CMK. Neither CMK nor AMK reacted completely, although samples made with CMK showed less unreacted material. By increasing the mixing intensity and duration, the amount of residual unreacted material was substantially reduced, and mechanical properties were improved.
26 April 2024 in Journal of the American Ceramic Society
Experimental investigations were conducted to assess the impact of factors such as relative humidity (RH%) and the H 2 O molarity of waterglass on the efflorescence behavior of geopolymer composites. Samples with sodium (Na) and potassium (K) bases were prepared, having varying waterglass molarities (M) (at 11 and 13 moles of water). These samples were categorized into three groups exposed to different average RH ranges: (i) 0%–70% RH, (ii) 70%–90% RH, and (iii) 90%–100% RH. This study analyzed the occurrence of efflorescence and its stability, employing analytical techniques such as x‐ray diffraction, scanning electron microscopy, and energy‐dispersive spectroscopy to examine the formation and characteristics of efflorescent deposits. Additionally, mechanical testing was conducted to evaluate the compressive and flexural strengths of the geopolymer samples, considering the impact of efflorescence on their durability. For instance, in the composite geopolymer specimen containing 11 M water, at a RH of 80%, the compressive strength is decreased by approximately 25% from 56.4 to 42.3 MPa. The findings revealed that when the RH falls within the 70%–90% range, a decrease in water molar content from 13 M to 11 M leads to a more pronounced occurrence of efflorescence when compared to other conditions. Efflorescence may also occur in different RH ranges and water molarities, but its occurrence is significantly lower compared to the 70%–90% RH and 11 M water.
8 April 2024 in International Journal of Applied Ceramic Technology
The objective of this project was to further develop new composites and a testing program for the performance‐based specification for natural Amazonian geopolymer (GP) for use in ceramics and construction. While fly ash‐based alkali activated materials are now an established technology, metakaolin‐based GPs still need to be developed and optimized regarding the knowledge of the specific characteristics and properties of local resources. Amazonian kaolin was calcined into metakaolin (AMK). AMK particle size reduction for better reactive material was evaluated by means of dry and wet ball milling and sieving. Three types of metakaolin were analyzed for particle size distribution, and their size d 50 ranged from 7.9 to 2.8 µm. Further GP characterization followed physical and mechanical properties in flexural strength tests. In addition, scanning electron microscopy and energy dispersive spectroscopy were used to investigate the microstructure of the materials. Energy dispersive X‐ray fluorescence was used to measure the GP material composition. Analysis of the results revealed that the strength and stiffness of sodium–metakaolin‐based GP were inversely proportional to particle size. All distinct particle size GPs showed, in general, some increase in strength and stiffness within curing times ranging from 3 to 28 days.
26 March 2022 in International Journal of Applied Ceramic Technology
29 April 2025 in International Journal of Applied Ceramic Technology
This research targets to produce new composites from a highly reactive metakaolin‐based geopolymer matrix reinforced with natural particles for use in sustainable ceramics, building and construction. Commercial waterglass and added mineral particles were optimized for geopolymer composites to provide higher strength, stability, and durability. The design method implicated higher flexural strength of one type of commercial metakaolin, one commercial waterglass formulation, a single‐low‐energy geopolymer processing, and seven types of added mineral particles. The particulate reinforcement formulations added to the geopolymer matrix were: (1) 20 wt% chamotte and 40 wt% Prairie fine sand; (2) 20 wt% chamotte and 40 wt% Quikrete medium sand; (3) 20 wt% chamotte and 40 wt% Quikrete fine sand; (4) 20 wt% ball‐milled fine sand; (5) 20 wt% ball‐milled fine sand and 40 wt% Quikrete fine sand; (6) 20 wt% ball‐milled fine sand and 40 wt% Prairie fine sand; (7) 10 wt% ball‐milled fine sand and 50 wt% Prairie fine sand. Potassium metasilicate Kasolv 16 with 11 M of water, Metamax metakaolin, reinforced with 20 wt% ball‐milled fine sand, and 40 wt% Prairie fine sand (BF20PF40) resulted in the highest strength geopolymer composite. BF20PF40 also yielded lower mass loss, higher packing density, and better thermal stability.