In this paper, the best fixture scheme for the TIG welding torch of nickel-base solid solution superalloy GH3536 in the welding process is explored. First of all, to meet the extremely high-dimensional accuracy requirements of the flame cylinder, a multifield coupling analysis model based on the flame cylinder is established on SYSWELD software. By studying the stress and deformation of welded parts under different line constraint positions and applied pressure, the trend of welding deformation is obtained, and the relevant mathematical model is established based on this. Finally, the particle swarm optimization (PSO) algorithm is used to calculate the best fixture scheme to make the welding stress and deformation better. The simulation results show that the welding deformation is negatively related to the line constraint distance and positively related to the applied pressure. According to the optimized clamping scheme of PS0, through simulation calculation, the average axial deformation is reduced by 82.5%, the maximum radial shrinkage deformation is reduced by 60.6%, and the maximum residual stress is reduced by 60.3%. Finally, it is verified by the flame barrel experiment that it meets the acceptance requirements and successfully solves the problem of serious axial shrinkage during the TIG welding of the outer ring of the flame barrel.
The two main process parameters of Bobbin tool friction stir welding (BT-FSW) are ω (rotational speed) and v (traverse speed). Both of these factors have a significant effect on heat input, microstructure, and mechanical properties. At present, most studies on friction stir welding adopt the control variable method to study the thermal cycling during the welding process and the mechanical properties of joints, and there are few studies on changing the two process parameters at the same time, because it can be difficult to assess the correlation between heat input and mechanical properties when changing both factors at the same time. In this study, the w/v ratio is defined as the thermal index, which is a characteristic value of heat input. The study uses ABAQUS 6.5 software to establish a BT-FSW CEL (coupled Eulerian–Lagrangian) thermal coupling model. This model explores the relationship between joint thermal cycles, microstructure, and mechanical properties for different w and v values with the same w/v ratio. The results show that increasing rotational and traverse speeds under the same w/v ratio leads to an increase in the peak temperature of the nugget zone (NZ). However, the peak temperature of the thermo-mechanically affected zone (TMAZ) and heat-affected zone (HAZ) remained almost constant. Joint strength was highest at a rotational speed of 750 r/min and a traverse speed of 650 mm/min, with a yield strength of 227 MPa. As rotational and traverse speeds increased, the recrystallized grain content of the NZ showed an increasing trend followed by a decreasing trend. The recrystallized grain content of the advancing side thermo-mechanically affected zone (AS-TMAZ) and retreating side thermo-mechanically affected zone (RS-TMAZ) showed a decreasing trend. Joint hardness had a “W” shaped distribution, with the highest average hardness value found in the NZ.