Fu-hua Lin

Dr. Fu-hua Lin

orcid

Research Focus & Metrics

Academic Career Length

9Years (2018-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
18 March 2019 in Polymers
Verified
Journal Article
Open access
PDF file
Bo WangBo Wang
Bo Wang
FLFu-hua Lin
Fu-hua Lin
XLXiangyang Li
Xiangyang Li
XJXu-Ran Ji
Xu-Ran Ji
SLSi-Xiao Liu
Si-Xiao Liu
JLJun Luo
Jun Luo
Isotactic polypropylene (iPP) is a commonly used thermoplastic polymer with many excellent properties. But high brittleness, especially at low temperatures, limits the use of iPP. The presence of transcrystallization of iPP makes it possible for fiber-reinforced iPP composites with higher strength. Bacterial cellulose (BC) is a kind of cellulose with great potential to be used as a new filler to reinforce iPP due to its high crystallinity, biodegradability and efficient mechanical properties. In this study, the iPP/BC hamburger composite was prepared by a simple hot press and maleic anhydride grafted polypropylene (MAPP) was used to improve the interface compatibility of iPP and BC. The polarizing microscope (POM) photograph shows that BC successfully induces the transcrystallization of iPP. The differential Scanning Calorimeter (DSC) date proves that the addition of BC could improve the thermal properties and crystallization rate of the composite. Especially, this change is more obvious of the iPP/MAPP/BC. The mechanical properties of the iPP/BC composites were greatly increased. This DSC date is higher than BC; we used BC particles to enhance the iPP in our previous research. The scanning Electron Microscope (SEM) analysis intuitively shows that the interface of the iPP/MAPP/BC is more smooth and flat than the iPP/BC. The fourier Transform infrared spectroscopy (FT-IR) analysis of the iPP/BC hamburger composites was shown that a new C=O group vibration appeared at 1743 cm−1, which indicated that the hydrogen bond structure of BC molecules was weakened and some hydroxyl groups were substituted after modification which can increase the lipophilicity of BC. These results indicated that the BC fiber can easily induce the transcrystallization of iPP, which has excellent mechanical properties. Moreover, the addition of MAPP contributes greatly to the interface compatibility of iPP and BC.

18 November 2018 in Polymers
Verified
Journal Article
Open access
PDF file
Bo WangBo Wang
Bo Wang
FLFu-hua Lin
Fu-hua Lin
XLXiangyang Li
Xiangyang Li
ZZZhong-Wei Zhang
Zhong-Wei Zhang
XXXiao-Rong Xue
Xiao-Rong Xue
JLJun Luo
Jun Luo
Bacterial cellulose (BC) is a new kind of cellulose with great potential in enhancing preparation of isotactic Polypropylene (iPP) composites, which have been found with excellent performance. However, the interface compatibility between BC and iPP is poor. In this study, iPP/BC composites were prepared by solution mixing. Esterification modified BC (CO) and Maleic anhydride grafted polypropylene (MAPP) added as a compatibilizer was both used to improve the interfacial compatibility of the iPP/BC composites. The rheology and isothermal crystallization behavior of the composites was tested and discussed. The result shows that the complex viscosity and storage modulus of the composite significantly increase in the rule iPP, iPP/BC2, iPP/CO2, and M-iPP/BC3, which indicates that the compatibility of the composite increases as this rule. According to the isothermal crystallization kinetics result, the crystal growth mode of iPP was not affected by the addition of BC and the interfacial compatibility. The spherulite growth rate of the iPP/BC composite increases with increasing crystallization temperature. Especially, the value decreases as the same rule with the complex viscosity and storage modulus of the composite at the same isothermal crystallization temperature. These results suggest that the interface compatibility of iPP/BC composites is greatly improved and the interface compatibility of the M-iPP/BC3 is better than the iPP/CO2.

2 April 2018 in Polymers
Verified
Journal Article
Open access
PDF file
Bo WangBo Wang
Bo Wang
KNKai Nie
Kai Nie
XXXiao-Rong Xue
Xiao-Rong Xue
FLFu-hua Lin
Fu-hua Lin
XLXiangyang Li
Xiangyang Li
JLJun Luo
Jun Luo
Microcrystalline cellulose (MCC) offers great potential to improve the mechanical and crystallization properties of isotactic polybutene-1 (iPB) because of its low cost, biodegradability, renewability and excellent mechanical properties. However, the compatibility of polar MCC and non-polar iPB is poor. In this study, maleic anhydride grafted polybutene (MAPB) was prepared by the solution method and was used as a compatibilizer in the fabrication of iPB/MCC composites by using a twin screw extruder. The ultimate tensile strength, tensile modulus, flexural strength, flexural modulus of the iPB/MCC composites increased by 3.1%, 16.5%, 10.7%, 6.5%, respectively, compared with that of pure iPB. With MAPB addition, these values increased by 17.2%, 31%, 17.5% and 10%, respectively, compared with that of pure iPB. The heat-distortion temperature and thermal-decomposition temperature of all composites increased with an increased MCC content. The non-isothermal crystallization of the iPB/MCC composites shows that MCC addition can promote iPB crystallization, because the non-isothermal crystallization curve of the composites moves toward a higher temperature, especially after MAPB addition. Scanning electron micrographs indicate that the compatibility of the iPB/MCC has been enhanced significantly.

2 December 2019 in Polymers
Verified
Journal Article
Open access
PDF file
Bo WangBo Wang
Bo Wang
FLFu-hua Lin
Fu-hua Lin
YZYu-Ying Zhao
Yu-Ying Zhao
XLXiangyang Li
Xiangyang Li
YLYan-Chao Liu
Yan-Chao Liu
YWYing-Hui Wei
Ying-Hui Wei
Isotactic polybutylene-1 (iPB) has lots of advantages and is best used as hot water pipe. However, to transform into stable crystal form I, the iPB needs as long as 7 days. In this process, the irreversible damage brings great difficulties to the use of the iPB. The method which convert it directly into crystal I has shortcomings such as being requiring complex operation and being expensive. In this study, an innovative idea was put forward, not paying attention to the crystal transformation of iPB but only focusing on reducing the time it can be applied. In this study, bamboo powder was modified by the silane coupling agent KH570 (KBP) to prepare iPB/KBP composite. The infiltration test and Fourier transform infrared (FTIR) analysis showed that the hydrophilicity of KBP is greatly reduced, which can greatly improve the compatibility of the iPB and KBP. The tensile strength, tensile modulus, flexural strength, and flexural modulus of the composites storage for 3 days is equal to the pure iPB with storage 7 days with the KBP additions of 3%, 3%, 7%, and 5%, respectively. The heat deformation temperature (HDT) of the composite with 3% KBP after 1-day storage reached the value of pure iPB storage for 7 days. This provides more space and possibilities for the industrialization of the iPB. The crystallization behavior of iPB/KBP composites proves that the addition of KBP accelerates the crystallization rate of iPB, but the crystallinity of the iPB/KBP composites is not changed. The SEM photograph of iPB/KBP composites showed that when the KBP addition was low the compatibility between KBP and iPB was good. When the KBP addition was increased the agglomeration of KBP in the iPB was very obvious, which leads to the poor mechanical properties of the composite.

13 September 2022 in Polymers
Verified
Journal Article
Open access
PDF file
SMShuangdan Mao
Shuangdan Mao
MZMi Zhang
Mi Zhang
FLFu-hua Lin
Fu-hua Lin
XLXiangyang Li
Xiangyang Li
YZYu-Ying Zhao
Yu-Ying Zhao
Bo WangBo Wang
Bo Wang
Isotactic polybutene (iPB) has a wide application in the water pipe field. However, the most valuable form I, needs 7 days to complete the transformation. In this study, the attapulgite (ATP), which produces lattice matching of the iPB form I, was selected to prepare an iPB/ATP composite. The Fischer–Tropsch wax (FTW) was grafted with maleic anhydride to obtain MAFT, and the ATP structure was reset by reactions with MAFT to the prepared FATP, which improved the interface compatibility of the ATP and iPB. The Fourier transform infrared spectroscopy (FT-IR) and the water contact angle test confirmed the successful synthesis of FATP. X-ray diffraction (XRD) verified that the graft of MAFT did not affect the crystal structure of ATP. The iPB + 5% FATP had the maximum flexural strength, which was 12.45 Mpa, and the flexural strength of the iPB + 5% FATP annealing for 1 day was much higher than others. Scanning electron microscope (SEM) photographs verified that FATP and iPB had good interface compatibility. The crystal transformation behavior indicated that the iPB + 5% FATP had the fastest crystal transformation rate, which proved that the reset structure, ATP, greatly accelerated the crystal transformation of iPB. This was a detailed study on the effect of lattice matching, interfacial compatibility and internal lubrication of the reset structure, ATP, in the nucleation and growth stages of iPB form I. The result was verified by XRD, differential scanning calorimetry (DSC), Avrami kinetics and polarizing microscope (POM) analysis.

19 May 2021 in Polymers
Verified
Journal Article
Open access
PDF file
Bo WangBo Wang
Bo Wang
SMShuangdan Mao
Shuangdan Mao
FLFu-hua Lin
Fu-hua Lin
MZMi Zhang
Mi Zhang
YZYuying Zhao
Yuying Zhao
JLJun Luo
Jun Luo
Isotactic poly (1-butene) (iPB) has excellent properties which are recognized as a green and energy saving product. However, the most stable and valuable crystal form I had a spontaneous transformation that took as long as seven days to complete. As a special solid waste, the herb residue (HR) is rich in cellulose which has great potential to accelerate the crystal transformation of the iPB. However, the polarity of HR results in the interface compatibility with non-polar iPB. In this study, the HR was modified by silane coupling agent (KH570) to obtain KHR and the iPB/HR composite was prepared. The FTIR spectrum was indicated that the organic functional groups of KH570 successfully graft onto the surface of HR and the water contact angle test was indicated that the hydrophilicity of the KHR was greatly decreased. The complete crystal transformation time is 7 days for iPB, 6 days for iPB+5% HR but only 3 days for iPB+5% KHR. The addition of the HR and KHR improve the thermal stability of the composite and this beneficial effect is more obvious for KHR. After annealing for 5 days, the physical properties value include tensile strength, flexural strength, and HDT of iPB+5% HR reach that of pure iPB after annealing for 7 days, but only 3 days for iPB+5% KHR. The TG analysis and SEM photographs give clear evidence that the beneficial effect of KH570 modified HR on improving the interface compatibility with iPB.