FeCo thin films with high saturation magnetization (4 πMs) can be applied in high-frequency electronic devices such as thin film inductors and microwave noise suppressors. However, due to its large magnetocrystalline anisotropy constant and magnetostrictive coefficient of FeCo, the coercivity (Hc) of FeCo films is generally high, which is detrimental to the soft magnetic properties. Meanwhile, the thickness and deposition temperature have significant effects on the coercivity and saturation magnetization of FeCo films. In this paper, FeCo thin films with different thicknesses were prepared by magnetron sputtering at different temperatures. The effects of thickness and deposition temperature on the microstructure and magnetic properties of FeCo thin films were systematically studied. When the film thickness increases from 50 nm to 800 nm, the coercivity would decrease from 309 Oe to 160 Oe. However, the saturation magnetization decreases from 22.1 kG to 15.3 kG. After that, we try to further increase the deposition temperature from room temperature (RT) to 475 °C. It is intriguing to find that the coercivity greatly decreased from 160 Oe to 3 Oe (decreased by 98%), and the saturation magnetization increased from 15.3 kG to 23.5 kG (increased by 53%) for the film with thickness of 800 nm. For the film with thickness of 50 nm, the coercivity also greatly decreased from 309 Oe to 10 Oe (decreased by 96%), but the saturation magnetization did not change significantly. It is contributed to the increase of deposition temperature, which will lead to the increase of grain size and the decrease of the number of grain boundaries. And the coercivity decreases as the number of grain boundaries decreases. Meanwhile, for the thicker films, when increasing the deposition temperature the thermal stress increases, which changes the appearance of (200) texture, and the saturation magnetization increases. Whereas, it has a negligible effect on the orientation of thin films with small thickness (50 nm). This indicates that high-temperature deposition is beneficial to the soft magnetic properties of FeCo thin films, particularly for the films with larger thickness. This FeCo thin film with high saturation magnetization and low coercivity could be an ideal candidate for high-frequency electronic devices.
In order to improve the magnetocaloric properties of MnNiSi-based alloys, a new type of high-entropy magnetocaloric alloy was constructed. In this work, Mn0.6Ni1−xSi0.62Fe0.4CoxGe0.38 (x = 0.4, 0.45, and 0.5) are found to exhibit magnetostructural first-order phase transitions from high-temperature Ni2In-type phases to low-temperature TiNiSi-type phases so that the alloys can achieve giant magnetocaloric effects. We investigate why chexagonal/ahexagonal (chexa/ahexa) gradually increases upon Co substitution, while phase transition temperature (Ttr) and isothermal magnetic entropy change (ΔSM) tend to gradually decrease. In particular, the x = 0.4 alloy with remarkable magnetocaloric properties is obtained by tuning Co/Ni, which shows a giant entropy change of 48.5 J∙kg−1K−1 at 309 K for 5 T and an adiabatic temperature change (ΔTad) of 8.6 K at 306.5 K. Moreover, the x = 0.55 HEA shows great hardness and compressive strength with values of 552 HV2 and 267 MPa, respectively, indicating that the mechanical properties undergo an effective enhancement. The large ΔSM and ΔTad may enable the MnNiSi-based HEAs to become a potential commercialized magnetocaloric material.
5 July 2022 in Journal of Thermal Spray Technology
Copper (Cu), Nitrogen (N) Co-doped diamond-like carbon ((Cu:N)-DLC) films and Cu doped DLC (Cu-DLC) films were fabricated by high power impulse magnetron sputtering technique (HiPIMS). The influence of copper and nitrogen incorporation on the microstructure and electrochemical properties of Cu-DLC and (Cu:N)-DLC films were investigated by X-ray photoelectron spectroscopy, raman spectra and electrochemical workstation. The surface of all the films is cauliflower-like clusters, no obvious large particle Cu clusters can be observed. XRD patterns of theses films have only diffraction peak of copper and no other compounds. Raman spectra illustrate that I d /I g varies from 2.79 to 3.01 as the N contents changes. XPS results identify that Cu does not form compounds or solid solution into DLC films. Electrochemical tests show that the electrode activity gradually increases with increasing the N contents of (Cu:N)-DLC electrode. Compared with (Cu:N)-DLC electrode, Cu-DLC electrode has a faster electron transfer rate (K 0 is 1.88 × 10 −2 cms −1 ), low transfer resistance (227.0 Ωcm 2 ), and a higher electrochemical activity (ΔEp is 93 mV). Consequently, the electrochemical properties of Cu doped DLC films are better than that of Cu, N co-doped DLC films.