30 April 2015 in Optical Materials Express
Verified
Journal Article
Open access
PDF file
FYFei-Peng Yu
Fei-Peng Yu
SOSin-Liang Ou
Sin-Liang Ou
Dong-Sing WuuDong-Sing Wuu
Dong-Sing Wuu
Monoclinic gallium oxide thin films were grown on (0001) sapphire at various substrate temperatures ranging from 400 to 1000 °C by pulsed laser deposition using a KrF excimer laser. The structural, optical and compositional properties of the films were analyzed by using x-ray diffraction, transmission electron microscopy, optical transmittance, and Rutherford backscattering spectroscopy. As the substrate temperature was increased to 800 °C, the gallium oxide film possesses single crystalline phase with a preferred growth orientation of (−201) plane and higher crystal quality than those at the other temperatures. Optical transmittance measurements reveal the films grown at 600-1000 °C exhibit a clear absorption edge at the deep ultraviolet region around 250 nm wavelength. Based on the results of Rutherford backscattering spectroscopy, the O/Ga ratio of gallium oxide film increased gradually with increasing substrate temperature. When the substrate temperature was raised to 800-1000 °C, the film composition was close to the formation of Ga2O3, indicating the O vacancies and defects were reduced. Furthermore, the films grown at 600 and 800 °C were chosen to fabricate solar-blind metal-semiconductor-metal photodetectors. At an applied bias of 5 V, the photodetector prepared with 800 °C-grown film has a lower dark current of 1.2 × 10−11 A and a higher responsivity of 0.903 A/W (at a wavelength of 250 nm) than those with 600 °C-grown films. The better device performance is ascribed to the higher crystal quality and fewer O vacancies in the 800 °C-grown film. Moreover, the results indicate the gallium oxide films presented in this study have high potential for deep ultraviolet photodetector applications.

24 May 2005 in Applied Physics Letters
Verified
Journal Article
Closed access
PDF file
Ray-Hua HorngRay-Hua Horng
Ray-Hua Horng
CYC. C. Yang
C. C. Yang
JWJ. Y. Wu
J. Y. Wu
SHS. H. Huang
S. H. Huang
CLC. E. Lee
C. E. Lee
Dong-Sing WuuDong-Sing Wuu
Dong-Sing Wuu
There is a significant gap between the internal and external efficiencies of conventional GaN light-emitting diodes (LEDs). The reason for this shortfall is the narrow escape cone for light in high refractive index semiconductors. In this letter, the p -side-up GaN∕sapphire LEDs with surface textured indium tin oxide (ITO) widow layers were investigated using natural lithography with polystyrene spheres as the etching mask. Under optimum etching conditions, the surface roughness of the ITO film can reach 140 nm while the polystyrene sphere on the textured ITO surface is maintained at about 250–300 nm in diameter. The output power of the ITO∕GaN LED with and without surface texturing is 10.9, and 8.5 mW at 20 mA, respectively. The LEDs fabricated using the surface-textured ITO produced an output power that exceeded that of the planar-surface LED by about 28% at 20 mA.

16 October 2006 in Applied Physics Letters
Verified
Journal Article
Closed access
Dong-Sing WuuDong-Sing Wuu
Dong-Sing Wuu
WWW. K. Wang
W. K. Wang
KWK. S. Wen
K. S. Wen
SHS. C. Huang
S. C. Huang
SLS. H. Lin
S. H. Lin
Ray-Hua HorngRay-Hua Horng
Ray-Hua Horng
An approach to improve the defect density and internal quantum efficiency of near-ultraviolet emitters was proposed using a combination of epitaxial lateral overgrowth (ELOG) and patterned sapphire substrate (PSS) techniques. Especially, a complementary dot array pattern corresponding to the underlying PSS was used for the ELOG - Si O 2 mask design. Based on the transmission-electron-microscopy and etch-pit-density results, the ELOG ∕ Si O 2 ∕ Ga N ∕ PSS structure can reduce the defect density to a level of 10 5 cm − 2 . The internal quantum efficiency of the InGaN-based ELOG-PSS light-emitting diode(LED) sample showed three times in magnitude as compared with that of the conventional GaN/sapphire one. Under a 20 mA injection current, the output powers of ELOG-PSS, PSS, and conventional LED samples were measured to be 3.3, 2.9, and 2.5 mW , respectively. The enhanced output power could be due to a combination of the reduction in dislocation density (by ELOG) and improved light extraction efficiency (by PSS). Unlike the previous double ELOG approaches, the presented ELOG-PSS structure needs only one regrowth process and will have high potential in future high-quality ultraviolet emitters, even blue/green laser diode applications.

25 January 2022 in Scientific Reports
Verified
Journal Article
Open access
PDF file
Ray-Hua HorngRay-Hua Horng
Ray-Hua Horng
CYChun-Xin Ye
Chun-Xin Ye
PCPo-Wei Chen
Po-Wei Chen
DIDaisuke Iida
Daisuke Iida
KOKazuhiro Ohkawa
Kazuhiro Ohkawa
Dong-Sing WuuDong-Sing Wuu
Dong-Sing Wuu
In this research, five sizes (100 × 100, 75 × 75, 50 × 50, 25 × 25, 10 × 10 µm2) of InGaN red micro-light emitting diode (LED) dies are produced using laser-based direct writing and maskless technology. It is observed that with increasing injection current, the smaller the size of the micro-LED, the more obvious the blue shift of the emission wavelength. When the injection current is increased from 0.1 to 1 mA, the emission wavelength of the 10 × 10 μm2 micro-LED is shifted from 617.15 to 576.87 nm. The obvious blue shift is attributed to the stress release and high current density injection. Moreover, the output power density is very similar for smaller chip micro-LEDs at the same injection current density. This behavior is different from AlGaInP micro-LEDs. The sidewall defect is more easily repaired by passivation, which is similar to the behavior of blue micro-LEDs. The results indicate that the red InGaN epilayer structure provides an opportunity to realize the full color LEDs fabricated by GaN-based LEDs.

18 June 2018 in Scientific Reports
Verified
Journal Article
Open access
PDF file
WPWu-Chang Peng
Wu-Chang Peng
YCYao-Ching Chen
Yao-Ching Chen
JHJu-Liang He
Ju-Liang He
SOSin-Liang Ou
Sin-Liang Ou
Ray-Hua HorngRay-Hua Horng
Ray-Hua Horng
Dong-Sing WuuDong-Sing Wuu
Dong-Sing Wuu
To acquire device-quality TiOx films usually needs high-temperature growth or additional post-thermal treatment. However, both processes make it very difficult to form the p-type TiOx even under oxygen-poor growth condition. With the aid of high energy generated by high power impulse magnetron sputtering (HIPIMS), a highly stable p-type TiOx film with good quality can be achieved. In this research, by varying the oxygen flow rate, p-type γ-TiO and n-type TiO2 films were both prepared by HIPIMS. Furthermore, p- and n-type thin film transistors employing γ-TiO and TiO2 as channel layers possess the field-effect carrier mobilities of 0.2 and 0.7 cm2/Vs, while their on/off current ratios are 1.7 × 104 and 2.5 × 105, respectively. The first presented p-type γ-TiO TFT is a major breakthrough for fabricating the TiOx-based p-n combinational devices. Additionally, our work also confirms HIPIMS offers the possibility of growing both p- and n-type conductive oxides, significantly expanding the practical usage of this technique.

1 January 2006 in Journal of the Electrochemical Society
Verified
Journal Article
Closed access
PDF file
Dong-Sing WuuDong-Sing Wuu
Dong-Sing Wuu
WWW. K. Wang
W. K. Wang
KWK. S. Wen
K. S. Wen
SHS. C. Huang
S. C. Huang
SLS. H. Lin
S. H. Lin
MPM. H. Pan
M. H. Pan
In this study, a wet-etched pyramidal patterned sapphire substrate (PSS) was used to fabricate the near-ultraviolet InGaN-based light-emitting diodes (LEDs). The pyramidal PSS was etched using a <mml:math display="inline"><mml:mrow><mml:mn>3</mml:mn><mml:msub><mml:mi mathvariant="normal">H</mml:mi><mml:mrow><mml:mn>2</mml:mn></mml:mrow></mml:msub><mml:mi mathvariant="normal">S</mml:mi><mml:msub><mml:mi mathvariant="normal">O</mml:mi><mml:mrow><mml:mn>4</mml:mn></mml:mrow></mml:msub><mml:mo>:</mml:mo><mml:mn>1</mml:mn><mml:msub><mml:mi mathvariant="normal">H</mml:mi><mml:mrow><mml:mn>3</mml:mn></mml:mrow></mml:msub><mml:mi mathvariant="normal">P</mml:mi><mml:msub><mml:mi mathvariant="normal">O</mml:mi><mml:mrow><mml:mn>4</mml:mn></mml:mrow></mml:msub></mml:mrow></mml:math>3H2SO4:1H3PO4 mixture solution and the activation energy of this reaction is determined to be <mml:math display="inline"><mml:mrow><mml:mn>28.2</mml:mn><mml:mspace width="0.3em"></mml:mspace><mml:mi>kcal</mml:mi><mml:mo>∕</mml:mo><mml:mi>mol</mml:mi></mml:mrow></mml:math>28.2kcal∕mol . Three symmetric sidewall facets of the etched pyramidal hole were <mml:math display="inline"><mml:mrow><mml:mo>{</mml:mo><mml:mn>11</mml:mn><mml:mover accent="true"><mml:mrow><mml:mn>2</mml:mn></mml:mrow><mml:mo stretchy="false">¯</mml:mo></mml:mover><mml:mover accent="true"><mml:mi>k</mml:mi><mml:mo stretchy="false">¯</mml:mo></mml:mover><mml:mo>}</mml:mo></mml:mrow></mml:math>{112¯k¯} on the (0001) sapphire. It was found that the GaN epi layer grew laterally from the top of the pyramid pit and overhung the cavity. An evident reduction in dislocation density of the GaN-on-PSS sample can be confirmed by the etch-pit-density, double-crystal X-ray, and micro photoluminescence measurement results. Under a <mml:math display="inline"><mml:mrow><mml:mn>20</mml:mn><mml:mspace width="0.3em"></mml:mspace><mml:mi>mA</mml:mi></mml:mrow></mml:math>20mA forward injection current, the output power of the conventional and pyramidal PSS LEDs (in epoxy lamp form, <mml:math display="inline"><mml:mrow><mml:msub><mml:mi>λ</mml:mi><mml:mi mathvariant="normal">D</mml:mi></mml:msub><mml:mo>=</mml:mo><mml:mn>400</mml:mn><mml:mspace width="0.3em"></mml:mspace><mml:mi>nm</mml:mi></mml:mrow></mml:math>λD=400nm ) were 7.45 and <mml:math display="inline"><mml:mrow><mml:mn>9.35</mml:mn><mml:mspace width="0.3em"></mml:mspace><mml:mi>mW</mml:mi></mml:mrow></mml:math>9.35mW , respectively. A 25% enhancement in output power was achieved in the pyramidal PSS LED as compared with that of the conventional LED sample. The enhanced output power is not only due to the improvement of the internal quantum efficiency upon decreasing the dislocation density, but also due to the enhancement of the extraction efficiency using a pyramidal PSS. From light-tracing calculation, the pyramidal reflector arrays can offer more probability of escaping photons from the GaN/sapphire interface, resulting in an increase in light extracting efficiency.