In order to build green mines, goaf is often filled, supported, and sealed with a high-water material to eliminate a series of environmental problems and safety hazards caused by goaf. In this study, ordinary Portland cement, sulphoaluminate cement, and alkali-activated cement were used as binders to prepare full-tailings high-water materials for filling, with various water-to-cement ratios. The compressive strength development of consolidated tungsten tailings specimens prepared with various curing binders was observed, and the influence of various water–cement ratios on the strength development was analyzed. The environmental impact of mine backfill materials was assessed according to the life cycle theory (LCA), and these mine backfill materials were prepared by using various binders. The results show that when the water-to-binder ratio is 3, the strength of alkali-activated cement can reach 3 MPa at 28 days; at that ratio, the microstructure of alkali-activated cement is more compact. Through LCA analysis, the environmental load of alkali-activated cement is shown to be significantly lower than that of either Portland cement or sulphoaluminate cement; the LCA results show that the primary energy consumption using alkali-activated cement is reduced from the Portland and sulphoaluminate cements by 1319.32 MJ and 945 kg, respectively. These unusual reduction percentages are achieved because the production of alkali-activated cement by LCA does not have any negative environmental impact—the production of alkali-activated cement, with its primary component being industrial byproduct slag, so that the use of alkali-activated cement in tailings’ consolidation has a positive environmental impact.
Magnesium phosphate cement (MPC) has gained attention in specialized construction applications due to its rapid setting and high early strength, though its inherent brittleness limits structural performance. This study developed an innovative toughening strategy through synergistic reinforcement using hybrid fibers and carbon fiber-reinforced polymer (CFRP) fabric capable of multi-scale crack control. The experimental program systematically evaluated the hybrid fiber system, dosage, and CFRP positioning effects through mechanical testing of 7-day cured specimens. The results indicated that 3.5% fiber dosage optimized flexural–compressive balance (45% flexural gain with 0.38). The developed composite system reduced brittleness through effective crack suppression across scales, confirming its capability to transform fracture behavior from brittle to quasi-ductile. This work advances MPC’s engineering applicability by resolving its mechanical limitations through rationally designed composite systems, with particular relevance to rapid repair scenarios requiring both early strength and damage tolerance, expanding its potential in specialized construction where conventional cement proves inadequate.