The densified MnZn ferrite ceramics were prepared using the cold sintering process under pressure, with an acetate ethanol solution used as the transient solvent. The effects of the transient solvent, the pressure and annealing temperature on the density, and the micromorphology and magnetic properties of the sintered MnZn ferrites were studied. The densified MnZn ferrite was obtained using the cold sintering process and its relative density reached up to 85.4%. The transient solvent and high pressure are essential to the cold sintering process for MnZn ferrite. The annealing treatment is indispensable in obtaining the sample with the higher density. The relative density was further increased to 97.2% for the sample annealed at 950 °C for 6 h. The increase in the annealing temperature reduces the power loss at high frequencies.
A new reduction–diffusion method for preparing submicron-sized Sm2Fe17N3 was developed. First, submicron-sized α-Fe/Sm2O3 composite precursors with good dispersibility were prepared directly by ultrasonic spray pyrolysis and hydrogen reduction (USP-HR). Then, the precursor was successfully converted into Sm2Fe17N3 powder by Ca reduction–diffusion and nitridation. The results displayed that the precursor prepared by USP-HR was a monodisperse homogeneous composite of spherical particles of α-Fe and Sm2O3. α-Fe and Sm2O3 exist in an intercalated structure in the composite spherical particles. This creates conditions for the preparation of ultrafine Sm2Fe17N3 particles with uniform sizes and dispersity. The results show that Sm2Fe17N3 is a single-phase, composed of submicron-sized particles with no other impurity phases. The physical property measurement system shows that the coercivity of 0.616 ± 0.347 µm particles reaches 14.7 kOe.
6 August 2024 in ACS Applied Materials & Interfaces