Wei Cai

Dr. Wei Cai

orcid

Research Focus & Metrics

Academic Career Length

7Years (2020-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
28 April 2023 in Materials
Verified
Journal Article
Open access
PDF file
YYYao Ying
Yao Ying
HHHu Linghuo Hu
Hu Linghuo Hu
ZLZhaocheng Li
Zhaocheng Li
JZJingwu Zheng
Jingwu Zheng
JYJing Yu
Jing Yu
Shenglei CheShenglei Che
Shenglei Che
The densified MnZn ferrite ceramics were prepared using the cold sintering process under pressure, with an acetate ethanol solution used as the transient solvent. The effects of the transient solvent, the pressure and annealing temperature on the density, and the micromorphology and magnetic properties of the sintered MnZn ferrites were studied. The densified MnZn ferrite was obtained using the cold sintering process and its relative density reached up to 85.4%. The transient solvent and high pressure are essential to the cold sintering process for MnZn ferrite. The annealing treatment is indispensable in obtaining the sample with the higher density. The relative density was further increased to 97.2% for the sample annealed at 950 °C for 6 h. The increase in the annealing temperature reduces the power loss at high frequencies.

1 May 2020 in AIP Advances
Verified
Journal Article
Open access
PDF file
JZJingwu Zheng
Jingwu Zheng
STShijun Tian
Shijun Tian
KLKaihua Liu
Kaihua Liu
WCWei Cai
Wei Cai
Yiping TangYiping Tang
Yiping Tang
Shenglei CheShenglei Che
Shenglei Che
A new reduction–diffusion method for preparing submicron-sized Sm2Fe17N3 was developed. First, submicron-sized α-Fe/Sm2O3 composite precursors with good dispersibility were prepared directly by ultrasonic spray pyrolysis and hydrogen reduction (USP-HR). Then, the precursor was successfully converted into Sm2Fe17N3 powder by Ca reduction–diffusion and nitridation. The results displayed that the precursor prepared by USP-HR was a monodisperse homogeneous composite of spherical particles of α-Fe and Sm2O3. α-Fe and Sm2O3 exist in an intercalated structure in the composite spherical particles. This creates conditions for the preparation of ultrafine Sm2Fe17N3 particles with uniform sizes and dispersity. The results show that Sm2Fe17N3 is a single-phase, composed of submicron-sized particles with no other impurity phases. The physical property measurement system shows that the coercivity of 0.616 ± 0.347 µm particles reaches 14.7 kOe.

28 July 2020 in Journal of Superconductivity and Novel Magnetism
Verified
Journal Article
Closed access
PDF file
YYYao Ying
Yao Ying
HWHuibin Wang
Huibin Wang
JZJingwu Zheng
Jingwu Zheng
JYJing Yu
Jing Yu
Wangchang LiWangchang Li
Wangchang Li
Shenglei CheShenglei Che
Shenglei Che

7 November 2022 in Magnetochemistry
Verified
Journal Article
Open access
PDF file
JZJingwu Zheng
Jingwu Zheng
SYShitong Yu
Shitong Yu
HHHeng Huang
Heng Huang
RLRongyao Li
Rongyao Li
WCWei Cai
Wei Cai
Shenglei CheShenglei Che
Shenglei Che
Sm2Fe17N3 compounds, having excellent intrinsic magnetic properties, are prone to decomposition at high temperatures; thus, a low melting point metal binder is the key to prepare high performance bulk magnets at low temperatures. In this paper, a new low melting point alloy Ce72Cu28-xAlx was used as the binders, and high-performance Ce-based alloy bonding Sm2Fe17N3 magnets were realized by the hot-pressing method. The experimental results demonstrated that the content of Al in the Ce-based alloys had an important influence on the performance of the magnets. High performance Sm-Fe-N bonded magnets with remanence of 10.19 KGs and maximum magnetic energy product of 21.06 MGOe were achieved by using 5 wt.% Ce72Cu22Al6 alloy as a binder. At the same time, it was found that the Ce72Cu28-xAlx alloy has a lower density and better bonding effect than the common Zn binder. Its bonding magnets still have higher performance even with extremely high oxygen content. Therefore, Ce72Cu28-xAlx alloy with low melting point is a promising new rare earth-based alloy binder. If the oxygen content of the alloy powders could be reduced, higher performance Sm2Fe17N3 bonded magnets can be prepared.

10 October 2022 in Materials
Verified
Journal Article
Open access
PDF file
QMQiangyi Mao
Qiangyi Mao
LQLiang Qiao
Liang Qiao
JZJingwu Zheng
Jingwu Zheng
YYYao Ying
Yao Ying
JYJing Yu
Jing Yu
WCWei Cai
Wei Cai
Ceramic injection molding is a near-net shape-processing technique, producing ceramic components with low tooling costs and complex shapes. In this paper, ZrO2 ceramics with high loading content in the green part were prepared by powder modification using zirconate coupling agent, injection molding and sintering, which benefited decreasing the usage of binders and deformation of ceramics. The rheological characteristics of feedstocks, densities, microstructures and mechanical properties of green and sintered parts with the different coupling media and sintering temperatures were studied. The results showed that the addition of a zirconate coupling agent with ethanol medium obviously increased the flowability of feedstocks and benefited achieving the green parts with high powder loading (86.5 wt.%) and bending strength (12.9 MPa) and the final unbroken ceramics. In addition, the sintering temperatures from 1500–1575 °C had no significant effects on the density, hardness, and surface morphology of the ceramic samples. However, the bending strength increased and some large grains with transgranular fracture occurred on the fractural surface at the sintering temperature of 1575 °C.

5 December 2022 in Materials
Verified
Journal Article
Open access
PDF file
SWSiyuan Wang
Siyuan Wang
JZJingwu Zheng
Jingwu Zheng
DZDanni Zheng
Danni Zheng
LQLiang Qiao
Liang Qiao
YYYao Ying
Yao Ying
Shenglei CheShenglei Che
Shenglei Che
The major method used to reduce the magnetic loss of soft magnetic composites (SMCs) is to coat the magnetic powder with an insulating layer, but the permeability is usually sacrificed in the process. In order to achieve a better balance between low losses and high permeability, a novel photodecomposition method was used in this study to create a ZnO insulating layer. The effect of the concentration of diethyl zinc on the formation of a ZnO insulating film by photodecomposition was studied. The ZnO film was best formed with a diethyl zinc n-hexane solution at a concentration of around 0.40 mol/L. Combined with conventional coupling treatment processes, a thin and dense insulating layer was coated on the surface of iron powder in situ. Treating the iron powder before coating by photodecomposition led to a synergistic effect, significantly reduced core loss, and the effective permeability only decreased slightly. An iron-based soft magnetic composite with a loss value of 124 kW/m3 and an effective permeability of 107 was obtained at the frequency of 100 kHz and a magnetic field intensity of 20 mT.