A surface nanocrystalline steel layer in the low alloy steel 41Cr4 was fabricated by using mechanical-pulse treatment (MPT) with different deformation modes. The structure parameters, the physical and mechanical properties, the wear resistance, and the surface topography parameters of the treated steel depending on the deformation mode were investigated. A tool with a smooth working surface was used for inducing unidirectional deformation in the top surface layer (shear), and a tool with the oppositely directed grooves was used for generating multidirectional deformation. The surface layer with a nanocrystalline structure formed by MPT using both of the tools was characterised by enhanced mechanical properties and wear resistance compared with those of the untreated or heat-treated steels. Inducing multidirectional deformation during the MPT resulted in a decrease in the grain size and an increase in the depth and microhardness of the surface layer due to it facilitating the generation of dislocations compared to those formed under unidirectional deformation. The results also demonstrated that favourable surface topography parameters providing the highest wear resistance of the steel were obtained at MPT using multidirectional deformation.
1 January 2018 in Advances in Materials Science and Engineering
The vibration‐centrifugal hardening forms a gradient ultrafine grain structure of the ferritic class with a grain size of 190 nm and a surface microhardness of 8.9 GPa and a depth of up to 6 mm on the surface of 40 Kh steel of the ferritic‐pearlitic structure. These parameters are formed due to an increase in the mass of the tool that acts on the processed surface through the balls and depend on the treatment modes. This surface ultrafine grain structure increases the wear resistance properties of steel in oil and oil‐abrasive environment and improves the electrochemical characteristics.
The residual stresses of the first kind, which are formed by vibration‐centrifugal hardening, are calculated. These are shown to increase in the hardened layer with increasing processing time and the weight of the hardening tool. The residual compressive stresses in the hardened layer after vibration‐centrifugal hardening for optimal parameters reach maximum values: circular stresses up to = 1600 MPa and radial stresses up to σr = 290 MPa. Their correlation with surface microhardness is shown.