Owing to its excellent mechanical properties and aesthetic tooth-like appearance, lithium disilicate glass–ceramic is more attractive as a crown for dental restorations. In this study, lithium disilicate glass–ceramics were prepared from SiO2–Li2O–K2O–P2O5–CeO2 glass systems with various Al2O3 contents. The mixed glass was then heat-treated at 600 °C and 800 °C for 2 h to form glass–ceramic samples. Phase formation, microstructure, mechanical properties and bioactivity were investigated. The phase formation analysis confirmed the presence of Li2Si2O5 in all the samples. The glass–ceramic sample with an Al2O3 content of 1 wt% showed rod-like Li2Si2O5 crystals that could contribute to the delay in crack propagation and demonstrated the highest mechanical properties. Surface treatment with hydrofluoric acid followed by a silane-coupling agent provided the highest micro-shear bond strength for all ceramic conditions, with no significant difference between ceramic samples. The biocompatibility tests of the material showed that Al2O3-added lithium disilicate glass–ceramic sample was bioactive, thus activating protein production and stimulating the alkaline phosphatase (ALP) activity of osteoblast-like cells.
Lithium disilicate glass ceramics with improved properties were prepared via a thermal treatment method by varying its composition. This study aims to investigate the influence of the concentration of Al2O3 additive oxides on the phase formation and mechanical properties of lithium disilicate glass ceramics prepared by conventional method. The Al2O3 concentration used are 3.0, 4.5, and 6.0 mol% for LCA1, LCA2, and LCA 3, respectively. As the content of Al2O3 increased the glass transition temperature (Tg), the crystallization temperature (Tc), phase formation, and mechanical properties of lithium disilicate glass ceramics varied considerably, demonstrating the substantial effect of Al2O3. After heat treatment at 600 °C and 800 °C for 1 h, the x-ray diffraction results showed that the major phase in all the glass-ceramic samples was Li2Si2O5 and the minor phases were CeO2, LiAlSi3O8, quartz, and Li2SiO3. For the lowest content of Al2O3, the highest flexural strength and Vickers hardness were obtained as 188.34 MPa and 776 HV, respectively. These results were attributed to the interlocking microstructure of rod-like Li2Si2O5 in the LCA1 sample.
We have investigated the magnetic properties of nanostructured magnetic crystals embedded in strontium hexaferrite-bioglass (SF-45S5). The crystallization kinetics, structure and phase formation of nanoparticles were also studied. The incorporation technique was employed to synthesize 45S5 glass. The crystallization rate constant (n) of the magnetic bioactive glass was found to be approximately 3. This suggests that bulk crystallization is occurs by a three-dimensional crystal growth. The presence of SrFe12O19, CaP4O11, Na2Ca3Si6O16 and Fe2O3 in all of the quenched glass samples was evidenced by X-ray diffraction results. Micrographs of the crystallized base glass SF-45S5 system, obtained from scanning electron microscopy, showed the presence of granular-like crystals in the glass ceramics. Characteristics of a hard-magnetic material were found for samples, as confirmed by their hysteresis loops.
1 November 2015 in Journal of Nanoscience and Nanotechnology
The incorporation method was employed to produce ferroelectric glass ceramics from the K2O– Nb2O5–B2O3 glass system. The nanocrystalline potassium niobate (KNbO3) was first prepared using a simple mixed oxide method, where the B2O3 was initially mixed and then melted to form glass. The successfully produced optically transparent glass was then subjected to a heat treatment schedule for further crystallization at temperatures ranging from 500 to 650 °C, which resulted in the precipitation of the KNbO3 phase, together with the K3B2Nb3O12 phase. Scanning electron microscopy (SEM) showed the presence of randomly oriented KNbO3 crystals dispersed in a continuous glass matrix. It was found that the glass ceramics subjected to the heat treatment at temperatures higher than 545 °C were opaque, while the lower gave a highly transparent glass ceramics. The crystal size and crystallinity were found to increase with increasing heat treatment temperature, which in turn plays an important role in controlling the properties of the glass ceramics, including physical, optical, and dielectric properties.