A novel Al-Mg-Si aluminum alloy with the addition of the micro-alloying element Er and Zr that was promptly quenched after extrusion has been studied. The solid solution and aging treatment of the novel alloy are studied by observing the microstructure, mechanical properties, and strengthening mechanism. Scanning electron microscopy (SEM) and transmission electron microscopy (TEM) techniques are employed to examine the changes in the microstructure resulting from various solid solution treatments and aging treatments. The best strengthening effect can be achieved when the solubility of the MgSi phase and precipitate β″ (Mg2Si phase) is at their maximum. The addition of Er and Zr elements promotes the precipitation of the β″ phase and makes the b″ phase more finely dispersed. The aging strengthening of alloys is a comprehensive effect of the dislocation cutting mechanism and bypass mechanism, the joint effect of diffusion strengthening of Al3(Er,Zr) particles and the addition of Er and Zr elements promoting the precipitation strengthening of β″ phases. In this paper, by adding Er and Zr elements and exploring the optimal heat treatment system, the yield strength of the alloy reaches 437 MPa and the tensile strength reaches 453 MPa after solid solution treatment at 565 °C/30 min and aging at 175 °C/10 h.
11 June 2024 in International Journal of Metalcasting
The hot deformation behavior of Al-Zn-Mg-Er-Zr alloy was investigated through an isothermal compression experiment at a strain rate ranging from 0.01 to 10 s−1 and temperature ranging from 350 to 500 °C. The constitutive equation of thermal deformation characteristics based on strain was established, and the microstructure (including grain, substructure and dynamic precipitation) under different deformation conditions was analyzed. It is shown that the steady-state flow stress can be described using the hyperbolic sinusoidal constitutive equation with a deformation activation energy of 160.03 kJ/mol. Two kinds of second phases exist in the deformed alloy; one is the η phase, whose size and quantity changes according to the deformation parameters, and the other is spherical Al3(Er, Zr) particles with good thermal stability. Both kinds of particles pin the dislocation. However, with a decrease in strain rate or increase in temperature, η phases coarsen and their density decreases, and their dislocation locking ability is weakened. However, the size of Al3(Er, Zr) particles does not change with the variation in deformation conditions. So, at higher deformation temperatures, Al3(Er, Zr) particles still pin dislocations and thus refine the subgrain and enhance the strength. Compared with the η phase, Al3(Er, Zr) particles are superior for dislocation locking during hot deformation. A strain rate ranging from 0.1 to 1 s−1 and a deformation temperature ranging from 450 to 500 °C form the safest hot working domain in the processing map.
A novel Al-Cu-Zr alloy is designed in this paper, which provides a method for further improving the strength of Al-Cu alloys. In this paper, the addition of the micro-alloying element Zr in Al-Cu alloy was studied. The effect of aging treatment on the mechanical properties and precipitation behavior of the alloy was studied. With the addition of Zr, Al3Zr phases were formed in the alloy, which acts as obstacles to dislocation motion. In addition, Al3Zr phases can be used as the nucleation site of θ′ phases to promote precipitation. All this can improve the strength of Al-Cu alloys. After one-step aging, corresponding to the highest hardness, the largest amount of θ′ phases were observed in the alloy matrix. By contrast, after two-step aging, the θ′ phases were finer, and a large amount of Guinier–Preston (GP) zones formed during the pre-aging step, which were transformed into denser and finer θ′ phases in the secondary aging step. After the same solution treatment (540 °C/12 h), undergoing 120 °C/4 h + 175 °C/10 h two-step aging, the ultimate tensile strength, yield strength, and elongation of the Al-Cu-Zr alloy were 398.7 MPa, 313.3 MPa, and 7.9%, respectively.
22 May 2024 in International Journal of Materials Research
The effects of addition of Er and Zr on the aging precipitation phase and mechanical properties in cast Al–Cu–Mn–Si–Mg alloy were studied. The addition of Er and Zr can refine the as-cast grains. The average grain size of as-cast alloy containing Er and Zr is 140.60 μm, while the average grain size of as-cast alloy without Er and Zr is 168.54 μm. After T6 heat treatment, the yield strength of the alloy containing Er and Zr reached 334.3 MPa, while the yield strength of the alloy without Er and Zr was only 284.3 MPa. After aging the strengthening precipitates of both alloys contain θ′ phase, Q′ phase and T phase. In the alloys containing Er and Zr the Al3(Er, Zr) phase with L12 structure precipitated during the solution process, which reduced the diameter of the θ′ phase during subsequent aging. After T6 heat treatment, the precipitation strengthening contributed 67.09 % and 61.31 % to the total strength of the alloy with Er, Zr and without Er, Zr, respectively.