Summary: Polymer gel is frequently used for conformance control in fractured reservoirs, where it is injected to reside in fractures or high-permeability streaks to reduce conductivity. With successful polymer-gel conformance control in place, increased pressure gradients across matrix blocks may be achieved during chase floods, diverting water, gas, or enhanced oil recovery (EOR) chemicals into the matrix to displace oil. Knowledge of gel behavior during placement and chase floods is important because it largely controls the success of subsequent injections. Polymer-gel behavior is often studied in corefloods, where differential pressure and effluents from fracture and matrix outlets give information about gel deposition during placement and flow paths during chase floods. The work presented in this paper uses complementary positron emission tomography (PET) chromatographic tomography (CT) imaging to quantify the behavior and blocking capacity of Cr(III)-acetate hydrolyzed polyacrylamide (HPAM) gel during chase waterflooding. In-situ imaging provides information about changes that may not be extracted from pressure measurements and material balance only, such as changes in local fluid saturations and dynamic spatial flow within the fracture and within the structure of the gel network. Polymer gel was placed in core plugs with longitudinal fractures that connected the inlet and outlet, and chase water was subsequently injected to measure the gel blocking capacity. The water phase was labeled with a positron emitting radiopharmaceutical (F-18) to visualize and quantify local flows with PET during gel rupture and subsequent flooding. By use of PET, we study gel rupture and the development of wormholes during gel erosion after rupture as a function of flow rate. A particular strength with access to dynamic, local flow patterns is the direct comparison to global measurements, such as differential pressure and production rate, to verify existing gel-behavior models.
23 December 2015 in SPE Reservoir Evaluation & Engineering
Summary: Polymer gels are frequently applied for conformance improvement in fractured reservoirs, where fluid channeling through fractures limits the success of waterflooding. Placement of polymer gel in fractures reduces fracture conductivity, thus increasing pressure gradients across matrix blocks during chase floods. A gel-filled fracture is reopened to fluid flow if the injection pressure during chase floods exceeds the gel-rupture pressure; thus, channeling through the fractures resumes. The success of a polymer-gel treatment, therefore, depends on the rupture pressure. Salinity differences between the gel network and surrounding water phase are known causes of gel swelling (e.g., observed in recent work on preformed particle gels). Gel swelling and its effect on fluid flow have, however, been less studied in conjunction with conventional polymer gels. By use of corefloods, this work demonstrates that low-salinity water can swell conventional Cr(III)-acetate hydrolyzed polyacrylamide (HPAM) gels, thereby significantly improving gel-blocking performance after gel rupture. Formed polymer gel was placed in fractured core plugs, and chase waterfloods were performed using four different brine compositions, of which three were low-salinity brines. The fluid flow rates through the matrix and differential pressures across the matrix and fracture were measured and shown to increase with decreasing salinity in the injected water phase. In some cores, the fractures were reblocked during low-salinity waterfloods, and gel-blocking capacity was increased above the initial level. Low-salinity water subsequently flooded the matrix during chase floods, which provided additional benefits to the waterflood. The improved blocking capacity of the gel was caused by a difference in salinity between the gel and injected water phase, which induced gel swelling. The results were reproducible through several experiments, and stable for long periods of time in both sandstone and carbonate outcrop core materials. Combining polymer gel placement in fractures with low-salinity chase floods is a promising approach in integrated enhanced oil recovery (IEOR).
Summary: This work investigates dehydration of polymer gel by capillary imbibition of water bound in gel into a strongly water-wet matrix. Polymer gel is a crosslinked-polymer solution of high water content, where water can leave the gel and propagate through porous media, whereas the large 3D polymer-gel structures cannot. In fractured reservoirs, polymer gel can be used for conformance control by reducing fracture conductivity. Dehydration of polymer gel by spontaneous imbibition (SI) contributes to shrinkage of the gel, which may open parts of the initially gel-filled fracture to flow and significantly reduce the pressure resistance of the gel treatment. SI of water bound in aged Cr(III)-acetate-hydrolized-polyacrcylamide (HPAM) gel was observed and quantified. Oil-saturated chalk-core plugs were submerged in gel, and the rate of SI was measured. Two boundary conditions were tested: all faces open (AFO) and two-end-open oil-water (TEO-OW), where one end was in contact with the imbibing fluid (gel or brine) and the other was in contact with oil. The rate of SI was significantly slower in gel compared with brine, and was highly sensitive to the ratio of matrix volume to surface open to flow, decreasing with increasing ratios. The presence of a dehydrated gel layer on the core surface lowered the rate of imbibition; continuous loss of water to the core increased the gel layer concentration and thus the barrier to flow between the core and fresh gel. Severe gel dehydration and shrinkage up to 99% were observed in the experiments, suggesting that gel treatments may lose efficiency over time in field applications where a potential for SI exists. The implications of gel dehydration by SI, and its relevance in field applications, are discussed for both gel and gelant field treatments.
Summary: Polymer gel has been used for water conformance control for several decades and may have significant potential in remediating unfavorable carbon dioxide (CO2) flow in the subsurface. High-mobility CO2 may channel quickly through sedimentary reservoirs, where unfavorable displacements are worsened in the presence of heterogeneities. Flow diversion technology targeting and withstanding CO2 is therefore essential to improving sweep efficiency and increasing storage potential. Polymer gel treatments have been demonstrated to remediate CO2 channeling in several enhanced oil recovery (EOR) field applications and have been proposed as a means to remediate wellbore and seal leakage during carbon sequestration. The goal of this review is to assess CO2 conformance control by polymer gel in published laboratory work related to both storage and EOR operations. Although field implementation of polymer gel has been successful in reducing CO2 flow, supporting experimental work on the laboratory scale is scattered, with both results and parameters varied. This paper summarizes the available literature and proposes a framework for future experimental work to aid more systematic assessment.