Graphite-based composites are well recognized as ideal functional materials in mechanical seals, bearings of canned pumps, and electrical contact systems because of their outstanding self-lubricating ability, thermostability, and chemical stability. Working in harsh conditions is a huge challenge for the graphite materials, and their tribological properties and wear mechanisms are not well studied. In this study, the tribological performance of metal-impregnated graphite, resin-impregnated graphite, and non-metal-impregnated graphite under high temperature and high load are studied using a ball-on-disc tribometer. The results show that the metal-impregnated graphite (Metal-IG) has a stable friction regime and exhibits better anti-friction and anti-wear properties than that of resin-impregnated graphite (Resin-IG) and non-impregnated graphite (Non-IG) under extreme pressure (200~350 MPa) and high temperature (100–350 °C). The Metal-IG and Resin-IG can reduce the wear depth by 60% and 80%, respectively, when compared with Non-IG substrate. The impregnated materials (metal or resin) can enhance the strength of the graphite matrix and improve the formation of graphite tribofilm on the counterpart surfaces. Friction-induced structural ordering of graphite and slight oxidation of metal in the formed mechanically mixed layer is also beneficial for friction and wear reduction. This study demonstrates the tribological characteristics of impregnated graphite under harsh conditions and provides the experimental basis for the advanced usage of high-reliability and self-lubrication graphite composites.
A spring-energized seal, whose PTFE plastic shell has excellent self-lubrication and a low temperature stability, is used widely in liquid fuel valves’ rotating end-face seals. However, in practical application, temperature has a larger effect on not only the physical and tribological properties of materials, but also on the leakage performance of spring-energized rings. Thus, a high and low temperature sealing test of the spring-energized seal that applies to an engine was carried out. In this paper, the leakage characteristics, friction torque and wear characteristics of a spring-energized ring under different temperatures were studied. The friction torque at high temperature was less than that at normal temperature, and a low temperature could effectively reduce the wear amount of PTFE material. In order to study the influence of temperature on PTFE filled with graphite, the friction and wear test of PTFE-2 was carried out. The results showed that the amount of wear of PTFE-2 was only 27.8% of that at the normal temperature but the friction coefficient was three times larger when the temperature was −45 °C.
Spring-energized seals demonstrate good sealing performance over a wide range of pressures and temperatures and can compensate for installation eccentricity, high-temperature aging, etc. However, as a contact seal, its polytetrafluoroethylene (PTFE) jacket material is easily worn during the rotation of the end face, which leads to a decline in sealing performance and, ultimately, seal failure. Based on the Archard wear model, a performance prediction model of the spring-energized seal was established by combining tests and numerical analyses. In order to improve the tribological performance of spring-energized seals made of PTFE, varied fillers were added to modify the PTFE, and the tribological and mechanical properties of PTFE composites with varied fillers were measured in experiments. Using a performance prediction model for spring-energized seals, the variation in the friction performance of seals made of these filled PTFEs during the operating cycle was analyzed. The results showed that the performance prediction model can accurately simulate this variation. After a certain amount of wear, the deviation between the simulated data and the experimental data was within ±5%. Compared with spring-energized seals made of pure PTFE, the friction torque of spring-energized seals made of GF/PTFE was reduced by 28.97% at most, and the friction torque reduction rate was lowered by 22.25%.