The microstructural evolution and corrosion behaviour of railroad flash-butt-welded U71Mn joints and the effect of heat treatment were investigated via scanning electron microscopy and electrochemical measurements. The joint structures were found to mainly comprise pearlite and a few ferrites. The grains became finer and more homogeneous after heat treatment. Additionally, there was a decrease in the corrosion current density (1.71 × 10−5 A cm−2) and increases in the absolute corrosion potential (0.86 mV) and corrosion resistance (1088.83 Ω−1cm2). This was primarily attributed to the fewer Cl− ions at the homogeneous grain boundaries and fewer oxidation reactions on the joints after heat treatment. The findings of this study explain corrosion failure and will guide the development of corrosion-resistant joints for improved railroad quality.
U75V rail steel is widely used in railways in China, including train tunnels in mountain and subsea projects, where it suffers from selective corrosion near welded joints. To ensure adequate railway service life, this study examines the effect of the normalisation process on the electrochemical behaviour of U75V rail-welded joints (URWJs) manufactured by flash butt welding (FBW) using potentiodynamic polarisation and electrochemical impedance spectroscopy (EIS). Corrosion morphology and elemental distribution analyses were performed to investigate the corrosion behaviour. The results show that the grains within the joints became finer and more homogeneous after normalisation, with a lower corrosion rate and higher corrosion resistance. It is demonstrated that fewer corrosion products were formed on the surface of the normalised joints after electrochemical test, and the corrosion resistance of the URWJs improved, owing to the formation of denser passivation films caused by normalisation. These mechanisms of corrosion response help explain corrosion failure in railway lines, as well as also help optimise the welding process and normalising processes to obtain a corrosion-resistant microstructure and ensure the quality of welded joints.