This study uses discarded tree leaves to produce biomass porous carbon nanosheets (PCNS) via carbonization and pore-forming processes, then modifies them with carboxymethyl chitosan (CMCS) and 8-hydroxyquinoline (8-HQ).
2 December 2024 in Journal of Iron and Steel Research International
C4H10O4 is an environmentally friendly phase change material that can release high phase change enthalpy, but its high super-cooling degree and low thermal conductivity hinder its wide application. This paper adopted C4H10O4 as a phase change material, and the composite phase change material was prepared by melting and blending C4H10O4 with carbon fiber, carbon particles. The results indicate that the composite phase change material with 1.5% filler has better comprehensive properties. Compared with pure C4H10O4, 167% improvement in thermal conductivity, the under-cooling decreases by 42%, and 3% increase in enthalpy of phase change. FT-IR analysis shows that no new substances are produced, and TG analysis shows that the chemical stability is good. Heat storage/release analysis shows that the exothermic time reaches 4 hours, and the exothermic time is 5 °C higher.
Phase change thermal storage fibers with high latent heat have attracted significant attention in thermal management and heat storage. Through fiber encapsulation, shape-stable phase change materials can be prepared, thereby expanding their applications. In this study, electro-blown spinning was utilized to prepare phase change materials (PCM) using erythritol, with polyethylene oxide (PEO) as the carrier material. Coaxial thermal storage fibers encapsulating the phase change materials were prepared using polyvinyl alcohol (PVA) and polyvinylpyrrolidone (PVP). The results indicate that the composite fibers have a smooth surface, uniform and smooth morphology, a maximum latent heat of 223.01 J/g, as well as excellent thermal stability. The coaxial fibers exhibit a distinct core–shell structure, with the coaxial fibers encapsulated with PVA as the shell material, demonstrating a high latent heat of 118.62 J/g, a residual rate of 93.81% after heating, and excellent thermal performance. The encapsulation efficiency is 53%, effectively addressing the issue of erythritol leakage. The research results provide valuable guidance for the efficient preparation of erythritol coaxial thermal storage fibers.