Incessant generation and mismanagement of industrial waste, resource scarcity, and environmental degradation have created non-sustainability in human life. Though industrial wastes are hazardous or non-hazardous in nature based on their source, open dumping disposal is commonly done for both types of waste. The adversity associated with waste enhances the environmental and health impacts. However, this waste has the potential to recycle and minimize resource scarcity. The circular economy works on the concept of reuse, recycling, and recovery to convert waste into a resource. Thus, industrial waste can benefit the environment and economic growth to build industrial ecology. However, the opportunities and challenges associated with industrial ecology for the reuse and recycling of waste have to be identified and preserved. Therefore, this study has identified challenges associated with waste, analyzed their impact, and industrial regulations, prioritized their criticality, and developed solution strategies to alleviate them. Two case studies on industrial byproducts, i.e., fly ash and red mud, based on different income groups are discussed in this study. It highlights the circular economy has minimized waste generation and enhanced the recovery of secondary resource materials. In addition, this study supports achieving the sustainable development goals (SDGs) 11 and 12 to build a sustainable industrial ecosystem.
The rising demands for critical metals and the environmental impact of solid waste disposal have increased interest in recycling of spent lithium-ion batteries (LiBs). This study was focused on hydrometallurgical recycling of LCMO type cathode batteries for the recovery of critical metals (lithium, cobalt, and manganese). The process involves sulfuric acid leaching in the presence of a reducing agent (H2O2) followed by the precipitation recovery of critical metals. The influential parameters like pulp density, H2SO4 concentration, H2O2 addition, agitation time, and temperature were optimized, yielding >98% leaching in 2.0 M H2SO4 with 4 vol.% of H2O2 at a moderate temperature of 50°C. Reaction kinetics revealed that the leaching was governed by the mixed-control process. Furthermore, the separation and recovery of metals from leach liquor was conducted by simple precipitation techniques, where KMnO4, C2H2O4, and Na2CO3 were used as precipitating reagents to recover MnO2, CoC2O4, and Li2CO3, respectively.