An anomalous deformation-induced dissolution of the intermetallics Ni3Al and Ni3Ti in the matrix of austenitic Fe–Ni–Al(Ti) alloys has been revealed in experiment at cryogenic temperatures (down to 77 K) under rolling and high pressure torsion. The observed phenomenon is explained as the result of migration of deformation-stipulated interstitial atoms from a particle into the matrix in the stress field of moving dislocations. With increasing the temperature of deformation, the dissolution is replaced by the deformation-induced precipitation of the intermetallics, which is accelerated due to a sufficient amount of point defects in the matrix, gained as well in the course of deformation at lower temperatures.
1 November 2006 in Materials Science and Engineering: A
Structure of a metastable austenitic invar alloy Fe-32% Ni preliminarily quenched for martensite and subjected to α → γ transformation using slow heating to various temperatures (430–500°C) with the...
17 June 2015 in Physics of Metals and Metallography
The structural state and the resistance to stress-corrosion cracking (SCC) at constant loads have been studied using samples with a grown crack by the method of the cantilever bending on quenched...
1 November 2006 in Materials Science and Engineering: A