We have investigated magnetization (M), magnetocaloric effect (MCE), and magnetothermopower (MTEP) in polycrystalline Pr0.6Sr0.4MnO3, which shows a second-order paramagnetic to ferromagnetic transition near room temperature (TC = 305 K). However, field-cooled M(T) within the long range ferromagnetic state shows an abrupt decrease at TS = 86 K for μ0H < 3 T. The low temperature transition is first-order in nature as suggested by the hysteresis in M(T) and exothermic/endothermic peaks in differential thermal analysis for cooling and warming cycles. The anomaly at TS is attributed to a structural transition from orthorhombic to monoclinic phase. The magnetic entropy change (ΔSm = Sm(μ0H)-Sm(0)) shows a negative peak at TC (normal MCE) and a positive spike (inverse MCE) at TS. ΔSm = −2.185 J/kg K (−3.416 J/kg K) with refrigeration capacity RC = 43.4 J/kg (103.324 J/kg) for field change of μ0ΔH = 1.5 T (3 T) at TC = 304 K is one of the largest values reported in manganites near room temperature. Thermopower (Q) is negative from 350 K to 20 K, which shows a rapid decrease at TC and a small cusp around TS in zero field. The MTEP [ΔQ/Q(0)] reaches a maximum value of 25% for μ0ΔH = 3 T around TC, which is much higher than 15% dc magnetoresistance for the same field change. A linear relation between MTEP and magnetoresistance and between ΔSm and ΔQ are found near TC. Further, ac magnetotransport in low dc magnetic fields (μ0H ≤ 0.1 T), critical analysis of the paramagnetic to ferromagnetic transition, and scaling behavior of ΔSm versus a reduced temperature under different magnetic fields are also reported. Coexistence of large magnetic entropy change and magnetothermopower around room temperature makes this compound interesting for applications.
Magnesium‐substituted CuCrO2 delafossite is a promising candidate for p‐type transparent conducting oxide applications owing to its relatively high electrical conductivity and optical transparency in the visible range. Here, the atomic layer deposition fabrication of semiconducting Cu(Cr1−xMgx)O2 (up to x = 0.043) thin films based on Cu(thd)2 (thd = 2,2,6,6‐tetramethyl‐3,5‐heptanedionate), Cr(acac)3 (acac = acetyl acetonate), and Mg(thd)2 as metal precursors and ozone as the oxygen source is reported. Smooth and homogeneous thin films with an accurately controlled Mg content are obtained at the deposition temperature of 250 °C. A limited substitution level is revealed from X‐diffraction patterns: peaks due to the spinel‐structured MgCr2O4 secondary phase appear for x ≥ 0.015 while the increase in lattice parameters of the delafossite Cu(Cr,Mg)O2 phase continues even up to x ≈ 0.03. The direct bandgap as determined from UV–vis spectrophotometric measurements is observed to decrease from 3.09 eV for x = 0 to 2.87 eV for x = 0.015 before increasing to 3.15 eV for x = 0.043. The observed transmittance is close to 80% in the visible range. These characteristics are superior to the thin films of the copper delafossite family prepared by any thin‐film technique.
We report on an experimental setup for the simultaneous measurement of the thermoelectric power (TEP) of two samples in the temperature range from 77 K to 500 K using optimum electronic instruments. The setup consists of two rectangular copper bars in a bridge arrangement for sample mounting, two surface mount (SM) chip resistors for creating alternate temperature gradient, and a type E thermocouple in differential geometry for gradient temperature (ΔT) measurement across the samples. In addition, a diode arrangement has been made for the alternate heating of SM resistors using only one DC current source. The measurement accuracy of ΔT increases with the differential thermocouple arrangement. For the calibration of the setup, measurements of TEP on a high purity (99.99%) platinum wire and type K thermocouple wires Chromel and Alumel have been performed from 77 K to 500 K with respect to copper lead wires. Additionally, this setup can be utilized to calibrate an unknown sample against a sample of known absolute TEP.