Specific features of the catalytic tar cracking in the presence of formic acid, BEA zeolite and 8% Ni-2.5% Mo/Sibunit catalyst were studied at 350 °C and 1.0 MPa pressure. The obtained results evidenced that formic acid can be used as a hydrogen donor during catalytic reactions. The formic acid addition made it possible to perform efficient hydrocracking of heavy feed such as tar. It was found that both the tar conversion and selectivity to light (gasoline-diesel) fractions grew in the sequence: tar < (tar - formic acid) < (tar - formic acid - BEA zeolite) < (tar - formic acid - BEA zeolite - 8% Ni-2.5% Mo/Sibunit catalyst). Furthermore, significantly lower concentrations of impurities containing sulfur and nitrogen were observed for the (tar - formic acid - BEA zeolite - 8% Ni-2.5% Mo/Sibunit catalyst) system. For example, the sulfur and nitrogen concentrations in the tar precursor were 1.50% and 0.86%, respectively. Meanwhile, their concentrations in the liquid products after the catalytic cracking were 0.73% and 0.18%, respectively.
A new method for the synthesis of boron-doped carbon nanomaterial (B-carbon nanomaterial) has been developed. First, graphene was synthesized using the template method. Magnesium oxide was used as the template that was dissolved with hydrochloric acid after the graphene deposition on its surface. The specific surface area of the synthesized graphene was equal to 1300 m2/g. The suggested method includes the graphene synthesis via the template method, followed by the deposition of an additional graphene layer doped with boron in an autoclave at 650 °C, using a mixture of phenylboronic acid, acetone, and ethanol. After this carbonization procedure, the mass of the graphene sample increased by 70%. The properties of B-carbon nanomaterial were studied using X-ray photoelectron spectroscopy (XPS), high-resolution transmission electron microscopy (HRTEM), Raman spectroscopy, and adsorption-desorption techniques. The deposition of an additional graphene layer doped with boron led to an increase of the graphene layer thickness from 2–4 to 3–8 monolayers, and a decrease of the specific surface area from 1300 to 800 m2/g. The boron concentration in B-carbon nanomaterial determined by different physical methods was about 4 wt.%.
A series of carbon-mineral composites with the carbon loading varying from 1.5 to 14.2 wt % has been synthesized by MgO carbonization in 1,3-butadiene at 600°C. The synthesized carbon-mineral...
A method for synthesis of nitrogen-doped graphene (N-graphene) with high specific surface area has been developed. In this method, magnesium oxide is used as a template where a carbon layer modified with nitrogen atoms is deposited. Nitrogen–carbon–mineral composites (N–C/MgO) containing from 5 to 27 wt % of nitrogen-doped carbon have been synthesized. After dissolving magnesium oxide, N-graphene with a specific surface area of 1300–1400 m2 g–1 has been synthesized for the first time. The synthesis of N-graphene has been characterized by electron microscopy, X-ray diffraction, and X-ray photoelectron spectroscopy.
The anthracene coking process has been investigated in the temperature range of 400–600°C. It has been shown that intermolecular interaction of two anthracene molecules resulting in the...