Structural quality of LuFeO epitaxial layers grown by pulsed-laser deposition on sapphire substrates with and without platinum Pt interlayers has been investigated by in situ high-resolution X-ray diffraction (reciprocal-space mapping). The parameters of the structure such as size and misorientation of mosaic blocks have been determined as functions of the thickness of LuFeO during growth and for different thicknesses of platinum interlayers up to 40 nm. By means of fitting of the time-resolved X-ray reflectivity curves and by in situ X-ray diffraction measurement, we demonstrate that the LuFeO growth rate as well as the out-of-plane lattice parameter are almost independent from Pt interlayer thickness, while the in-plane LuFeO lattice parameter decreases. We reveal that, despite the different morphologies of the Pt interlayers with different thickness, LuFeO was growing as a continuous mosaic layer and the misorientation of the mosaic blocks decreases with increasing Pt thickness. The X-ray diffraction results combined with ex situ scanning electron microscopy and high-resolution transmission electron microscopy demonstrate that the Pt interlayer significantly improves the structure of LuFeO by reducing the misfit of the LuFeO lattice with respect to the material underneath.
Systematic investigations into the phase evolution during reactive annealing of copper–zinc–tin–selenide (CZTSe) precursors for the fabrication of kesterite solar cell absorber layers have been paramount in understanding and suppressing the formation of secondary phases that deteriorate device performance. In this study, the phase evolution during annealing of low-temperature co-evaporated CZTSe precursors is investigated. A detailed analysis of films selenized at different temperatures is used to reveal the possible reaction pathway of CZTSe formation. Utilizing a combination of x-ray diffraction, Raman spectroscopy, scanning electron microscopy, transmission electron microscopy, and energy-dispersive x-ray spectroscopy, it is shown that CZTSe formation starts by Cu out-diffusion to the surface and Cu–Se phase formation at a temperature of 350 °C. An intimate mixing of binaries and ternaries during low-temperature selenization is observed. On the contrary, only binaries are observed at high-temperature selenization. This suggests that the CZTSe formation pathway involves reaction schemes where (i) a competition between binary and ternary phases dominates at low-temperature and (ii) binary reactions dominate the process at high temperatures. However, the number of binary phases decreases with increasing selenization temperature until they become undetectable by XRD and Raman spectroscopy at a temperature of 540 °C (selenization time 10 min). Utilizing the presented selenization conditions, prototype solar cells with an efficiency of up to 7.5%, an open-circuit voltage of 407 mV, and a fill factor of 59%, could be demonstrated. The temperature-dependent current density–voltage characteristics indicate that the performance of the prototype devices is limited by bulk Schottky–Read–Hall recombination.
12 December 2019 in Semiconductor Science and Technology
Cu(In,Ga)Se2 thin-film solar cells were fabricated with Inx(O,S)y as buffer material, where the buffer was deposited by either solution growth or radio-frequency sputtering. To elucidate the influence of the particular deposition technique on the properties of the Inx(O,S)y layers, their structural peculiarities were characterized by high-resolution transmission electron microscopy (TEM) and nanobeam electron diffraction. Energy-dispersive x-ray spectroscopy in combination with scanning TEM was used for chemical analysis of the interfacial regions between Cu(In,Ga)Se2 absorber and Inx(O,S)y layer as well as of the buffer itself. In general, the solution-grown and sputtered Inx(O,S)y layers show a nanocrystalline structure. In both types of Inx(O,S)y buffer layers, crystalline phases of tetragonal In2S3 and cubic In2O3 were detected. In addition, there are hints for the formation of a Cu-containing phase, e.g. hexagonal CuS in the sputtered Inx(O,S)y layer. Moreover, there are also distinct differences in the chemical composition of the two analyzed Inx(O,S)y layers, namely in the solution-grown Inx(O,S)y buffer layer the oxygen content is considerably higher than in the sputtered Inx(O,S)y layer.
We investigate magnetron-sputtered In2(OxS1−x)3 compounds acting as an alternative buffer system to the solution-grown CdS or Zn(O,S) buffer layers in Cu(In,Ga)Se2 (CIGS) thin-film solar cells. The influence of the oxygen content on the solar cell performance, microstructure of the mixed systems, bandgap, and band offsets to CIGS is investigated experimentally and also characterized by calculations based on density functional theory. Samples in a series with different chemical compositions ranging from In2S3 to In2O3 are either directly deposited from ceramic targets or from a pure In2S3 target by reactive sputtering by adding O2 in the Ar sputtering gas. The binary compounds In2S3 and In2O3 sputtered at 220 °C substrate temperature from ceramic targets exhibit a crystalline structure, whereas the ternary In2(O,S)3 compounds are either nanocrystalline in the case of In2(O0.25S0.75)3 or amorphous for In2(O0.5S0.5)3 and In2(O0.75S0.25)3. For [O]/([O] + [S]) ratios above 0.25, the cell efficiencies decrease drastically, mainly due to lower open-circuit voltages (VOC). This behavior can be explained by an increase of the negative conduction band offset between the CIGS absorber and the oxygen-rich In2(OxS1−x)3 or In2O3 buffer, resulting in pronounced VOC losses. Adding oxygen to In2S3 with optical bandgap energies of around 2 eV results in a bowing of the values to below 2 eV and finally reaching values of around 2.7 eV for In2O3 if an indirect band transition is assumed. In summary, our results reveal that pronounced oxygen incorporation in In2S3 is not beneficial in terms of CIGS device efficiency because oxygen is electronically inactive and poorly miscible.
The morphology and crystal structure of Pt films grown by pulsed laser deposition (PLD) on yttria-stabilized zirconia (YSZ)at high temperatures Tg = 900 °C was studied for four different film thicknesses varying between 10 and 70 nm. During the subsequent growth of the capping layer, the thermal stability of the Pt was strongly influenced by the Pt film’s thickness. Furthermore, these later affected the film morphology, the crystal structure and hillocks size, and distribution during subsequent growth at Tg = 900 °C for a long duration. The modifications in the morphology as well as in the structure of the Pt film without a capping layer, named also as the as-grown and encapsulated layers in the bilayer system, were examined by a combination of microscopic and scattering methods. The increase in the thickness of the deposited Pt film brought three competitive phenomena into occurrence, such as 3D–2D morphological transition, dewetting, and hillock formation. The degree of coverage, film continuity, and the crystal quality of the Pt film were significantly improved by increasing the deposition time. An optimum Pt film thickness of 70 nm was found to be suitable for obtaining a hillock-free Pt bottom electrode which also withstood the dewetting phenomena revealed during the subsequent growth of capping layers. This achievement is crucial for the deposition of functional bottom electrodes in ferroelectric and multiferroic heterostructure systems.