20 December 2022 in Microscopy and Microanalysis
Contamination is an undesired side effect in many electron microscopy studies that covers structures of interest and degrades resolution. Although contamination has been studied for decades, open questions remain regarding favorable imaging conditions for contamination minimization and the efficiency of contamination-mitigation strategies. This work focuses on electron-beam-induced carbon contamination in scanning transmission electron microscopy at electron energies of 30 keV and below. A reliable method to measure contamination thicknesses was developed in this work and enables the identification of imaging conditions that minimize contamination. Thin amorphous carbon films were used as test samples. The variation of important imaging parameters shows that the contamination thickness increases with the reduction of the electron energy to about 1 keV but decreases below 1 keV. Contamination increases with the beam current but saturates at high currents. Applying a given dose with a high dose rate reduces contamination. Among the tested contamination-mitigation methods, plasma cleaning and beam showering are most effective. Most experiments in this work were performed with focused scanning illumination. Experiments were also carried out with a stationary defocused beam for comparison with a theoretical contamination model with good agreement between measured and calculated contamination thickness.
30 April 2021 in Angewandte Chemie International Edition
The first liquid‐phase synthesis of high‐quality, small‐sized rare‐earth metal nanoparticles (1–3 nm)—ranging from lanthanum as one of the largest (187 pm) to scandium as the smallest (161 pm) rare‐earth metal—is shown. Size, oxidation state, and reactivity of the nanoparticles are examined (e.g., electron microscopy, electron spectroscopy, X‐ray absorption spectroscopy, selected reactions). Whereas the nanoparticles are highly reactive (e.g. in contact to air and water), they are chemically stable as THF suspensions and powders under inert conditions. The reactivity can be controlled to obtain inorganic and metal–organic compounds at room temperature.
28 October 2022 in Journal of Microscopy
Backscattered‐electron scanning electron microscopy (BSE‐SEM) imaging is a valuable technique for materials characterisation because it provides information about the homogeneity of the material in the analysed specimen and is therefore an important technique in modern electron microscopy. However, the information contained in BSE‐SEM images is up to now rarely quantitatively evaluated. The main challenge of quantitative BSE‐SEM imaging is to relate the measured BSE intensity to the backscattering coefficient η and the (average) atomic numberZto derive chemical information from the BSE‐SEM image. We propose a quantitative BSE‐SEM method, which is based on the comparison of Monte–Carlo (MC) simulated and measured BSE intensities acquired from wedge‐shaped electron‐transparent specimens with known thickness profile. The new method also includes measures to improve and validate the agreement of the MC simulations with experimental data. Two different challenging samples (ZnS/Zn(OxS1–x)/ZnO/Si‐multilayer and PTB7/PC71BM‐multilayer systems) are quantitatively analysed, which demonstrates the validity of the proposed method and emphasises the importance of realistic MC simulations for quantitative BSE‐SEM analysis. Moreover, MC simulations can be used to optimise the imaging parameters (electron energy, detection‐angle range) in advance to avoid tedious experimental trial and error optimisation. Under optimised imaging conditions pre‐determined by MC simulations, the BSE‐SEM technique is capable of distinguishing materials with small composition differences.
22 March 2001 in Journal of Applied Physics
The growth and vertical organization of CdSe quantum dots in three-layer stacks consisting of CdSe with a nominal thickness of 2.5 monolayers (ML) and ZnSe spacers with thicknesses between 10 and 20 ML was investigated by reflection high energy electron diffraction during the growth and different transmission electron microscopy techniques. The samples were grown by molecular beam epitaxy at 400 °C. It was found that up to 10 ML spacer thickness all three CdSe layers and ZnSe spacers form one broad (Cd, Zn)Se alloy layer with a small Cd concentration containing Cd-rich islands with a size of ∼15 nm. For spacers with a larger thickness (12–20 ML) three separated ternary (Cd, Zn)Se layers are observed which contain Cd-rich inclusions (small islands) with a size of less than 10 nm. A preferential vertical correlation of the small islands occurs for the 12 ML spacer thickness. With increasing spacer thickness, the number of the correlated small islands is reduced displaying a tendency to uncorrelated growth.
11 January 2002 in Physica Status Solidi (b)
20 May 2002 in Physical Review B
The transformation between a quasicrystal and an orthorhombic approximant is studied at the nominal composition by electron diffraction and high-resolution transmission electron microscopy. A series of transition states indicating a continuous transformation is monitored. First, the material transforms to a single-oriented one-dimensional quasicrystal. In the course of this process out-of-phase domains are formed. The approximant results from ordering of these domains to a periodic structure.