Sungmo Moon

Prof. Sungmo Moon

1. Surface Materials Division, Korea Institute of Materials Science (KIMS), Gyeongnam 51508, Korea
+1
orcid

Research Focus & Metrics

Academic Career Length

18Years (2009-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
10 March 2013 in Metals and Materials International
Verified
Journal Article
Closed access
PDF file
NPNguyen Van Phuong
Nguyen Van Phuong
KLKyuhwan Lee
Kyuhwan Lee
DCDoyon Chang
Doyon Chang
MKMan Kim
Man Kim
SLSangyeoul Lee
Sangyeoul Lee
Sungmo MoonSungmo Moon
Sungmo Moon

27 May 2016 in Journal of Mechanical Science and Technology
Verified
Journal Article
Closed access
PDF file
CYCheolnam Yang
Cheolnam Yang
Sungmo MoonSungmo Moon
Sungmo Moon
YKYangdo Kim
Yangdo Kim

12 March 2013 in Discover Nano
Verified
Journal Article
Open access
PDF file
TKTae-Hyung Koo
Tae-Hyung Koo
JBJyoti S Borah
Jyoti S Borah
ZXZhi-Cai Xing
Zhi-Cai Xing
Sungmo MoonSungmo Moon
Sungmo Moon
YJYongsoo Jeong
Yongsoo Jeong
IKInn-Kyu Kang
Inn-Kyu Kang
Self-assembled layers of vertically aligned titanium nanotubes were fabricated on a Ti disc by anodization. Pamidronic acids (PDAs) were then immobilized on the nanotube surface to improve osseointegration. Wide-angle X-ray diffraction, X-ray photoelectron microscopy, and scanning electron microscopy were employed to characterize the structure and morphology of the PDA-immobilized TiO2nanotubes. Thein vitrobehavior of osteoblast and osteoclast cells cultured on an unmodified and surface-modified Ti disc was examined in terms of cell adhesion, proliferation, and differentiation. Osteoblast adhesion, proliferation, and differentiation were improved substantially by the topography of the TiO2nanotubes, producing an interlocked cell structure. PDA immobilized on the TiO2nanotube surface suppressed the viability of the osteoclasts and reduced their bone resorption activity.

8 September 2013 in Journal of Solid State Electrochemistry
Verified
Journal Article
Closed access
PDF file
Sungmo MoonSungmo Moon
Sungmo Moon

21 June 2023 in Metals
Verified
Journal Article
Open access
PDF file
DKDuyoung Kwon
Duyoung Kwon
HPHien Van Pham
Hien Van Pham
PSPung Keun Song
Pung Keun Song
Sungmo MoonSungmo Moon
Sungmo Moon
This study aims to clarify how a solution’s pH can influence the corrosion and formation of surface films on the AZ31 Mg alloy in aqueous solutions containing sulfate ions. The corrosion and surface film formation behaviors were examined using in situ observation, open-circuit potential (OCP) transient, weight change measurement and electrochemical impedance spectroscopy (EIS). The morphologies of the surface films were analyzed via metal/insulator/metal (MIM) coloring and FESEM. The findings show that at pH 2, severe corrosion occurred together with rapid hydrogen evolution and formation of a highly porous surface film with numerous cracks. However, at pH 3, the corrosion rate dropped significantly and remarkably low corrosion rates were observed at pH 4 and 10. At pH 11 and 12, weight gains were noticed, suggesting the growth of surface films on the AZ31 Mg alloy. Flake-like films formed at pH 12, while needle-like structures were present between pH 3 and 11. Impedance measurements revealed increased impedance at higher pH of sulfate-ion-containing solutions. Higher impedance was related to the formation of denser surface films on the AZ31 Mg alloy. In addition, the films displayed metal/insulator/metal (MIM) colors via Au coating above pH 4, indicating uniform film thickness despite the presence of needle-like or flake-like structures.

16 May 2023 in Metals
Verified
Journal Article
Open access
PDF file
DKDuyoung Kwon
Duyoung Kwon
HPHien Van Pham
Hien Van Pham
SMSungmo Moon
Sungmo Moon
Sungmo MoonSungmo Moon
Sungmo Moon
This work demonstrates the corrosion behavior of the AZ31 Mg alloy as a function of an immersion time of 48 h in 0.1 M HCl, H2SO4, H3PO4 and HF solutions, in which pH was adjusted to 6 to exclude the contribution of hydrogen ions (H+) and hydroxide ions (OH−). In situ observations, open circuit potential (OCP), weight changes and AC impedance measurements were performed with an immersion time of 48 h and the morphologies and chemical compositions of the surface products after 48 h of immersion were analyzed by SEM, EDS and XPS. In the chloride ion (Cl−)-containing solution, the corrosion of the AZ31 Mg alloy initiated locally and propagated discontinuously over the surface with immersion time. The OCP value of the AZ31 Mg alloy showed an initial increase from −1.51 VAg/AgCl to −1.47 VAg/AgCl after about 5 h of immersion and then a decrease to −1.51 VAg/AgCl due to corrosion initiation. In the F−-containing solution, after 48 h of immersion, the OCP showed an extremely large value of −0.6 VAg/AgCl, while the relatively lower values of −1.52 VAg/AgCl, −1.59 VAg/AgCl were seen in the solutions containing SO42− and PO43, respectively. In the sulfate ion (SO42−)-containing neutral aqueous solution, needle-like surface films were formed and there were no changes in the weight of the AZ31 Mg alloy with immersion time. In the phosphate ion (PO43−)-containing neutral aqueous solution, a vigorous gas evolution occurred, together with the formation of black surface films with cracks, and a high corrosion rate of −13.8018 × 10−3 g·cm−2·day−1 was obtained. In the fluoride ion (F−)-containing neutral aqueous solution, a surface film with crystalline grains of MgF2 was formed and the weight of the AZ31 Mg alloy increased continuously with immersion time. In conclusion, the corrosion of the AZ31 Mg alloy occurred uniformly in neutral phosphate solution but locally in chloride solution. No corrosion was observed in either the neutral sulfate or fluoride solutions.