This article deals with the development of concretes intended to be used as construction materials in the Czech deep repository for radioactive waste. The basic requirements for this concrete are a reduced pH value, which must maintain a constant reduced pH with a value of around 11 in the long term, and mechanical properties comparable to conventional concrete. The raw materials for the production of the proposed low pH concrete come exclusively from the Czech Republic. Material characteristics were measured on fresh mixtures and concrete after 28, 56, and 90 days of curing. In addition to the basic raw materials (aggregate, cement, water), plasticizers, microsilica or slag, and defoaming agents were added to the mixture. The aggregate:binder ratio was approximately 5:1 and the w/c water coefficient was approximately 0.6. The mechanical properties of the final concrete were similar to the reference recipe of conventional concrete (the decrease was less than 10%) and the pH value was even below 11 after 90 days. The issue of a sprayed variant of the LPC mixture was solved within the project.
In this paper water transport and storage parameters of hydrophobic plasters are studies. This article is focused on behavior of water and its degradation process inside of material matrix. Most of physic-chemical deteriorations of building materials are related to the penetration of moisture into building structure. For higher resistance of penetration water into materials, hydrophobic additions are used. Especially inner hydrophobic additive was applied to the interior structure to reduce destructive effect of water. Water storage parameters are slightly better for plaster without hydrophobisation. However, from the quantitative point of view the difference was not so important. Comparative measurements with pure lime-metakaolin plaster were done as well. DOI: http://dx.doi.org/10.5755/j01.ms.24.1.17876