BiFeO3–based ceramics possess an advantage over large spontaneous polarization and high Curie temperature, and are thus widely explored in the field of high–temperature lead–free piezoelectrics and actuators. However, poor piezoelectricity/resistivity and thermal stability of electrostrain make them less competitive. To address this problem, (1 − x) (0.65BiFeO3–0.35BaTiO3)–xLa0.5Na0.5TiO3 (BF–BT–xLNT) systems are designed in this work. It is found that piezoelectricity is significantly improved with LNT addition, which is contributed by the phase boundary effect of rhombohedral and pseudocubic phase coexistence. The small–signal and large–signal piezoelectric coefficient (d33 and ) peaks at x = 0.02 with 97 pC/N and 303 pm/V, respectively. The relaxor property and resistivity are enhanced as well. This is verified by Rietveld refinement, dielectric/impedance spectroscopy and piezoelectric force microscopy (PFM) technique. Interestingly, a good thermal stability of electrostrain is obtained at x = 0.04 composition with fluctuation η = 31% (), in a wide temperature range of 25–180 °C, which is considered as a compromise of negative temperature dependent electrostrain for relaxors and the positive one for ferroelectric matrix. This work provides an implication for designing high–temperature piezoelectrics and stable electrostrain materials.
The TiAlMoN coatings were deposited by arc ion plating under different substrate bias voltages, and the effects of substrate bias on the composition, phase structure, microstructure, and mechanical properties of the coatings were systematically investigated. The results showed that, as the bias voltage increased from 0 V to −75 V, enhanced ion bombardment promoted coating densification, the N/(Ti + Al + Mo) atomic ratio decreased from 1.33 to 1.05, and the deposition rate increased from 124.7 nm/min to 138.2 nm/min. XRD peak fitting revealed that the TiAlMoN coatings may consist of three phases: c-TiN, fcc Mo-N, and c-AlN. With increasing negative bias voltage, the preferred (111) orientation became more pronounced, while the Mo-N phase gradually evolved from B1-MoN to γ-Mo2N. As the substrate bias voltage increased, the grain size initially reduced and then slightly increased, and the compressive residual stress sharply increased from 0.68 GPa to 2.21 GPa. Owing to coating densification, grain refinement, and increased compressive residual stress, the hardness increased from 16.7 GPa to 33.9 GPa. The adhesion strength reached a maximum of 59.7 N at −25 V and decreased at higher bias voltages because of excessive residual stress. Appropriate control of the substrate bias voltage enables the synergistic optimization of structural strengthening and interfacial stability in TiAlMoN coatings.