The damage mode of U75V rail steel in application is determined by its rolling wear behavior. In this paper, the pearlite microstructure of U75V steel is characterized to investigate the relationship between wear and fatigue behavior. The results show that, with decreasing of pearlite lamellar spacing, the wear resistance of the steel increases and the contact fatigue resistance decreases. The spacing decreasing causes the change of the wear mechanism from abrasive wear to adhesive wear, as well as the damage mode from wear damage to fatigue damage. The smaller the pearlite lamellar spacing is, the stronger the deformation of the cementite lamellar is. The thin cementite lamellar is hardly broken in the rolling friction to pile up a large number of dislocations in the ferrite matrix and the work hardening degree was improved. So, the plastic deformation layer is difficult to remove, and fatigue cracks are easy to initiate and extend to the interior of the material.
As a core load-bearing component for railway vehicles, rails are largely responsible for the safety and stability of train operation, and their service performance is inherently governed by material microstructure. In this study, rails with varied pearlite interlamellar spacing were prepared and laid on field tracks for 8 months of service testing to investigate the influence of pearlite interlamellar spacing on rail wear and rolling contact fatigue (RCF). The results indicate that decreasing pearlite interlamellar spacing facilitated tread work hardening and reduced cumulative wear loss of rails. At the early service stage, rails with coarse pearlite lamellae exhibited earlier RCF crack initiation and longer crack morphologies, while rails featuring finer pearlite lamellae exhibited the latest-occurring crack initiation. With prolonged service duration, wear loss rose continuously, and the tread hardening rate first increased sharply and then tended to gradually become stable. Obvious differences in damage evolution were observed for rails with different pearlite interlamellar spacing. Coarse-lamellar rail suffered sparse short cracks dominated by wear; fine-lamellar rail developed dense fast-growing cracks controlled by RCF; and medium-lamellar rail achieved a relatively good balance between wear and RCF. A competitive relationship exists between wear and RCF during rail service. Reasonable regulation of pearlite interlamellar spacing facilitates a balanced evolution of wear and RCF, which provides a feasible microstructural optimization strategy for improving the service performance and service life of pearlitic rails.
A transverse fracture occurred in U75V pearlitic rail after 5 months of service on a sharp radius curved track of mixed passenger-freight railway. Systematic tests including chemical composition analysis, mechanical properties testing, macroscopic fracture inspection, metallographic observation and microscopic morphology characterization were conducted on the failed rail sample. The results indicate that the rail base metal has qualified metallurgical quality. Its chemical composition, fundamental mechanical properties and microstructure fully meet the requirements of Chinese railway standard TB/T 2344.1-2020. The failure mode is identified as instantaneous brittle fracture. Severe mechanical extrusion and impact cause prominent plastic deformation on the rail foot, leading to surface plastic flow and further triggering micro-crack initiation. Under continuous cyclic stress induced by train loads, the micro-crack tips undergo repeated tearing and closing. Severe stress concentration accelerates the formation of transgranular cracks, which propagate rapidly and unstably toward the rail interior, eventually resulting in catastrophic transverse fracture. Standardized procedures in rail transportation, hoisting and laying are essential to avoid mechanical damage, while regular line inspection and timely replacement of damaged rails should be strictly enforced.