Calcium hydroxide derived from eggshells can remove F − efficiently in water with the adsorption capacity of 370.15 mg g −1 , and the final concentration can meet the guidelines of the WHO, which is below 1.5 mg L −1 .
15 December 2023 in Separation and Purification Technology
This study presents a series of Cu-Mn/Al2O3 catalysts prepared by the polyol method to improve the toluene combustion process. The catalytic activity evaluation results showed that the different polyols have a great influence on catalyst activity, in which the catalyst prepared with glycerol through a hydrothermal reaction at 90 °C displayed the highest catalytic activity. The lowest T90 and T50 values could be achieved by CMA-GL-90 with 260 and 237 °C, respectively. Moreover, the XRD and BET results showed that the hydrothermal treatment was more favorable with Cu-Mn crystal formation, and an abundance of mesopores remained in all catalysts with a high specific surface area from 94.37 to 123.03 m2·g−1. The morphology analysis results by SEM and TEM indicated that employing glycerol coupled with hydrothermal treatment at 90 °C could enhance the formation of CuMn2O4 spinel. The toluene catalytic combustion mechanism of Cu-Mn/Al2O3 catalysts was discussed based on XPS and H2-TPR, and a high atomic ratio of Mn3+ could be obtained with 51.03%, and the ratio of Oads/Olatt also increased to 2.85 in CMA-GL-90. The increase in Mn3+ species and oxygen vacancies on the surface of catalysts exhibited excellent activity and stability for toluene combustion. These findings offer valuable insights for optimizing the design and application of Cu-Mn/Al2O3 catalysts in addressing the catalytic oxidation reactions of organic volatile compounds.
Ca–Zr–Sn composite oxides catalysts for 1,4-butanediol (BDO) selective dehydration to 3-butene-1-ol (BTO) are synthesized by impregnation and co-precipitation in the present work. The results show that Ca–Zr–Sn catalysts prepared from co-precipitation by using NaOH-Na2CO3 mixing alkali solution as precipitant exhibit an excellent catalytic property for BDO dehydration to BTO. For instance, Ca–Zr–Sn oxide with Ca/Zr and Sn/Zr molar ratio of 0.68 and 0.28 calcined at 650 °C gives a BDO conversion and BTO selectivity of about 97% and 82%, respectively, and exhibits no deactivation during 1000 h scale-up experimental testing. X-ray diffraction results indicate that catalytic active centers for BDO dehydration to BTO are from Ca0.15Zr0.85O crystal phase. NH3- and CO2-temperature programmed desorption prove that the surface of obtained catalysts can provide a large amount of acid and base sites simultaneously. FT-IR spectra of pyridine-adsorbed samples show that acid sites on the surface of Ca–Zr–Sn oxide catalyst mainly exist in a state of Lewis acid, which activates terminal -OH groups of BDO molecule through complexing. The activated -OH interacts with β-H activated on base sites O2− anions relative to Ca species, thereby the CH2=CH- bonds are produced through dehydration to form BTO.