Magnesium and nickel were recovered from nickel-rich serpentine through sulfation roasting and water leaching. The factors affecting the extraction percentages of Mg and Ni were discussed. Under the conditions of the ratio of acid to ore of 0.8:1 and roasting temperature of 650 °C for 120 min, 91.6% of Mg and 88.7% of Ni but only 4.8% of Fe were extracted. The roasting kinetics of Mg and Ni were investigated. The results showed that the roasting stage was governed by internal diffusion in the temperature range of 350–650 °C, and the activation energy of nickel and magnesium were different in the time ranges of 0–30 min and 60–120 min, with 17.45 kJ⋅mol−1 (0–30 min) and 14.12 kJ⋅mol−1 (60–120 min) for magnesium and 15.48 kJ⋅mol−1 (0–30 min) and 12.46 kJ⋅mol−1 (60–120 min) for nickel. The kinetic equations were obtained.
This paper describes a leaching-purifying-precipitation process to recover magnesium from serpentine acid-leaching solution and to synthesize high purity Mg(OH)2 and 4MgCO3·Mg(OH)2·4H2O. Fe, Al, and Cr in the leaching solution were removed using the oxidation precipitation method with active MgO as a precipitant and H2O2 as an oxidant. Ni, Co and Mn were removed by Na2S precipitation to obtain a pure MgSO4 solution. Mg2+ ions were first precipitated with NH3·H2O to synthesize Mg(OH)2, followed by NH4HCO3 precipitation to obtain 4MgCO3·Mg(OH)2·4H2O. A small part of MgSO4 coprecipitates with Mg(OH)2 to form MgSO4·5Mg(OH)2·3H2O. The Mg(OH)2 was aged with a diluted NaOH solution to remove the sulfur; the two-stage precipitation percentage of Mg is 96.3%. Mg(OH)2 has a purity of 98.48% with a sulfur content of 0.28%. This process provides a promising method for the high-efficiency recovery of Mg and the large-scale production of the high purity of Mg(OH)2 from the serpentine.