Magnesium and nickel were recovered from nickel-rich serpentine through sulfation roasting and water leaching. The factors affecting the extraction percentages of Mg and Ni were discussed. Under the conditions of the ratio of acid to ore of 0.8:1 and roasting temperature of 650 °C for 120 min, 91.6% of Mg and 88.7% of Ni but only 4.8% of Fe were extracted. The roasting kinetics of Mg and Ni were investigated. The results showed that the roasting stage was governed by internal diffusion in the temperature range of 350–650 °C, and the activation energy of nickel and magnesium were different in the time ranges of 0–30 min and 60–120 min, with 17.45 kJ⋅mol−1 (0–30 min) and 14.12 kJ⋅mol−1 (60–120 min) for magnesium and 15.48 kJ⋅mol−1 (0–30 min) and 12.46 kJ⋅mol−1 (60–120 min) for nickel. The kinetic equations were obtained.
With the depletion of solid lithium ore, extracting lithium from salt lake brine has become a critical focus for future endeavors. A four-step method was used to synthesize high-purity H1.6Mn1.6O4 for extracting Li+. Porous cubic Mn2O3 was hydrothermally synthesized with carbon spheres and surfactants as templates. Then, it was converted to LiMnO2 by calcining with Li2CO3. After roasting and acid pickling, H1.6Mn1.6O4 was successfully synthesized. The impacts of calcination temperature, Li/Mn molar ratio and glucose addition on LiMnO2 composition, loss percentage of dissolved Mn in precursor, and the adsorption characteristics of the lithium ion sieve were studied. Glucose inhibited the formation of LiMn2O4 and promoted the formation of pure LiMnO2. The resulting precursor without impurities showed porous structure. After acid pickling, H1.6Mn1.6O4 showed a high-adsorption performance and excellent cycle performance. After five cycles, adsorption capacity remained above 30 mg/g, and the loss percentage of dissolved Mn stabilized at about 1%. The Li+–H+ exchange conformed to pseudo-second-order adsorption dynamics and the Langmuir adsorption isotherm equation, indicating that the adsorption process can be classified as monolayer chemical adsorption.