Conventional radiation-shielding composites usually contain lead, which results in high toxicity and poor portability. Tungsten (W) is an ideal radiation-shielding element that can replace lead due to its high atomic number and non-toxicity. In this work, radiation-shielding composites were prepared using natural rubber (NR) as a matrix and three different particle size powders, namely W, WO3 and WC, as fillers. The results show that, for X-rays, the linear attenuation coefficient of radiation-shielding composites based on natural rubber containing WC with a particle size of 50 μm (50 WC/NR) is 27.005 cm−1 at an X-ray tube voltage of 40 kV, which is more than 14 times the linear attenuation coefficient of NR. For γ-rays, a linear attenuation coefficient of 50 WC/NR achieves 8.320 cm−1 at 81 keV, which is over 55 times the linear attenuation coefficient of NR. In addition, 50 WC/NR had the highest elongation at break at 548.989% and had the lowest hardness at 62 HA. In summary, 50 WC/NR can be used as an alternative to traditional radiation-shielding materials containing lead and has wide application prospects.
The fluororesin membrane emerges as an ideal chemical-protective clothing material due to its excellent permeation resistance. However, using a fluororesin membrane with a low surface energy for compounding fabrics is very challenging. Herein, we demonstrate a strategy to modify the surface of a poly(ethylene-alt-tetrafluoroethylene) (ETFE) membrane by the atmospheric pressure dielectric barrier discharge (DBD) of plasma under different working voltages, processing times, and concentrations of acrylic acid (AA) in a helium (He) atmosphere. The increase in the hydrophilicity of the ETFE membrane is confirmed by the wettability test, which shows a significant decrease in the water contact angle, from 96° to 50°, after plasma modification. The interfacial T-peel strength of an ETFE membrane composited with polyester fabric increased from 0.53 N/cm to 13.64 N/cm after plasma modification. Significantly, the T-peel strength of the composite using a modified ETFE membrane with ultrasonic washing could still reach 11.75 N/cm. Various characterization methods clearly disclosed the physical and chemical changes on the ETFE membrane surface, such as introducing the polar -COOH group at a nano-level, improving the roughness, decreasing the ratios of the F/C element, and increasing the ratios of the O/C element, suggesting using nano-level grafted polyacrylic acid (g-PAA) on the surface of the membrane by DBD.