The aim of the present investigation is to evaluate the influence of the powder size of Cr3C2-25NiCr spraying powder on the fatigue behavior of HVOF-sprayed coating on the ASTM A516 steel substrate. Conventional commercial Cr3C2-25NiCr spraying powder was previously treated through high-energy milling. The crystallite sizes of milled powders were measured by X-ray diffraction and transmission electronic microscopy. Three different powder formats of the same Cr3C2-25NiCr composite were subjected to HVOF spraying to produce (i) a Milled-Coating (from high-energy milled spray powder), (ii) an Original-Coating (from conventional commercial spray powder), and (iii) a 50%–50% mixture of both (Milled + Original-Coating). The same spraying conditions were adopted for all the assessed cases. The sprayed coatings were investigated through the Knoop hardness test and SEM-EDS analysis. In addition, 3-point bending fatigue tests were conducted at different stress levels up to 107 cycles. The coating morphology and roughness effects on fatigue behavior were analyzed. The Cr3C2-25NiCr milled coating presented a lower fatigue life above the fatigue limit and a higher fatigue limit than other coatings; this outcome could be attributed to its lower surface roughness and finer grain size microstructure.
New β titanium alloys such as Ti-45Nb have been investigated for biomedical applications due to their promising mechanical and biocompatible properties. However, studies on micro-arc oxidation applied to Ti-45Nb surfaces are still scarce. This study explores the effect of micro-arc oxidation treatments on Ti-45Nb alloy surfaces using two different acidic electrolytes for anodization. The resulting surfaces were characterized by scanning electron microscopy, X-ray diffraction, contact angle measurements, surface energy analysis, roughness parameters, open-circuit potential, potentiodynamic polarization, and electrochemical impedance spectroscopy. Anodization significantly increased surface roughness, especially with sulfuric acid affecting the Ra parameter and phosphoric acid influencing Rt. Wettability and surface energy improved noticeably with reduced dispersive and increased polar components. The combined acid treatment (H3PO4 + H2SO4) provided superior corrosion resistance, as demonstrated by more stable Open-Circuit Potential, lower corrosion current densities, and higher impedance values. Equivalent circuit modeling suggested a more protective and complex oxide layer, attributed to greater surface heterogeneity and oxide thickness. These results indicate that anodization with the mixed acid solution is the most effective method to enhance corrosion resistance and surface performance of Ti-45Nb alloys for biomedical implants.
1 January 2024 in Anais do Congresso Nacional de Engenharia de Petróleo, Gás Natural e Biocombustíveis
O sistema de produção submarino é composto por diversos equipamentos e componentes que em conjunto realizam o processo de exploração de poços de petróleo e gás nas profundezas marinhas. O cabo umbilical, é um componente responsável por auxiliar no monitoramento remoto de parâmetros de variáveis como temperatura e pressão durante o processo de extração. Este cabo é composto no seu interior por diversas camadas contendo componentes funcionais e estruturais. Dentro deste contexto, está a armadura de tração, responsável por suportar esforços mecânicos como cargas axiais e cíclicas. Esta resistência é conferida através da união de um conjunto de arames de aço, médio e alto carbono, como o cabo umbilical possui dimensões quilométricas, os arames necessitam ser unidos através de soldas para ocupar toda extensão do cabo. Dessa forma, se faz necessário que o processo de soldagem seja efetivo e promova união entre as partes sem afetar de forma significativa a resistência dos arames. Com isso, este estudo traz a técnica de soldagem por fricção rotativa como alternativa à aplicação deste processo na união dos arames de armadura de tração. Diante dos resultados, a técnica se mostrou promissora, pois apresentou bom desempenho mecânico, com valores médios de tração e dureza. No entanto, a presença da microestrutura martensítica formada durante o processo de soldagem ainda é um fator a se corrigir no processo, dada a susceptibilidade à fragilização nesta região.
20 May 2026 in Journal of Failure Analysis and Prevention
High-carbon steel wires (0.7%C) are widely used in engineering due to their high strength and versatility. Among their various applications, their use under severe conditions, including embrittling environments and fatigue loading, is particularly noteworthy. Wire welding can introduce imperfections and weaken the material, an effect further aggravated by hydrogen-inducing agents. Although butt resistance welding is the most commonly employed technique for wires, it presents several limitations. This study investigates rotary friction welding as an alternative process, evaluating fatigue resistance and hydrogen embrittlement in 5.2 mm diameter wires, in comparison with the conventional resistance welding method. The results showed that friction-welded joints exhibited an approximately 90% increase in fatigue life and effectively eliminated the hydrogen embrittlement susceptibility observed in resistance welds, raising the success rate in testing from 20 to 100%. It is concluded that the rotary friction process reduces the formation of brittle microstructures and provides high resistance to hydrogen embrittlement. Therefore, the adoption of rotary friction welding is recommended for critical applications of high-carbon steel wires subjected to fatigue and hydrogen-susceptible environments.
27 March 2022 in Research, Society and Development
The umbilical cable is today an important technology used to control equipment on the seabed in the production of offshore oil in deep and ultra-deep waters. The umbilical is composed of several components, including steel tube for transporting fluids for hydraulic control of equipment in the bed. Such tubes are susceptible to fatigue during their life in umbilical operation. Fatigue strength is influenced by the accumulated plastic strain (APS) undergone by the tubes during the entire manufacturing process until installation/storage on spools. This present study investigated whether the way in which the APS is applied influences the fatigue strength of the tubes. Fatigue test specimens were machined from super duplex umbilical tube, which received 5% of APS by cyclic bending in two different ways: repeated bending and alternating bending. Microstructural and microhardness analyzes were performed on the specimens after fatigue fracture. No significant difference neither in microstructure, nor on the microhardness of the two groups of specimens was found after fatigue fracture. However, the group subjected to alternating plastic strain experienced lower fatigue strength. Therefore, the way in wich the tubes are deformed during manufacture and storage influences their fatigue performance.
RESUMO Ligas de titânio, especialmente Ti-6Al-4V, são empregadas em aplicações biomédicas. No entanto, elementos como alumínio e vanádio podem apresentar efeitos citotóxicos, estimulando a busca por novas ligas. A liga Ti-45Nb apresenta elevado potencial para uso em implantes dentários, devido ao seu baixo módulo de elasticidade, alta resistência à corrosão e biocompatibilidade. Apesar dessas propriedades, estudos sobre sua usinabilidade são escassos. Este trabalho experimental teve como objetivo caracterizar a microestrutura, composição elementar, propriedades físico-químicas e mecânicas, bem como avaliar a usinabilidade da liga Ti-45Nb. Amostras foram obtidas em barras maciças e preparadas por metalografia. A microestrutura foi revelada e analisada por microscopia óptica, MEV/EDS e DRX. Ensaios de microdureza seguiram normas ASTM, com análise estatística por ANOVA. A usinagem foi realizada por torneamento CNC utilizando fresas e parâmetros específicos. Resultados mostraram uma microestrutura monofásica β, dureza média de 187 HV e módulo de Young de 62 GPa. A usinagem foi eficaz, obtendo rugosidade e acabamento comparáveis aos implantes convencionais em Ti-Cp. A geometria dos implantes fabricados correspondeu ao projeto original. Conclui-se que a liga Ti-45Nb apresenta propriedades adequadas para aplicação em implantes dentários. Estudos futuros devem explorar aspectos biológicos e parâmetros ideais de usinagem, visando otimizar o desempenho clínico da liga.