It is shown that the phase transformations in the coating of the Fe-Al system produced by explosion welding of an aluminum AD1 with steel St3 and double occur in the following sequence: Fe 2 Al 5 → FeAl 2 → FeAl → Fe 3 Al → Fe (Al). They are accompanied by an increase in its thickness. The layered FeAl / Fe 3 Al / Fe (Al) coating on the inter-phase FeAl / Fe 3 Al boundary formed on a steel basis is porous, and inclusions of sulphides of manganese are present in alumina Fe 3 Al. The layered FeAl / Fe 3 Al / Fe (Al) coating on the steel base has a porous structure at the FeAl / Fe 3 Al interface, and inclusions of manganese sulfides in the Fe 3 Al aluminide region.
7 March 2023 in Materials and Manufacturing Processes
The results of studies of explosively welded NiCr-alloy (Cr20Ni80) + titanium alloy (OT4/VT20) composites are presented. The main parameters of explosive welding have been calculated. The wavy profile parameters and peel strength of composites after explosive welding in various modes was determined. It is shown that the change in the structure and properties of the welded joint is due to both the change in the initial hardness of the titanium alloy and the change in the collision point velocity. It was established that the molten metal are heterogeneous mixtures based on Ni(Cr,Ti) and Ti(Ni,Al) solid solutions and NiTi and Ni3Ti intermetallics. FEM modeling was carried out to determine the lifetime of the molten metal in the liquid state during the welding process. The calculated values of the molten metal cooling rates are 107–1010 K/s. Due to these values both stable crystalline and unstable (amorphous) phases are formed.
27 April 2021 in The International Journal of Advanced Manufacturing Technology